Abstract
To guide development of microwave process technology that could be used during in situ construction on the Moon, we measured the high-temperature basic dielectric properties (εʹ and εʺ) of 17 lunar simulants and related materials. In order to confidently use these data one needs to understand the data’s strengths and weaknesses. Therefore, a goal of this publication is to provide insights into the comparative effects of sample composition, pre-treatments, experimental variables, high temperatures, and other factors on the measured response. The dielectric measurements were performed using the cavity perturbation method over a temperature range between room temperature to 1000 °C, or higher, and provided the real and imaginary components of permittivity at six frequencies. The utility of the original values was limited by the varying density of the pellets used in the measurement. Therefore, all of the εʹ and εʺ measurements at the frequency of 2466 MHz have been scaled to a constant density, 1.75 g/cm 3 . Here the data are presented as graphs chosen to aid analysis within and across simulant groups. To gain additional insight into the processes happening at the elevated temperatures in the dielectric measurements, heat capacity data was obtained using differential scanning calorimetry (DSC) on several of the simulant materials. Our data show that over the frequency range 397 MHz – 2985 MHz a material’s behavior does not greatly change, as compared to the scale of differences observed between lunar mare and highland simulants at high temperatures. For example at 1000 °C, the mare simulant JSC-1A absorbs 10 times more power than the highland simulant NUW-LHT-5M. We observe that as melting temperatures are reached both permittivity and dielectric loss rise non-linearly, helping to explain thermal runaway during microware heating. Our data show that even less than a few weight % of many non-lunar minerals, and the use of mixtures in simulants can affect the dielectric behavior at higher temperatures. A comparison of our results with published dielectric data for Apollo samples and with remote sensing of the Moon supports the conclusion the simulants and lunar material at room temperature have very similar dielectric values.
Explore related subjects
Keep this discovery
Douglas L Rickman, Ronald M Hutcheon, Holly S Shulman, Jozef Mouris, Austin Patridge, Alan Whittington. 2026-05-08. High Temperature Dielectric Properties and Differential Scanning Calorimetry of Lunar Simulants. https://ntrs.nasa.gov/citations/20260000919
Cite the original work for its findings. Save a collection to share your selection of sources.
Discover connections
Connections use source metadata and explicit phrase matches, not verified experimental comparisons.