Compounds and composition for preparation of lithium-loaded plastic scintillators

A scintillator material includes a polymer matrix, a primary dye in the polymer matrix, the primary dye being a fluorescent dye; a secondary dye, and a Li-containing compound in the polymer matrix, where the Li-containing compound is a Li salt of a short-chain aliphatic acid. In addition, the scintillator material exhibits an optical response signature for thermal neutrons that is different than an optical response signature for fast neutrons.

Zaitseva, Natalia P.↗

Defect-resistant plastic scintillators with aliphatic additives

A plastic scintillator includes a polymer matrix, an aliphatic additive present in the polymer matrix in an effective amount to impart fog resistance to the plastic scintillator, and at least one fluorescent dye in the polymer matrix, the dye being effective to provide scintillation upon exposure to radiation. The effective amount of the aliphatic additive is in a range of greater than 0 weight percent up to 5 weight percent relative to the total weight of the plastic scintillator. Moreover, the aliphatic additive has a structure comprising up to 300 repeat units.

Mabe, Andrew Neil↗

Synthesis and processing of lithium-loaded plastic scintillators on the kilogram scale

Plastic scintillators that can discriminate between gamma rays, fast neutrons, and thermal neutrons were synthesized and characterized while considering the performance at the kilogram scale. The synthesis and processing of these plastic scintillators on the kilogram scale required examination of several factors. The examination of these factors was necessitated by the inclusion of 0.1 wt.% lithium-6 to enable detection of thermal neutrons. First, methacrylic acid was used as an additive to solubilize salts of lithium-6, which allow for a thermal-neutron capture reaction that produces scintillation light following energy transfer. Second, a trade-off between scintillation performance and processability was considered because the increasing content of the methacrylic acid that aided processability resulted in a sharp decrease in the light output. The use of small amounts of methacrylic acid (≤3 wt.%) resulted in better performance but required high processing temperatures. At large scales, these high temperatures could initiate exothermic polymerization that results in premature curing and/or defects. Additionally, the deleterious effects of the methacrylic acid may be mitigated by using m-terphenyl as a primary dye rather than 2,5-diphenyloxazole (PPO), which has been traditionally used in organic scintillators. Finally, the curing environment was controlled to avoid defects like cracking and discolouration​ while maintaining solubility of dopants during curing. For scintillators that were produced from kilogram-scale batches of precursors, the effective attenuation of scintillation light was characterized.