Surface analysis in composite bonding
Abstract
X ray photoelectron spectroscopy and contact angle measurements on graphite fiber composites pretreated in a number of different ways including mechanical, chemical, and light irradiation were analyzed. Data acquired on surface contamination as a result of fabrication techniques provides answers to the strength and durability of adhesively bonded composites. These techniques were shown to provide valuable information on surface analysis of pretreated composites prior to adhesive bonding and following lap shear fracture.