Experimental Validation and Continuous Testing of an On-Purpose High-Yield Pitch Synthesis Process for Producing Carbon Fiber from US Domestic Coal
This project aims to develop technology that converts domestic United States (US) raw coal to high quality, high value, and marketable carbon fiber. More specifically, the project aims to significantly improve the selectivity and yield of carbon fiber produced per ton of coal over conventional coal pitch-based production by using low-severity direct coal conversion technology to maximize the yield of pitch from coal, suitable for production of carbon fiber. To meet the stated objective of developing a technology platform, capable of producing high quality, high-value and marketable carbon fiber from domestic US coal, the proposed scope of work involves testing of a low-severity direct coal liquefaction (LS-DCL) process approach. The isotropic pitch produced from the LS-DCL process will be thermally treated using conventional processes to convert to a liquid crystal or “mesophase” pitch as a precursor for structural carbon fibers. This mesophase pitch will then be melt-spun into fiber, oxygen stabilized, and carbonized using conventional processes. The resulting carbon fiber will be evaluated for mechanical properties and suitability for structural applications such as automotive parts and spars for wind turbine blades. The overall process is expected to significantly lower the cost of fiber compared to state of the art fibers produced from polyacrylonitrile (PAN) precursors.