Engineering Papers⌕ Search

DOE OSTI · 1633727

Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization

Abstract

Improvements in energy-water systems will necessitate fabrication of high-performance separation membranes. To this end, interface engineering is a powerful tool for tailoring properties, and atomic layer deposition (ALD) has recently emerged as a promising and versatile approach. However, most non-polar polymeric membranes are not amenable to ALD processing due to the absence of nucleation sites. Here, a sensitization strategy for ALD-coating is presented, illustrated by membrane interface hydrophilization. Facile dip-coating with polyphenols effectively sensitizes hydrophobic polymer membranes to TiO2 ALD coating. Tannic acid-sensitized ALD-coated membranes exhibit outstanding underwater crude oil repulsion and rigorous mechanical stability through bending and rinsing tests. As a result, these membranes demonstrate outstanding crude oil-in-water separation and reusability compared to untreated membranes or those treated with ALD without polyphenol pretreatment. A possible polyphenol-sensitized ALD mechanism is proposed involving initial island nucleation followed by film intergrowth. This polyphenol sensitization strategy enriches the functionalization toolbox in material science, interface engineering, and environmental science.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Yang, Xiaobin, Sun, Pan, Zhang, Huiru, Xia, Zijing, Waldman, Ruben Z., Mane, Anil U., Elam, Jeffrey W., Shao, Lu, Darling, Seth B.. 2020-02-16. Polyphenol-Sensitized Atomic Layer Deposition for Membrane Interface Hydrophilization. https://doi.org/10.1002/adfm.201910062

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗