Stitching two-dimensional atomic crystals by atomic layer deposition as stable interfaces for batteries

Abstract

An anode includes: (1) a current collector; and (2) an interfacial layer disposed over the current collector. The interfacial layer includes a film of a layered material and a reinforcing material selectively disposed over certain regions of the film, while other regions of the film remain exposed from the reinforcing material.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Cui, Yi, Xie, Jin, Liao, Lei. 2022-11-15. Stitching two-dimensional atomic crystals by atomic layer deposition as stable interfaces for batteries. https://www.osti.gov/biblio/1986821