Atomic Layer Deposition for Materials-Based H2 Storage: Mg(BH4)2 as a Case Study

Abstract

To meet the requirements for vehicular solid-state hydrogen (H2) storage, novel materials such as metal borohydrides have increasingly been investigated, in particular, magnesium borohydride (Mg(BH4)2). While these materials have a high H2 capacity (> 14 wt%), poor hydrogenation-dehydrogenation cyclability and material degradation, (e.g., loss of boron), need to be overcome. Prior research has indicated that nano-encapsulation and chemical additives can address these challenges. Therefore, we pursued these two strategies simultaneously with atomic layer deposition (ALD) on Mg(BH4)2. We investigated the use of metal-oxides (e.g., Al2O3, TiO2, CeO2), Pt- group metals (e.g., Pd, Ru) as well as pulsing only one precursor molecule (e.g., Al(CH3)3, BBr3, TiCl4), and assessed these modified Mg(BH4)2 in terms of their H2 storage properties. This presentation will also present the benefits and limitations of using vapor-phase techniques to modify the properties of Mg(BH4)2.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Leick, Noemie (ORCID:0000000220146264), Strange, Nicholas A., Gennett, Thomas, Christensen, Steven T.. 2022-09-13. Atomic Layer Deposition for Materials-Based H2 Storage: Mg(BH4)2 as a Case Study. https://www.osti.gov/biblio/1888023

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Fabrication of Catalytic Distillation Membranes with Atomic Layer Deposition

The integration of catalysts onto the surface of membranes enables simultaneous physical separation and catalytic transformation of constituents in a feed stream, facilitating improved contaminant removal and fouling mitigation. Distillation membranes are a particularly attractive platform for catalytic membranes because they reject nonvolatile species and exhibit exceptional resistance to oxidative and radical-driven degradation. However, imparting catalytic functionality onto hydrophobic, porous distillation membranes has proven challenging since the membranes used are chemically inert and difficult to modify. Furthermore, catalysts on the membrane surface can decrease hydrophobicity and increase the membrane’s susceptibility to pore wetting and failure. In this work, we create a catalytic distillation membrane by coating a polytetrafluoroethylene membrane surface with titanium dioxide (TiO 2 ) via plasma-assisted atomic layer deposition (ALD). By precisely tuning the ALD parameters, we demonstrate localized growth of TiO 2 near (within approximately 1 μm) the surface of polytetrafluoroethylene membranes, forming a catalytically active interface while preserving the underlying hydrophobic pore structure. Localized growth of TiO 2 is confirmed by electron microscopy and spectroscopy techniques, and membranes coated with 500 cycles of ALD show pressure tolerance up to 12.8 bar and higher than 95% salt rejection in pressure-driven distillation. Photocatalytic activity is demonstrated via the degradation of methylene blue dye under UV irradiation, where increasing TiO2 loading leads to an enhancement in dye degradation. These results establish a general strategy for integrating catalytic functionality into chemically inert, hydrophobic membranes without compromising distillation performance, providing a pathway toward multifunctional membranes that couple advanced oxidation with membrane separation for water treatment.

atomic layer deposition↗

Synergistic Solvent-Surface Interactions Enable Alkyne Semihydrogenation at Palladium

Enabling higher yield and better selectivity for fine-chemical synthesis through heterogeneous catalysis is intricately linked to the interplay of active sites, reaction conditions, and mass transfer influence provided by the catalyst. Alkyne semihydrogenation is ubiquitous in the production of bulk chemicals in the pharmaceutical, polymer, or fine-chemical industries, but product selectivity remains a major challenge. Here, in this study, we demonstrate that the design of catalysts encompassing nickel (Ni) foams as contiguous monolith supports, decorated with ultralow loading of Pd/PdO x nanoparticles on a carbonized polydopamine interface and tuned with a thin layer of Al 2 O 3 , in conjunction with an optimized reaction environment leads to highly selective alkyne semihydrogenation. The reactions demonstrate good functional group tolerance and applicability to flow reactor systems. Combined computational and experimental studies are presented to describe the synergistic effect between the solvent-surface interaction and the degree of Pd surface reduction that are necessary to promote this selectivity. The system highlights the opportunity for catalyst-solvent codesign as a benign alternative to more complex reactants featuring extrinsic poisons or less-favored dopants.

atomic layer deposition↗

Probing Interfacial Reaction Pathways in Atomic Layer Deposition on Sulfide Superionic Conductors

Sulfide superionic conductors (e.g., argyrodite Li 6 PS 5 Cl, LPSCl) are extremely promising for all solid-state batteries, but poor atmospheric stability and high interfacial reactivity limit widespread adoption. Coating LPSCl powders with ultrathin coatings using atomic layer deposition (ALD) mitigates these problems, protecting against atmospheric degradation and reducing reactivity with Li metal, yielding more stable cycling. Despite significant promise, the ALD mechanism is unknown, hampering the development of new coating chemistries. In this study, we elucidate the mechanism for Al 2 O 3 ALD on LPSCl using trimethyl aluminum (TMA) and H 2 O by combining in situ Fourier transform infrared spectroscopy, ex situ solid-state magic angle spinning nuclear magnetic resonance, UV Raman spectroscopy, X-ray photoelectron spectroscopy, and density functional theory calculations. We determine that ALD Al 2 O 3 nucleates promptly via TMA reaction with native —OH, —SH, and PS 3 -OH groups to form transient C–Al–O(S) species that are rapidly hydrolyzed during the subsequent H 2 O exposure. This reversible transformation maintains surface nucleophilicity and prevents sulfide decomposition. The resulting layer-by-layer growth leads to highly conformal Al 2 O 3 coatings on LPSCl that are readily scalable to ≥ 50 g quantities using a rotating drum fixture. This detailed understanding of ALD surface reactions provides critical insights guiding the selection of future ALD chemistries with improved performance.

atomic layer deposition↗