Quantitative Hydrocarbon Surface Analysis

Abstract

The elimination of ozone depleting substances, such as carbon tetrachloride, has resulted in the use of new analytical techniques for cleanliness verification and contamination sampling. The last remaining application at Rocketdyne which required a replacement technique was the quantitative analysis of hydrocarbons by infrared spectrometry. This application, which previously utilized carbon tetrachloride, was successfully modified using the SOC-400, a compact portable FTIR manufactured by Surface Optics Corporation. This instrument can quantitatively measure and identify hydrocarbons from solvent flush of hardware as well as directly analyze the surface of metallic components without the use of ozone depleting chemicals. Several sampling accessories are utilized to perform analysis for various applications.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Douglas, Vonnie M.. 2000-01-01. Quantitative Hydrocarbon Surface Analysis. https://ntrs.nasa.gov/citations/20000039372

Cite the original work for its findings. Save a collection to share your selection of sources.