Atomic Layer Deposition for SRF Cavities

Abstract

We have begun using Atomic Layer Deposition (ALD) to synthesize a variety of surface coatings on coupons and cavities as part of an effort to produce rf structures with significantly better performance and yield than those obtained from bulk niobium, The ALD process offers the possibility of conformally coating complex cavity shapes with precise layered structures with tightly constrained morphology and chemical properties. Our program looks both at the metallurgy and superconducting properties of these coatings, and also their performance in working structures. Initial results include: 1) evidence from point contact tunneling showing magnetic oxides can be a significant limitation to high gradient operation, 2) experimental results showing the production sharp niobium/oxide interfaces from a high temperature bake of ALD coated Al2O3 on niobium surfaces, 3) results from ALD coated structures.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Norem, J, Pellin, M J, Antoine, C Z, Ciovati, G, Kneisel, P, Reece, C E, Rimmer, R A, Cooley, L, Gurevich, A V, Ha, Y, Proslier, Th, Zasadzinski, J. 2009-05-01. Atomic Layer Deposition for SRF Cavities. https://engineeringpapers.com/record/osti%3A1021867/atomic-layer-deposition-for-srf-cavities

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Engineering Papers by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗