Engineering Papers⌕ Search

DOE OSTI · 22489080

Highly reflective polymeric substrates functionalized utilizing atomic layer deposition

Abstract

Reflective surfaces are one of the key elements of solar plants to concentrate energy in the receivers of solar thermal electricity plants. Polymeric substrates are being considered as an alternative to the widely used glass mirrors due to their intrinsic and processing advantages, but optimizing both the reflectance and the physical stability of polymeric mirrors still poses technological difficulties. In this work, polymeric surfaces have been functionalized with ceramic thin-films by atomic layer deposition. The characterization and optimization of the parameters involved in the process resulted in surfaces with a reflection index of 97%, turning polymers into a real alternative to glass substrates. The solution we present here can be easily applied in further technological areas where seemingly incompatible combinations of polymeric substrates and ceramic coatings occur.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Zuzuarregui, Ana, Gregorczyk, Keith E., Coto, Borja, Ruiz de Gopegui, Unai, Barriga, Javier, Rodríguez, Jorge, Knez, Mato. 2015-08-10. Highly reflective polymeric substrates functionalized utilizing atomic layer deposition. https://doi.org/10.1063/1.4928375. https://engineeringpapers.com/record/osti%3A22489080/highly-reflective-polymeric-substrates-functionalized-utilizing-atomic-layer-deposition

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Engineering Papers by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related reports

Vidyut3d: A GPU accelerated fluid solver for non-equilibrium plasmas on adaptive grids

We present the numerical methods, programming methodology, verification, and performance assessment of a non-equilibrium plasma fluid solver that can effectively utilize current and upcoming central processing and graphics processing unit (CPU+GPU) architectures, in this work. Our plasma fluid model solves the coupled conservation equations for species transport, electrostatic Poisson and electron temperature on adaptive Cartesian grids. Our solver is written using performance portable adaptive-grid/particle management library, AMReX, and is portable over widely available vendor specific GPU architectures. We present verification of our solver using method of manufactured solutions that indicate formal second order accuracy with central diffusion and fifth-order weighted-essentially-non-oscillatory (WENO) advection scheme. We also verify our solver with published literature on capacitive discharges and atmospheric pressure streamer propagation. We demonstrate the use of our solver on two 3D simulation cases: an atmospheric streamer propagation in Ar-H2 mixtures and a low pressure three-electrode radio frequency reactor. Our performance studies on three different CPU+GPU architectures indicate ~ 150-400X speed-up using AMD and NVIDIA GPUs per time step compared to a single CPU core for a 4 million cell simulation with 15 species.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Evaluating the Limits of QAOA Parameter Transfer at High-Rounds on Sparse Ising Models With Geometrically Local Cubic Terms

The emergent practical applicability of the Quantum Approximate Optimization Algorithm (QAOA) for approximate combinatorial optimization is a subject of considerable interest. One of the primary limitations of QAOA is the task of finding a set of good parameters, which is usually done using a variational optimization loop. Parameter transfer, or parameter concentration, is a phenomenon where QAOA angles trained on problem instances that are self-similar tend to perform well for other problem instances from that similar class. This suggests a potentially highly efficient and scalable non-variational learning method for QAOA angle finding. In this work, we systematically study QAOA parameter transferability from small problem sizes (16 and 27 decision variables) onto large problem instances (up to 156 qubits) for heavy-hex graph Ising models with geometrically local higher order terms using the Julia based QAOA simulation tool \texttt{JuliQAOA} to perform classical angle finding for up to $49$ QAOA layers ($p$). Parameter transfer of the fixed angles is validated using a combination of full statevector, Projected Entangled Pair States (PEPS), Matrix Product State (MPS), and LOWESA numerical simulations. We find that the QAOA parameter transfer from single instances applied to other (unseen) problem instances does not in general provide monotonically improving performance as a function of $p$ - there are many cases where the performance temporarily decreases as a function of $p$ - but despite this the transferred angles have a general trend of improved expectation value as the QAOA depth increases, in many cases converging close to the true ground-state energy of the $100+$ qubit instances. We also sample the hardware-compatible Ising models using the ensemble of transfer-learned QAOA parameters on several superconducting qubit IBM Quantum processors with 127, 133, and 156 qubits. We find continuous solution quality improvement of the hardware-compatible QAOA circuits run on the IBM NISQ processors up to $p=5$ on \texttt{ibm\_fez}, up to $p=9$ on \texttt{ibm\_torino}, and up to $p=10$ on \texttt{ibm\_pittsburgh}.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗