Engineering Papers⌕ Search

Engineering topics

Wolverton, C.

Publications and source records attributed to Wolverton, C..

At least 55 records · Page 3

First-Principles Prediction of Intermediate Products in the Decomposition of Metal Amidoboranes

The non-volatile products remaining after the thermal decomposition of metal amidoboranes ([M]n+[NH2BH3] - , M = alkali or alkaline metal atom) are amorphous and incompletely characterized increasing the complexity of devising regeneration strategies for these potential hydrogen storage materials. Utilizing the combined prototype electrostatic ground state search (PEGS) and density-functional theory (DFT) methodology (PEGS+DFT), we have searched for crystal structures of possible intermediate phases with [NHBH2] - , [NBH] - , [N3H2B3H3] - , and polymer-M[NHBH2] anion groups in the decomposition of lithium amidoborane (LiAB) and calcium amidoborane (CaAB). All these potential reaction products are calculated to be significantly endothermic, in contrast to the experimentally measured nearly thermo neutral values [3 to 5 kJ/(mol H2) in LiAB and 3.5 kJ/(mol H2) in CaAB] suggesting that there are alternative products formed. The dianion group [NHBHNHBH3] 2- has recently been suggested to form in the decomposition of a calcium amidoborane complex in solution. In LiAB and CaAB, we use PEGS+DFT calculations to predict intermediate metal-dianion compounds, and the static H2 release enthalpy is 27.4 kJ/(mol H2) in LiAB and 27.3 kJ/(mol H2) in CaAB, respectively. Introducing vibrational effects by phonon calculations, the enthalpies are shifted down by a roughly constant amount, _25 kJ/(mol H2) at 0 K and _22 kJ/(mol H2) at 300 K. Thus, our theoretical H2 release enthalpies agree with the experimentally measured nearly thermo-neutral data in the decomposition of LiAB and CaAB. This agreement supports the existence of the dianion phases as products in the decomposition of metal amidoboranes. Then, using the dianion compound as an intermediate in the decomposition of MAB, we further study the stability trends of a series of MAB (M=Li, Na, K, Ca), and find that the reaction enthalpies generally obey the following trend: The amidoborane becomes more stable, i.e., MAB stability increases as the metal cation moves down in the periodic table along a given column (LiAB>NaAB>KAB), or as metal cation moves to the left along a given row (KAB>CaAB). T.A. acknowledges the Fuel Cell Technology Program at USDOE, Office of Energy Efficiency and Renewable Energy. Pacific Northwest National Laboratory is operated by Battelle for the US Department of Energy.

36 MATERIALS SCIENCE↗

First Principles Simulations of the Electrochemical Lithiation and Delithiation of Faceted Crystalline Silicon

Silicon is of significant interest as a next-generation anode material for lithium-ion batteries due to its extremely high capacity. The reaction of lithium with crystalline silicon is known to present a rich range of phenomena, including electrochemical solid state amorphization, crystallization at full lithiation of a Li15Si4 phase, hysteresis in the first lithiation–delithiation cycle, and highly anisotropic lithiation in crystalline samples. Very little is known about these processes at an atomistic level, however. To provide fundamental insights into these issues, we develop and apply a first principles, history-dependent, lithium insertion and removal algorithm to model the process of lithiation and subsequent delithiation of crystalline Si. The simulations give a realistic atomistic picture of lithiation demonstrating, for the first time, the amorphization process and hinting at the formation of the Li15Si4 phase. Voltages obtained from the simulations show that lithiation of the (110) surface is thermodynamically more favorable than lithiation of the (100) or (111) surfaces, providing an explanation for the drastic lithiation anisotropy seen in experiments on Si micro- and nanostructures. Analysis of the delithiation and relithiation processes also provides insights into the underlying physics of the lithiation–delithiation hysteresis, thus providing firm conceptual foundations for future design of improved Si-based anodes for Li ion battery applications.

Environmental Molecular Sciences Laboratory↗