High Gradient Accelerator Cavities Using Atomic Layer Deposition

Abstract

In the Phase I program, Calabazas Creek Research, Inc. (CCR), in collaboration with North Carolina State University (NCSU), fabricated copper accelerator cavities and used Atomic Layer Deposition (ALD) to apply thin metal coatings of tungsten and platinum. It was hypothesized that a tungsten coating would provide a robust surface more resistant to arcing and arc damage. The platinum coating was predicted to reduce processing time by inhibiting oxides that form on copper surfaces soon after machining. Two sets of cavity parts were fabricated. One was coated with 35 nm of tungsten, and the other with approximately 10 nm of platinum. Only the platinum cavity parts could be high power tested during the Phase I program due to schedule and funding constraints. The platinum coated cavity exhibit poor performance when compared with pure copper cavities. Not only did arcing occur at lower power levels, but the processing time was actually longer. There were several issues that contributed to the poor performance. First, machining of the base copper cavity parts failed to achieve the quality and cleanliness standards specified to SLAC National Accelerator Center. Secondly, the ALD facilities were not configured to provide the high levels of cleanliness required. Finally, the nanometer coating applied was likely far too thin to provide the performance required. The coating was ablated or peeled from the surface in regions of high fields. It was concluded that the current ALD process could not provide improved performance over cavities produced at national laboratories using dedicated facilities.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Ives, Robert Lawrence, Parsons, Gregory, Williams, Philip, Oldham, Christopher, Mundy, Zach, Dolgashev, Valery. 2014-12-09. High Gradient Accelerator Cavities Using Atomic Layer Deposition. https://doi.org/10.2172/1165161

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Design and Integration of High Precision Superconducting Magnet Power Supply Systems

This paper reviews the design and integration approach being taken to power more than 400 superconducting magnets in Electron Ion Collider (EIC) by power supplies ranging from 20V to 400V and 100A to 18kA. A major challenge is to integrate existing legacy power supplies with new high current systems and maximize performance and reduce costs. Successful implementation requires coordinated integration of power convertors, current regulation, quench protection, energy extraction, machine protection, controls and existing accelerator infrastructure.

43 PARTICLE ACCELERATORS↗

Searching for the Most Harmful Field Errors in the HSR IR Superconducting Magnets

In this project, we improve beam stability for the Electron-Ion Collider. Magnetic field errors can reduce beam stability, making it essential to identify the field errors that have the greatest impact on accelerator performance. However, this is particularly challenging because beam stability depends on the complex interactions of many magnetic field errors, resulting in a high-dimensional and nonlinear optimization problem. We determine which field errors are the most influential for the large physical aperture superconducting magnet B2PF, a critical magnet in the Interaction Region (IR) in the Hadron Storage Ring (HSR). We complete and analyze nearly 30,000 simulations on the Brookhaven National Laboratory Linux Cluster by varying 18 nonlinear magnetic field errors. We evaluate beam stability using the dynamic aperture and the tune diffusion. We identify the field errors that most strongly influence beam stability and establish quantitative field error tolerances that improve accelerator performance.

43 PARTICLE ACCELERATORS↗