Advanced protective coating for superalloys

Abstract

Superior oxidation protection for nickel-base alloys at temperatures up to 1367 K was obtained with cobalt-base alloy coating. Coating had 25 Cr, 14 Al, and 0.5 Y weight percent composition. Coating was applied by electron beam vapor deposition to thickness of 76 to 127 microns.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Elam, R. C., Talboom, F. P., Wilson, L. W.. 1972-12-01. Advanced protective coating for superalloys. https://ntrs.nasa.gov/citations/19720000150