Phase patterning of metallic glasses through superfast quenching of ion irradiation-induced thermal spikes

Amorphous metallic glasses (MGs) convert to crystalline solids upon annealing at a high temperature. Such a phase change, however, does not occur with the local melting caused by damage cascades introduced by ion irradiation, although the resulting thermal spikes can reach temperatures > 1000 K. This is because the quenching rate of the local melting zone is several orders of magnitude higher than the critical cooling rate for MG formation. Thus the amorphous structure is sustained. This mechanism increases the highest temperature at which irradiated MG sustains amorphous phase. More interestingly, if an irradiated MG is pre-annealed to form a polycrystalline structure, ion irradiation can locally convert this crystalline phase to an amorphous phase if the grains are nanometers in size and comparable to the damage cascade volume size. Combining pre-annealing and site selective ion irradiation, patterned crystalline-amorphous heterogeneous structures have been fabricated. This finding opens new doors for various applications.

36 MATERIALS SCIENCE↗

A quantitative study of retention and release of deuterium and tritium during irradiation of y-LiAlO2 pellets

This study reports on the quantification of deuterium in ion-irradiated gamma-LiAlO2 pellets as a function of dose and temperature. The gamma-LiAlO2 pellets were sequentially irradiated with He+ and D2+ ions to the same fluences of 5E16, 1E17 and 2E17 He++D+/cm2 at 188 K. Additional irradiation was performed to 1E17, 2E17 and 4E17 He++D+/cm2 at 573 K. A set of the pellets irradiated at 188 K was shipped and stored at low temperatures from 80 to 132 K and characterized using time-of-flight secondary ion mass spectrometry at ~173 K. The deuterium depth profiles show a Gaussian-like distribution in the low-temperature pellets. The total deuterium retention is found to be directly proportional to the ion fluence. About 27 at.% of the implanted deuterium atoms were released from the pellet irradiated to 2E17 He++D+/cm2 at 188 K during storage at room temperature for ~1 month. Retention of the trapped or bound deuterium during ion irradiation at 573 K increases initially with ion fluence and tends to saturate at a high fluence. The amount of the released deuterium is observed to be quantitatively consistent with that of the released tritium from similar standard pellets during neutron irradiation at 573 K.

Deuterium retention and release, ion irradiation, ↗

Irradiation-induced swelling of pure chromium with 5 MeV Fe ions in the temperature range 450–650 °C

A surface coating using pure chromium has been proposed to increase the accident tolerance of Zircaloy cladding in pressurized water reactors. However, there is not much irradiation experience with Cr alloys and especially pure Cr. In the present study, pure chromium was irradiated with 5 MeV Fe ions to 50 peak dpa (displacements per atom) at temperatures of 450, 500, 550, 600 and 650 °C. Then irradiation at the peak swelling temperature of 550 °C was conducted to 50, 100, 150 peak dpa. Swelling at 50 dpa was observed over the entire temperature range studied, 450–650 °C, but appeared to be decreasing strongly at the temperature boundaries of the experiment. After an initial transient of rapid swelling, chromium was observed to swell at a rate of ~0.03–0.04%/dpa (up to 120 local dpa), which is much lower than pure Fe at 0.2%/dpa. This low swelling rate was found to be relatively insensitive to dpa rate, which varied by a factor of ~2 over the depth of data collection. Here, swelling was observed to begin quickly with an incubation period less than 10 dpa. Self-organization in the form of void ordering was observed to be developing at 50 dpa, becoming better defined with increasing dose. The void alignment direction is determined to be the $\langle$111$\rangle$ axial direction.

36 MATERIALS SCIENCE↗

Strain modulation using defects in two-dimensional MoS 2

We investigate the nature of strain in MoS 2 and correlate it to defect types and densities, while systematically assessing the tolerance of this low dimensional material to He and Au ion irradiations. Through a series of theoretical predictions and experimental observations, we establish the onset of the crystalline-to-amorphous transition in MoS 2 and identify sulfur vacancies as the most favorable defects introduced during irradiation. We note the presence of both tensile and compressive strains, which depend on the types of defects introduced into the lattice and vary with increasing fluence. In conclusion, the results show that defects can be used to tune strain in two-dimensional materials and provide an exciting pathway for using external stimuli to control properties of low dimensional materials.

2-dimensional systems↗

Radiation response of FeCrAl-coated Zircaloy-4

Coating the surface of Zircaloy-4 light water reactor fuel cladding tube is of considerable interest for enhancing its accident tolerance. In this study, thermal annealing of FeCrAl-coated Zircaloy-4 at 725 °C for 500 h, was used to induce interfacial reactions between Zircaloy-4 and FeCrAl. The interface zones were then irradiated by 3.5 MeV Zr ions at 400 °C, up to 50, 100, 150 peak dpa values. Transmission electron microscopy (TEM) and scanning TEM were used to characterize microstructural and composition changes before and after ion irradiation. Three interfacial phases were identified: FeZr 3 , (Fe,Cr) 2 Zr, and ZrC. The widest intermetallic layer, FeZr3, had large grains. The narrower phases, (Fe,Cr)2Zr and ZrC, contained small grains and were often mixed. The unexpected observation of the ZrC phase was attributed to the presence of very small impurity level concentrations of carbon in the powder material. No void swelling was observed in any of the phases, including the FeCrAl coating and Zircaloy-4 substrate. (Fe,Cr) 2 Zr, however, fully amorphized after irradiation, even at the lowest dpa.

36 MATERIALS SCIENCE↗

Ni coating on 316L stainless steel using cage plasma treatment: Feasibility and swelling studies

A modified cage plasma nitriding technique is used to coat a Ni film onto a 316L substrate as a protective layer for austenitic steels in molten fluoride salts. The coating is achieved by deposition of Ni atoms sputtered from a Ni cage with a 316L substrate floated at the same potential as the cage to reduce plasma sputtering on the substrate. The Ni coating is porosity-free and precipitation-free and forms a γ-(Fe, Ni) phase due to interdiffusion from the substrate. Beneath the interdiffusion layer exists a thick γ-phase layer mainly affected by long-range nitrogen diffusion along the grain boundary. This layer develops grain boundary Cr nitride precipitates. Ion irradiation on the polished cross-section of the plasma-treated sample shows no void swelling in the surface-deposited Ni layer, very limited void formation in N diffusion layer, and significant void swelling in bulk unaffected by nitrogen. The studies demonstrate the feasibility of the technique for Ni coating and show good swelling resistance of the coating layer and N diffusion-affected layer. Mechanisms are discussed in this paper.

36 MATERIALS SCIENCE↗

Effect of helium on dispersoid evolution under self-ion irradiation in a dual-phase 12Cr oxide-dispersion-strengthened alloy

As one candidate alloy for future Generation IV and fusion reactors, a dual-phase 12Cr oxide-dispersion-strengthened (ODS) alloy was developed for high temperature strength and creep resistance and has shown good void swelling resistance under high damage self-ion irradiation at high temperature. However, the effect of helium and its combination with radiation damage on oxide dispersoid stability needs to be investigated. In this study, 120 keV energy helium was preloaded into specimens at doses of 1 × 10 15 and 1 × 10 16 ions/cm 2 at room temperature, and 3.5 MeV Fe self-ions were sequentially implanted to reach 100 peak displacement-per-atom at 475 °C. He implantation alone in the control sample did not affect the dispersoid morphology. After Fe ion irradiation, a dramatic increase in density of coherent oxide dispersoids was observed at low He dose, but no such increase was observed at high He dose. The study suggests that helium bubbles act as sinks for nucleation of coherent oxide dispersoids, but dispersoid growth may become difficult if too many sinks are introduced, suggesting that a critical mass of trapping is required for stable dispersoid growth.

36 MATERIALS SCIENCE↗

Development of a Faraday cup fast ion loss detector for keV beam ions

The development and testing of a Faraday cup fast-ion loss detector capable of measuring sub 100 keV particles is documented. Such measurement capabilities play an important role in the assessment of particle confinement of nuclear fusion experiments. The detector is manufactured using thin-film deposition techniques, building upon previous work using discrete foils. This new manufacturing method allows the form factor of the sensor to become that of essentially a microchip. Analysis of the diagnostic response is performed using Monte-Carlo particle simulations. These simulations show peaks in the detector response at 40 and 70 keV. The sensor is then tested in a tunable linear accelerator capable of accelerating protons from 20 to 120 keV. Finally, the detector response was found to be well matched to simulations. Improvements to the design to facilitate robustness are discussed.

47 OTHER INSTRUMENTATION↗

Radiation response of Ti 2 AlC MAX phase coated Zircaloy-4 for accident tolerant fuel cladding

A Ti 2 AlC MAX phase material was deposited on Zircaloy-4 substrate using the cold spray process, with the goal of enhancing the accident tolerance of zirconium-alloy fuel cladding in light water reactors. The samples were annealed up to 923 K to study the intermetallic phase formation between the coating and Zircaloy-4 substrate. Three interface compounds, ZrAl 2 , ZrAl, and Zr 3 Al, were identified and the activation energy of the interfacial intermetallic compound growth was determined. The radiation response of the coating material and interfacial intermetallic compounds after 3.5 MeV Zr 2+ ion irradiation was investigated by transmission electron microscopy and nanoindentation. Ion irradiation disrupted the nanolamellar structure of the Ti 2 AlC coating while amorphization was observed some of the intermetallic compounds. Furthermore, nanoindentation revealed overall hardening of the Ti 2 AlC coating and Zr 3 Al phase, with no significant change observed in the ZrAl 2 and ZrAl phases.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Radiation Tolerance in Nano-Structured Crystalline Fe(Cr)/Amorphous SiOC Composite

The management of irradiation defects is one of key challenges for structural materials in current and future reactor systems. To develop radiation tolerant alloys for service in extreme irradiation environments, the Fe self-ion radiation response of nanocomposites composed of amorphous silicon oxycarbide (SiOC) and crystalline Fe(Cr) were examined at 10, 20, and 50 displacements per atom damage levels. Grain growth in width direction was observed to increase with increasing irradiation dose in both Fe(Cr) films and Fe(Cr) layers in the nanocomposite after irradiation at room temperature. However, compared to the Fe(Cr) film, the Fe(Cr) layers in the nanocomposite exhibited ~50% less grain growth at the same damage levels, suggesting that interfaces in the nanocomposite were defect sinks. Moreover, the addition of Cr to α-Fe was shown to suppress its grain growth under irradiation for both the composite and non-composite case, consistent with earlier molecular dynamic (MD) modeling studies.

36 MATERIALS SCIENCE↗

Resistance to Helium Bubble Formation in Amorphous SiOC/Crystalline Fe Nanocomposite

The management of radiation defects and insoluble He atoms represent key challenges for structural materials in existing fission reactors and advanced reactor systems. To examine how crystalline/amorphous interface, together with the amorphous constituents affects radiation tolerance and He management, we studied helium bubble formation in helium ion implanted amorphous silicon oxycarbide (SiOC) and crystalline Fe composites by transmission electron microscopy (TEM). The SiOC/Fe composites were grown via magnetron sputtering with controlled length scale on a surface oxidized Si (100) substrate. These composites were subjected to 50 keV He+ implantation with ion doses chosen to produce a 5 at% peak He concentration. TEM characterization shows no sign of helium bubbles in SiOC layers nor an indication of secondary phase formation after irradiation. Compared to pure Fe films, helium bubble density in Fe layers of SiOC/Fe composite is less and it decreases as the amorphous/crystalline SiOC/Fe interface density increases. Our findings suggest that the crystalline/amorphous interface can help to mitigate helium defect generated during implantation, and therefore enhance the resistance to helium bubble formation.

36 MATERIALS SCIENCE↗

Helium Irradiation and Implantation Effects on the Structure of Amorphous Silicon Oxycarbide

Despite recent interest in amorphous ceramics for a variety of nuclear applications, many details of their structure before and after irradiation/implantation remain unknown. Here we investigated the short-range order of amorphous silicon oxycarbide (SiOC) alloys by using the atomic pair-distribution function (PDF) obtained from electron diffraction. The PDF results show that the structure of SiOC alloys are nearly unchanged after both irradiation up to 30 dpa and He implantation up to 113 at%. TEM characterization shows no sign of crystallization, He bubble or void formation, or segregation in all irradiated samples. Irradiation results in a decreased number of Si-O bonds and an increased number of Si-C and C-O bonds. This study sheds light on the design of radiation-tolerant materials that do not experience helium swelling for advanced nuclear reactor applications.

36 MATERIALS SCIENCE↗