Dopamine-Mediated Polymer Coating Facilitates Area-Selective Atomic Layer Deposition

Abstract

Area-selective atomic layer deposition (ALD) has the potential to significantly improve current fabrication approaches by introducing a bottom-up process in which robust and conformal thin films are selectively deposited onto patterned substrates. This bottom-up approach requires selective areas of the substrates to be masked to inhibit deposition. Spontaneous self-assembly and organization of a mask, incorporating adhesion and other functions, are particularly attractive for this role as they do not require a separate patterning step. In this work, we make use of the pH/light tunability of catechol adhesion to develop a catechol-functionalized polymer that exhibits tunable adhesion strengths on different materials based on their specific chemistry. Tunable selective deposition was shown between metal/metal oxide substrates by controlling the local pH. Moreover, by controlling the adhesion strength through UV light, the deposition of hafnium oxide (HfO 2 ) during ALD was successfully inhibited.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Papananou, Hellen, Katsumata, Reika, Neary, Zachary, Goh, Rubayn, Meng, Xiangxi, Limary, Ratchana, Segalman, Rachel A.. 2021-09-08. Dopamine-Mediated Polymer Coating Facilitates Area-Selective Atomic Layer Deposition. https://doi.org/10.1021/acsapm.1c00692

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗