Materials Data on FeIr by Materials Project

Abstract

FeIr crystallizes in the trigonal R-3m space group. The structure is three-dimensional. there are three inequivalent Fe sites. In the first Fe site, Fe is bonded to six equivalent Fe and six equivalent Ir atoms to form distorted FeFe6Ir6 cuboctahedra that share corners with twelve FeFe6Ir6 cuboctahedra, edges with twelve FeFe6Ir6 cuboctahedra, edges with twelve equivalent IrFe6Ir6 cuboctahedra, faces with six equivalent FeFe6Ir6 cuboctahedra, and faces with twelve equivalent IrFe6Ir6 cuboctahedra. All Fe–Fe bond lengths are 2.64 Å. All Fe–Ir bond lengths are 2.59 Å. In the second Fe site, Fe is bonded to six equivalent Fe and six Ir atoms to form distorted FeFe6Ir6 cuboctahedra that share corners with five equivalent IrFe6Ir10 cuboctahedra, corners with twelve FeFe6Ir6 cuboctahedra, edges with ten IrFe6Ir6 cuboctahedra, edges with twelve FeFe6Ir6 cuboctahedra, faces with six equivalent FeFe6Ir6 cuboctahedra, and faces with fifteen IrFe6Ir6 cuboctahedra. All Fe–Fe bond lengths are 2.64 Å. All Fe–Ir bond lengths are 2.59 Å. In the third Fe site, Fe is bonded to six equivalent Fe and six Ir atoms to form distorted FeFe6Ir6 cuboctahedra that share corners with five equivalent IrFe6Ir10 cuboctahedra, corners with twelve FeFe6Ir6 cuboctahedra, edges with ten IrFe6Ir6 cuboctahedra, edges with twelve FeFe6Ir6 cuboctahedra, faces with six equivalent FeFe6Ir6 cuboctahedra, and faces with fifteen IrFe6Ir6 cuboctahedra. All Fe–Fe bond lengths are 2.64 Å. All Fe–Ir bond lengths are 2.59 Å. There are two inequivalent Ir sites. In the first Ir site, Ir is bonded to six Fe and six equivalent Ir atoms to form distorted IrFe6Ir6 cuboctahedra that share corners with twelve IrFe6Ir6 cuboctahedra, edges with twelve FeFe6Ir6 cuboctahedra, edges with twelve IrFe6Ir6 cuboctahedra, faces with six equivalent IrFe6Ir6 cuboctahedra, and faces with twelve FeFe6Ir6 cuboctahedra. All Ir–Ir bond lengths are 2.64 Å. In the second Ir site, Ir is bonded to six Fe and ten equivalent Ir atoms to form distorted IrFe6Ir10 cuboctahedra that share corners with ten FeFe6Ir6 cuboctahedra, corners with twelve IrFe6Ir6 cuboctahedra, edges with eight FeFe6Ir6 cuboctahedra, edges with sixteen IrFe6Ir6 cuboctahedra, faces with sixteen equivalent IrFe6Ir10 cuboctahedra, and faces with eighteen FeFe6Ir6 cuboctahedra. There are a spread of Ir–Ir bond distances ranging from 2.64–5.28 Å.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

2020-05-03. Materials Data on FeIr by Materials Project. https://doi.org/10.17188/1695881

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗