Heterogeneous catalysts are a key enabler of the transition towards a sustainable, bio-based economy for fuels and chemicals. However, the harsh conditions in many biomass conversion processes lead to nanoparticle sintering, support collapse, and metal leaching in conventional PGM catalysts. Next-generation catalysts must be developed to address these stability challenges. This presentation will discuss ongoing work between the Catalytic Carbon Transformation & Scale-Up Center at NREL and various industrial partners to develop scalable, cost-effective atomic layer deposition (ALD) coatings for improving the performance of biomass conversion catalysts. Substantial focus will be devoted to the benefits of TiO2 ALD coatings on supported Pd hydrogenation catalysts. Ten cycles of TiO2 ALD were found to dramatically improve the activity of a conventional Pd/Al2O3 catalyst towards aromatic hydrogenation, despite partial coverage of the Pd sites by the ALD layer. Subsequent advanced characterization and atomic-scale computational modeling revealed that the ALD coating influenced the adsorption strength of hydrogenation surface intermediates in unexpected ways, leading to higher reaction rates. Reaction testing after exposure to sulfur impurities, high temperature oxidation, and hydrothermal treatment demonstrated the improved stability of the ALD-coated catalyst. Additionally, the ALD synthesis process was found to be scalable over two orders of magnitude with minimal deviation in synthesized catalyst properties. These results were contextualized with cost models of industrial ALD coating and aromatic hydrogenation processes to further refine the value proposition of ALD coatings. Given the demonstrated improvements in hydrogenation, TiO2 ALD coatings have also been applied to supported Pt catalysts for use in other biomass conversion reactions, such as hydrodeoxygenation for production of sustainable aviation fuel (SAF) and the oxidation of glucose for bio-derived gluconic acid. Recent findings from these experimental campaigns will also be shared. ALD technology holds great potential in the development of next-generation catalysts for biofuels and bioproducts and this work constitutes an important examination of the impact of ALD coatings in a variety of reaction environments.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

McNeary, W. Wilson. 2021-09-27. Atomic Layer Deposition for Improved Biomass Conversion Catalysts. https://www.osti.gov/biblio/1823441

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Impacts of Pasture Conversion to Sugarcane on Water Fluxes and Water Use Efficiency in the Southeastern US

The expansion of sugarcane (cane), a high-yielding perennial crop, will likely reshape the bioenergy landscape in the Southeastern US. However, its ecohydrological implications, particularly following conversion from grazed pastures, a dominant land use in the region, remain highly uncertain. We investigated the impact of cane expansion on evapotranspiration (ET) and its partitioning, and the mechanisms influencing both ET components and water use efficiency (WUE) across multiple scales and growth cycles in subtropical Florida. We combined eddy covariance, biometric measurements, and process-based stomatal conductance (g s ) models. ET was 1.7% lower in cane than in improved pasture (IMP) but exceeded that in semi-native pasture (SN) by 21%. Transpiration (T) followed a similar pattern, consistent with lower g s in cane relative to IMP. Cane had more conservative water use and greater sensitivity of g s to vapor pressure deficit (VPD) compared to IMP pasture, suggesting cane may be more tolerant of increasing atmospheric water demand. In contrast, SN showed lower g s and weaker stomatal sensitivity to VPD compared to cane, resulting in lower T. In cane, stomatal regulation and T varied across growth cycles, with stomata becoming less water conservative as stands matured, highlighting the importance of incorporating stand age-dependent stomatal regulation into hydrological models. Evaporation (E) was higher in cane than pastures (19%–26%), partially offsetting WUE gains. Cane exhibited higher intrinsic WUE (GPP/g s ; Gross Primary Productivity), ecosystem WUE (GPP/ET), and harvest WUE (harvest/ET) than both pasture types. Large-scale pasture-to-cane conversion could produce widely contrasting hydrological outcomes. The net regional impact will depend on the proportion of each pasture type converted and on cane's high g s sensitivity to VPD, which triggers tight stomatal regulation and conservative water use, both of which will become increasingly consequential under intensifying atmospheric water demand.

bioenergy↗

OxyR regulates the oxidative stress response in Zymomonas mobilis during oxic growth and anoxic biofuel fermentation

The bacterium Zymomonas mobilis is widely studied for its potential as an industrial biofuel producer. Anoxic fermentation by Z. mobilis in lignocellulosic hydrolysate can generate bioethanol from renewable plant biomass. In this study, we deleted a gene from the Z. mobilis genome encoding a homolog of OxyR, a transcription factor that activates an oxidative stress response in bacteria to reduce reactive oxygen species (ROS). Deletion of this transcription factor inhibited growth of Z. mobilis in oxic, but not anoxic, conditions in laboratory media. RNA-Sequencing was perfromed on wild-type Z. mobilis (ZM4) and ∆oxyR in both oxic and anoxic conditions in rich media (ZRMG). This study reveals the indirect regulon of OxyR in Z. mobilis, which is important for both oxic growth and anoxic biofuel fermentation.

bioenergy↗

Outreach_and_Workforce_Development_Bioproduct_Activity_Kits

The Center for Bioenergy Innovation Outreach and Workforce Development Bioproduct Activity Kits includes gackground, materials, and other information for 5 different hands-on activities that can be used in outreach events with the public to cultivate interest and knowledge in biomass- and bioproduct-related scientific concepts used in CBI. The main document includes suggestions for kit materials, talking points, documentation that can be displayed or printed; and supplementary files include the board game and cards that can be printed for use. The kits are designed for various age groups and can be adapted for different needs, audiences, and standards.

bioenergy↗