Creep Testing of Vectran Yarn
Abstract
Presentation detailing the creep testing of Vectran yarn using two different test stands.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Sarah L. Langston. Creep Testing of Vectran Yarn. https://ntrs.nasa.gov/citations/20205007607