Two-Dimensional Covalent Organic Framework Solid Solutions
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Yeung, Michael T..
Explore the source record for details and available documents.
Materials with superior hardness can be categorized as ultrahard (Vickers hardness, H v ≥ 80 GPa) and superhard (H v ≥ 40 GPa). These materials are commonly used as cutting tools and abrasives in the machining and manufacturing industries. With its extreme hardness, diamond is the best known and most used ultrahard material for industrial applications. However, it is ineffective at cutting and drilling ferrous alloys due to diamond's high reactivity with iron and poor thermal stability in air. Additionally, the synthesis of diamond requires both high pressure (HP) and high temperature, making it an expensive process. These limitations have driven the search for alternative superhard materials that are capable of cutting steels and other materials at lower costs. This article reviews the concept of hardness and summarizes advancements in the synthesis and mechanical properties of hard materials. It begins with a review of methods to measure hardness, adding HP diffraction methods to more conventional hardness measurements. It then considers new ultrahard materials that exist within the B–C–N ternary system, with hardness approaching diamond but improved chemical stability. Finally, it surveys superhard nitrides, oxides, and borides as potential alternative materials, focusing on transition metal boride systems where the synthesis can be readily achieved at ambient pressure and scaled for industrial applications. We hope that this article serves as an overview of hard materials and guide for the comparison of data reported in the literature.
Not Available
Single-phase metal dodecaboride solid solutions, Zr 0.5 Y 0.5 B 12 and Zr 0.5 U 0.5 B 12 , were arranged by arc melting from pure elements. The phase purity and composition were established by powder X-ray diffraction (PXRD), energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and 10 B and 11 B solid-state nuclear magnetic resonance (NMR) spectroscopy. The effects of carbon addition to Zr 1-x Y x B 12 were studied and it was found that carbon causes fast cooling and as a result rapid nucleation of grains, as well as “templating” and patterning effects of the surface morphology. The hardness of the Zr 0.5 Y 0.5 B 12 phase is 47.6 ± 1.7 GPa at 0.49 N load, which is ~17% higher than that of its parent compounds, ZrB 12 and YB 12 , with hardness values of 41.6 ± 2.6 and 37.5 ± 4.3 GPa, respectively. The hardness of Zr 0.5 U 0.5 B 12 is ~54% higher than that of its UB 12 parent. The dodecaborides were confirmed to be metallic by band structure calculations, diffuse reflectance UV–vis, and solid-state NMR spectroscopies. The nature of the dodecaboride colors—violet for ZrB 12 and blue for YB 12 —can be applied to charge-transfer. XPS indicates that the metals are in the following oxidation states: Y 3+ , Zr 4+ , and U$^{{5+}/^{6+}}$. The superconducting transition temperatures (T c ) of the dodecaborides were determined to be 4.5 and 6.0 K for YB 12 and ZrB 12 , respectively, as shown by resistivity and superconducting quantum interference device (SQUID) measurements. The T c of the Zr 0.5 Y 0.5 B 12 solid solution was suppressed to 2.5 K.
Abstract The deformation behavior of the three metal dodecaborides (YB 12 , ZrB 12 , and Zr 0.5 Y 0.5 B 12 ) is investigated using radial X‐ray diffraction under nonhydrostatic compression up to ≈60 GPa with a goal of understanding how bonding and metal composition control hardness. Zr 0.5 Y 0.5 B 12 , which has the highest Vickers hardness ( Hv = 45.8 ± 1.3 GPa at 0.49 N load), also shows the highest bulk modulus ( K 0 = 320 ± 5 GPa). The 0.49 N hardness for ZrB 12 and YB 12 are both lower and very similar, and both show lower bulk moduli ( K 0 = 276 ± 7 GPa, and K 0 = 238 ± 6 GPa, respectively). Differential stress is then measured to study the strength and strength anisotropy. Zr 0.5 Y 0.5 B 12 supports the highest differential stress, in agreement with its high hardness, a fact that likely arises from atomic size mismatch between Zr and Y combined with the rigid network of boron cages. The (200) plane for all samples supports the largest differential strain, while the (111) plane supports the smallest, consistent with the theoretically predicted slip system of {111} [ ]. Strain softening is also observed for ZrB 12 . Finally, the full elastic stiffness tensors for ZrB 12 and YB 12 are solved. ZrB 12 is the most isotropic, but the extent of elastic anisotropy for all dodecaborides studied is relatively low due to the highly symmetric boron cage network.
The differential strain behavior of Ta x W 1-x B solid solutions has been studied as a function of composition using high-pressure radial X-ray diffraction in a diamond-anvil cell under non-hydrostatic pressure (up to ~65 GPa) to understand the hardening mechanisms in this family of materials. The hardness of tungsten monoboride (WB) can be increased by adding tantalum and reaches a maximum at a doping level of 50 at. % with a value of 42.8 ± 2.6 GPa under an applied load of 0.49 N. Plateaus were observed in the differential strain data for both the (020) and (002) directions, suggesting that this is the primary slip system in this material. These plateaus were modified by the addition of Ta, indicating that strengthening of the (002) and (020) planes by solid solution hardening was primarily responsible for the hardness enhancements in Ta x W 1-x B solid solutions. In contrast, the differential strain supported by the (200) plane linearly increases with pressure up to the highest pressures reached in this work (>60 GPa) and shows almost no change with metal composition. Because of the very different compression behavior in the (200) and (020) planes, change in the b/a ratio with pressure provides a unique way to visualize the onset of plastic behavior. This onset varies from ~15 GPa for samples with 5% Ta to more than 30 GPa for the sample with 50% Ta. Finally, the ambient bulk modulus of each solid-solution sample was determined using the second-order Birch-Murnaghan equation-of-state and found to be ~340 GPa for all phases.