Engineering PapersSearch

Engineering topics

Wei, W.

Publications and source records attributed to Wei, W..

PMT calibration for the JSNS^2-II far detector with an embedded LED system

The JSNS^2-II (the second phase of JSNS^2, J-PARC Sterile Neutrino Search at J-PARC Spallation Neutron Source) is an experiment aimed at searching for sterile neutrinos. Here, this experiment has entered its second phase, employing two liquid scintillator detectors located at near and far positions from the neutrino source. Recently, the far detector of the experiment has been completed and is currently in the calibration phase. The following properties of all functioning Photo-Multiplier-Tubes (PMTs) to detect the neutrino events in the far detector have been calibrated: PMT gain, its dependence of supplied High Voltage (HV), Peak-to-Valley (PV), and signal timing. This paper presents a detailed description of the calibration process utilizing the LED system. The LED system of the far detector uses two Ultra-Violet (UV) LEDs, which are effective in calibrating all of the PMTs at once. The UV light is converted into the visible light wavelengths inside liquid scintillator via the wavelength shifters, providing pseudo-isotropic light. To achieve a good energy resolution for physics events, a relative gain adjustment of up to 10% is required for all functioning PMTs. This will be achieved using the HV curves measured and the results of the LED calibration. The Peak-to-Valley (PV) ratio values, which distinguish the single photo-electron signal from the pedestal, are similar to those from the production company. Additionally, the precision of the PMT signal timing is measured to be 2.1 ns. This meets the event reconstruction requirement of 10 ns.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS

Muon tagging with flash ADC waveform baselines

Here, this manuscript describes an innovative method to tag muons using the baseline information of the Flash ADC (FADC) waveform of PMTs in the JSNS 2 (J-PARC Sterile Neutrino Search at J-PARC Spallation Neutron Source) experiment. The experiment is designed to search for evidence of sterile neutrinos, and a reliable method for muon tagging is an essential component for background rejection because the detector is located above ground, on the 3rd floor of the J-PARC Material and Life Science Experimental Facility (MLF). Cosmogenic muons that stop within the detector volume and produce a Michel electron are a particularly important background that must be rejected for our sterile neutrino search. Utilizing this innovative method, more than 99.8 % of Michel electrons can be rejected even without using information from the detector’s veto region PMTs. This technique can be employed by any experiments which uses a similar detector configuration.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS

Characterization of ion beam modified ceramic wear surfaces using Auger electron spectroscopy

An investigation of the surface chemistry and morphology of the wear surfaces of ceramic material surfaces modified by ion beam mixing has been conducted using Auger electron spectroscopy and secondary electron microscopy. Studies have been conducted on ceramic/ceramic friction and wear couples made up of TiC and NiMo-bonded TiC cermet pins run against Si3N4 and partially stabilized zirconia disc surfaces modified by the ion beam mixing of titanium and nickel, as well as ummodified ceramic/ceramic couples in order to determine the types of surface changes leading to the improved friction and wear behavior of the surface modified ceramics in simulated diesel environments. The results of the surface analyses indicate that the formation of a lubricating oxide layer of titanium and nickel, is responsible for the improvement in ceramic friction and wear behavior. The beneficial effect of this oxide layer depends on several factors, including the adherence of the surface modified layer or subsequently formed oxide layer to the disc substrate, the substrate materials, the conditions of ion beam mixing, and the environmental conditions.

Wei, W.

Friction and wear behaviour of ion beam modified ceramics

In the present study, the sliding friction coefficients and wear rates of carbide, oxide, and nitride materials for potential use as sliding seals (ring/liner) were measured under temperature, environmental, velocity, and loading conditions representative of a diesel engine. In addition, silicon nitride and partially stabilized zirconia discs were modified by ion mixing with TiNi, nickel, cobalt and chromium, and subsequently run against carbide pins, with the objective of producing reduced friction via solid lubrication at elevated temperature. Unmodified ceramic sliding couples were characterized at all temperatures by friction coefficients of 0.24 and above. However, the coefficient at 800 C in an oxidizing environment was reduced to below 0.1, for certain material combinations, by the ion implantation of TiNi or cobalt. This beneficial effect was found to derive from lubricious titanium, nickel, and cobalt oxides.

Lankford, J.

Sliding Seal Materials for Adiabatic Engines, Phase 2

An essential task in the development of the heavy-duty adiabatic diesel engine is identification and improvements of reliable, low-friction piston seal materials. In the present study, the sliding friction coefficients and wear rates of promising carbide, oxide, and nitride materials were measured under temperature, environmental, velocity, and loading conditions that are representative of the adiabatic engine environment. In addition, silicon nitride and partially stabilized zirconia disks were ion implanted with TiNi, Ni, Co, and Cr, and subsequently run against carbide pins, with the objective of producing reduced friction via solid lubrication at elevated temperature. In order to provide guidance needed to improve materials for this application, the program stressed fundamental understanding of the mechanisms involved in friction and wear. Electron microscopy was used to elucidate the micromechanisms of wear following wear testing, and Auger electron spectroscopy was used to evaluate interface/environment interactions which seemed to be important in the friction and wear process. Unmodified ceramic sliding couples were characterized at all temperatures by friction coefficients of 0.24 and above. The coefficient at 800 C in an oxidizing environment was reduced to below 0.1, for certain material combinations, by the ion implanation of TiNi or Co. This beneficial effect was found to derive from lubricious Ti, Ni, and Co oxides.