Surface Analysis and Tools

Abstract

This article is a chapter of the book entitled, "Tribology of Mechanical Systems," to be published by ASME Press, New York, NY. It describes selected analytical techniques, which are being used in understanding phenomena and mechanisms of oxidation, adhesion, bonding, friction, erosion, abrasion, and wear, and in defining the problems. The primary emphasis is on microanalytical approaches to engineering surfaces.