Friction pull plug welding: top hat plug design
Abstract
Friction Pull Plug Welding is a solid state repair process for defects up to one inch in length, only requiring single sided tooling, or outside skin line (OSL), for preferred usage on flight hardware. The most prevalent defect associated with Friction Pull Plug Welding (FPPW) was a top side or inside skin line (ISL) lack of bonding. Bonding was not achieved at this location due to the reduction in both frictional heat and welding pressure between the plug and plate at the end of the weld. Thus, in order to eliminate the weld defects and increase the plug strength at the plug `top` a small `hat` section is added to the pull plug for added frictional heating and pressure.
Keep this discovery
Explore connections, maps & timelines
Coletta, Edmond R., Cantrell, Mark A.. 2001-07-03. Friction pull plug welding: top hat plug design. https://engineeringpapers.com/record/nasa%3A20080004890/friction-pull-plug-welding-top-hat-plug-design
Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Engineering Papers by Indiciae: BibTeX · RIS.