Using atomic layer deposited tungsten to increase thermal conductivity of a packed bed

This study investigated the effective thermal conductivity (k{sub eff}) of packed-beds that contained porous particles with nanoscale tungsten (W) films of different thicknesses formed by atomic layer deposition (ALD). A continuous film on the particles is vital towards increasing k{sub eff} of the packed beds. For example, the k{sub eff} of an alumina packed bed was increased by three times after an ∼8-nm continuous W film with 20 cycles of W ALD, whereas k{sub eff} was decreased on a polymer packed bed with discontinuous, evenly dispersed W-islands due to nanoparticle scattering of phonons. For catalysts, understanding the thermal properties of these packed beds is essential for developing thermally conductive supports as alternatives to structured supports.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Enhanced Dry Reforming of Methane on Ni and Ni-Pt Catalysts Synthesized by Atomic Layer Deposition

Atomic layer deposition (ALD) was used to deposit Ni and Pt on alumina supports to form monometallic and bimetallic catalysts with initial particle sizes of 1–2.4 nm. The ALD catalysts were more active (per mass of metal) than catalysts prepared by incipient wetness (IW) for dry reforming of methane (DRM), and they did not form carbon whiskers during reaction due to their sufficiently small size. Catalysts modified by Pt ALD had higher rates of reaction per mass of metal and inhibited coking, whereas NiPt catalysts synthesized by IW still formed carbon whiskers. Temperature-programmed reduction of Ni catalysts modified by Pt ALD indicated the presence of bimetallic interaction. Density functional theory calculations suggested that under reaction conditions, the NiPt surfaces form Ni-terminated surfaces that are associated with higher DRM rates (due to their C and O adsorption energies, as well as the CO formation and CH4 dissociation energies).

Environmental Molecular Sciences Laboratory↗

Metal ferrite spinel energy storage devices and methods for making and using same

1-100 nm metal ferrite spinel coatings are provided on substrates, preferably by using an atomic layer deposition process. The coatings are able to store energy such as solar energy, and to release that stored energy, via a redox reaction. The coating is first thermally or chemically reduced. The reduced coating is then oxidized in a second step to release energy and/or hydrogen, carbon monoxide or other reduced species.

25 ENERGY STORAGE↗