Residual Silicone Detection

Abstract

Both photoelectron emission and ellipsometry proved successful in detecting silicone contamination on unpainted and epoxy painted metal surfaces such as those of the external tank and the solid rocket booster. Great success was achieved using photoelectron emission (PEE). Panels were deliberately contaminated to controlled levels and then mapped with PEE to reveal the areas and levels that were contaminated. The panels were then tested with regard to adhesive properties. Tapes were bonded over the contaminated and uncontaminated regions and the peel force was measured, or the contaminated panels were bonded (with CPR 483 foam) to uncontaminated panels and made into lap shear specimens. Other panels were bonded and made into wedge specimens for hydrothermal stress endurance tests. Strong adhesion resulted if the PEE signal fell within an acceptance window, but was poor outside the acceptance window. A prototype instrument is being prepared which can automatically be scanned over the external liquid hydrogen tank and identify those regions that are contaminated and will cause bond degradation.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Smith, T.. 1980-12-01. Residual Silicone Detection. https://ntrs.nasa.gov/citations/19810009875

Cite the original work for its findings. Save a collection to share your selection of sources.