Superalloys Development at NETL: Design, Processing, Characterization and Mechanical Testing

Abstract

Seminar at Oregon State University, March 1, 2021

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Detrois, Martin, Jablonski, Paul, Gao, Michael, Rozman, Kyle A., Hawk, Jeffrey. 2021-03-01. Superalloys Development at NETL: Design, Processing, Characterization and Mechanical Testing. https://www.osti.gov/biblio/1844509