Superalloy composition modeling

Abstract

Development of a predictive method for determination of the gamma/gamma prime phase fields, i.e., gamma prime volume fraction as a function of the multicomponent composition, is described. The cluster variation method used for binary alloys in which the precipitated phase is coherent with the matrix phase is extended for application to the multicomponent coherent gamma/gamma prime nickel-based superalloys. It is shown that the cluster variation method can accurately describe the equilibrium (incoherent) gamma/gamma prime phase fields in the binary Ni-Al phase diagram. The gamma/gamma prime phase field for the Ni-Cr-Al ternary phase diagram is computed as a function of temperature. A reasonable fit results between the calculated and the experimental diagrams. The modeling of the six-component Ni-Cr-Al-Co-Mo-Ti base superalloy and the effect of Ni substitution of Co are discussed.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Barefoot, J., Jarrett, R., Sanchez, J., Tien, J.. 1982-10-01. Superalloy composition modeling. https://ntrs.nasa.gov/citations/19830003014

Cite the original work for its findings. Save a collection to share your selection of sources.