High-pressure creep tests

Abstract

The automotive Stirling engine, presently being developed by the U.S. Department of Energy and NASA, uses high-pressure hydrogen as a working fluid; its long-term effects on the properties of alloys are relatively unknown. Hence, creep-rupture testing of wrought and cast high-temperature alloys in high-pressure hydrogen is an essential part of the research supporting the development of the Stirling cycle engine. Attention is given to the design, development, and operation of a 20 MPa hydrogen high-temperature multispecimen creep-rupture possessing high sensitivity. This pressure vessel allows for the simultaneous yet independent testing of six specimens. The results from one alloy, XF-818, are presented to illustrate how reported results are derived from the raw test data.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Bhattacharyya, S., Lamoureux, J., Hales, C.. 1986-07-01. High-pressure creep tests. https://ntrs.nasa.gov/citations/19860061826

Cite the original work for its findings. Save a collection to share your selection of sources.