Electrolyte Study for High-Nickel LiNi 0.9 Mn 0.05 Co 0.05 O 2 Cathodes

With an increasing demand for intermittent renewable energy and electric vehicles, it is imperative to develop lithium-ion batteries with Earth-abundant cathode materials. Cobalt (Co) is preferred to be kept at a minimum because of its high cost and limited mining options, yet it has played an essential role in the high-performance transition metal oxides (TMOs). Herein, we report work from Argonne National Laboratory, conducted under the U.S. DoE's Vehicle Technologies Office, Deep Dive consortium on Next-Generation Cathodes, to optimize electrolytes for LiNi 0.9 Mn 0.05 Co 0.05 O 2 . LiNi 0.9 Mn 0.05 Co 0.05 O 2 is a high-Ni TMO benchmark as it outperforms most other TMOs under standard cycling conditions. In this study, we use the figure-of-merit approach to optimize electrolytes for this novel cathode material. Dual-salt carbonate electrolytes containing lithium difluorooxyphosphate and hexafluorophosphates were found to be the best for capacity retention and slowing the impedance rise. Importantly, transition metal dissolution and lithium inventory losses in the solid electrolyte interface were found to be the major causes for capacity fade.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Evolution of LiNi 0.5 Mn 0.3 Co 0.2 O 2 Particle Damage from Fast Charging in Optimized, Full Li-Ion Cells

Fast charging batteries are critical to the widespread adoption of electric vehicles to compete with refueling times of combustion-based vehicles. In the near term, adapting current commercial battery technologies to perform better under fast charging conditions through engineering optimizations will greatly expedite the process while exploratory fast-charging electrode materials are being pursued. To do so, the degradation modes in optimized Li-ion batteries need to be completely explored to understand fast charging limits while maintaining a high energy density and a long cycle life. While lithium plating on graphite still remains a challenge, cathode degradation also plays a key role in battery performance. In this work, we used nano- and micro-X-ray computed tomography to characterize the mechanical degradation of LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) in optimized Li-ion batteries cycled at three rates, 1C, 6C, and 9C, and at different stages of cycle life, 225 and 600 cycles. We report despite using a conservative upper voltage cutoff limit aimed to minimize extensive cathode degradation, higher charging rates and increased cycling caused the polycrystalline NMC532 particles to fracture and pulverize, which likely drives cathode capacity fade and contributes to the decrease in overall cell performance.

25 ENERGY STORAGE↗

Exploring the Promise of Multifunctional “Zintl-Phase-Forming” Electrolytes for Si-Based Full Cells

Li-M-Si ternary Zintl phases have gained attention recently due to their high structural stability, which can improve the cycling stability compared to a bulk Si electrode. Adding multivalent cation salts (such as Mg 2+ and Ca 2+ ) in the electrolyte was proven to be a simple way to form Li-M-Si ternary phases in situ in Si-based Li-ion cells. To explore the promise of Zintl-phaseforming electrolytes, we systematically investigated their application in pouch cells via electrochemical and multiscale postmortem analysis. The introduction of multivalent cations, such as Mg 2+ , during charging can form Li x M y Si ternary phases. They can stabilize Si anions and reduce side reactions with electrolyte, improving the bulk stability. More importantly, Mg 2+ and Ca 2+ incorporate into interfacial side reactions and generate inorganic-rich solid- electrolyte interphase, thus enhancing the interfacial stability. Therefore, the full cells with Zintl-phase-forming electrolytes achieve higher capacity retentions at the C/3 rate after 100 cycles, compared to a baseline electrolyte. Additionally, strategies for mitigating the electrode-level fractures of Si were evaluated to make the best use of Zintl-phase-forming electrolytes. In conclusion, this work highlights the significance of synergistic impact of multifunctional additives to stabilize both bulk and interface chemistry in high-energy Si anode materials for Li-ion batteries.

25 ENERGY STORAGE↗

Simultaneous neutron and X-ray tomography for visualization of graphite electrode degradation in fast-charged lithium-ion batteries

Advanced battery characterization using neutron and X-ray-based imaging modalities is crucial to reveal fundamental degradation modes of lithium-ion batteries (LIBs). Taking advantage of the sensitivity of neutrons to some low-Z (Li) and X-rays to high-Z materials (Cu), here we demonstrate the viability of simultaneous neutron and X-ray tomography (NeXT) as a non-destructive imaging platform for ex-situ 3D visualization of graphite electrode degradation following extreme fast charging (XFC). In addition, we underscore the benefits of the simultaneous of NeXT by combining the neutron and X-ray tomography data from the same sample location for material identification and segmentation of one pristine and two XFC-cycled graphite electrodes (9C charge for 450 cycles). Our ex-situ results and methodology development pave the way for the design of NeXT-friendly LIB geometries that will allow operando and/or in-situ 3D visualization of electrode degradation during XFC.

25 ENERGY STORAGE↗

Extreme Fast Charging: Effect of Positive Electrode Material on Crosstalk

Extreme fast charging (XFC) is a key requirement for the adoption of battery-based electric vehicles by the transportation sector. However, XFC has been shown to accelerate degradation, causing the capacity, life, and safety of batteries to deteriorate. We tested cells containing five positive electrode chemistries, LFP (olivine structure), LMO (spinel), LCO (layered), NMC811 (layered) and NCA (layered), using fast-charging protocols. After testing, the negative electrodes from cells containing positive electrodes crystallizing with a layered structure were found to have more lithium deposited on their surfaces. Further, those crystallizing with a layered structure also tended to have a larger increase in impedance than those crystallizing with a spinel or olivine structure. Characterization of the negative electrodes by X-ray photoelectron spectroscopy showed that using the concentrations of LiF and Li x PO y F z as metrics, the concentration of LiF in the SEI from the cell with different positive electrodes is LFP > LMO > LCO ~ NMC811 > NCA; and for Li x PO y F z , the order is LMO > LFP > NCA > NMC811 > LCO. Clearly, the positive-electrode material was influencing the amounts of these materials formed.

25 ENERGY STORAGE↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Fast charging of Li-ion cells: Effect of separator membranes and mapping of “safe lines” to avoid Li plating

An experimental method is introduced that uses microprobe Li/Cu reference electrodes to map "safe" charging regimes to avoid Li metal plating on graphite anodes at rates to 8C. With this method, a Li-ion cell closely approaches the Li plating condition but avoids descending into this regime. This "safe" approach is used to demonstrate effects of the microporous separator on Li plating in cells consisting of a layered nickel-manganese -cobalt oxide cathode and graphite anode. We argue that most of the difference in behaviors for different separators arises from time delayed Li + ion percolation through the membrane. In conclusion, our study suggests that explicitly treating kinetics of phase transitions in the lithiated graphite anode is essential for electrochemical models predicting "safe" lines for fast charging cells.

25 ENERGY STORAGE↗

Extreme fast charge aging: Effect of electrode loading and NMC composition on inhomogeneous degradation in graphite bulk and electrode/electrolyte interface

Empowering extreme fast charging (XFC) requires a comprehensive understanding of its application with advanced anode and cathode materials in lithium-ion batteries. No report exists for the full extent of limitations for the anode with crosstalk effect from paired cathode as well as Li plating due to electrode loading under XFC. In this study, a combination of cell testing and multiple length characterization is used to investigate XFC aging mechanism in cells with a low loading of 1.5 mAh cm -2 and high loading of 2.5 mAh cm -2 for graphite (Gr)/Ni-rich LiNi x Mn y Co 1-x-y O 2 (NMCs). Operando XRD mappings show 1.5 mAh cm -2 loadings result in higher strain in graphite for all three cathode types. Among the three NMC cathodes, the graphite from NMC532 and NMC811 cells show comparable strain. Scanning electron microscopy (SEM) images show distinct differences between 6-C-charged anodes in two loadings. Significantly increased electrode thickness can be seen due to more damage in the graphite bulk and accumulation of the electrolyte decomposition products in electrode pores. X-ray photoelectron spectroscopy (XPS) reveals both cathode chemistry and Li plating influence the non-uniform SEI composition on graphite surface. We report higher Ni content in NMC811 promotes the higher levels of salt decomposition on the SEI and formation of higher mass of electrolyte aging products.

25 ENERGY STORAGE↗

Compositionally complex doping for zero-strain zero-cobalt layered cathodes

We report the high volatility of the price of cobalt and the geopolitical limitations of cobalt mining have made the elimination of Co a pressing need for the automotive industry. Owing to their high energy density and low-cost advantages, high-Ni and low-Co or Co-free (zero-Co) layered cathodes have become the most promising cathodes for next-generation lithium-ion batteries. However, current high-Ni cathode materials, without exception, suffer severely from their intrinsic thermal and chemo-mechanical instabilities and insufficient cycle life. Here, in this paper, by using a new compositionally complex (high-entropy) doping strategy, we successfully fabricate a high-Ni, zero-Co layered cathode that has extremely high thermal and cycling stability. Combining X-ray diffraction, transmission electron microscopy and nanotomography, we find that the cathode exhibits nearly zero volumetric change over a wide electrochemical window, resulting in greatly reduced lattice defects and local strain-induced cracks. In-situ heating experiments reveal that the thermal stability of the new cathode is significantly improved, reaching the level of the ultra-stable NMC-532. Owing to the considerably increased thermal stability and the zero volumetric change, it exhibits greatly improved capacity retention. This work, by resolving the long-standing safety and stability concerns for high-Ni, zero-Co cathode materials, offers a commercially viable cathode for safe, long-life lithium-ion batteries and a universal strategy for suppressing strain and phase transformation in intercalation electrodes.

25 ENERGY STORAGE↗

Li-Ion Battery Electrode Contact Resistance Estimation by Mechanical Peel Test

Li-ion battery electrode electronic properties, including bulk conductivity and contact resistance, are critical parameters affecting cell performance and fast-charge capability. Contact resistance between the coating and current collector is often the largest electronic resistance in an electrode and is affected by chemical, microstructural, and interfacial variations. Direct measurements of contact resistance and bulk conductivity have proven to be challenging. In their absence, a mechanical electrode peel test is often used to compare adhesion and electrical contact resistance. However, using a micro-flexible-surface probe, contact resistance can be directly determined. Here, this work compares contact resistance and mechanical peel strength of multiple commercial-grade HE5050 and NCM523 cathodes and graphite and silicon anodes. It was found that peel strength correlates well with contact resistance in a carefully curated data set (p < 0.05) and in some situations may be a good metric to estimate electrical properties. However, there were distinct outliers in the data set, indicating that peel strength may not accurately reflect electrical properties when there is significant variation in electrode composition. These results illustrate the value of the micro-flexible-surface probe in quantifying contact resistance and bulk conductivity to better understand how battery composition and processing steps affect microstructure and resulting cell performance.

25 ENERGY STORAGE↗

Batteries (2021 Annual Progress Report)

This document summarizes the progress of VTO battery R&D projects supported during the fiscal year 2021 (FY 2021). In FY 2021, the DOE VTO battery R&D funding was approximately $\$$115 million. Its R&D focus was on the development of high-energy batteries for EVs as well as very high-power devices for hybrid vehicles. The electrochemical energy storage roadmap (which can be found at the EERE Roadmap web page2) describes ongoing and planned efforts to develop electrochemical storage technologies for EVs. To advance battery technology, which can in turn improve market penetration of PEVs, the program investigates various battery chemistries to overcome specific technical barriers, e.g., battery cost, performance, life (both the calendar life and the cycle life), its tolerance to abusive conditions, and its recyclability/sustainability. VTO R&D has had considerable success, lowering the cost of EV battery packs to $\$$185/kWh in 2019 (representing more than 80% reduction since 2008) yet even further cost reduction is necessary for EVs to achieve head-to-head cost competitiveness with ICEs (without Federal subsidies). In addition, today’s batteries also need improvements in such areas as their ability to accept charging at a high rate, referred to as extreme fast charging (XFC) (15 minute charge) – to provide a “refueling” convenience similar to ICEs, and the ability to operate adequately at low temperatures. Research into “next-gen lithium-ion” batteries which would provide such functionalities is one of the R&D focus areas. VTO is funding research on both “next gen” chemistries (which employ an alloy anode and/or a high voltage cathode) and beyond lithium-ion (BLI) chemistries (which can, for example, employ a lithium metal anode).

25 ENERGY STORAGE↗

Evaluating the Effect of Electrolyte Additive Functionalities on NMC622/Si Cell Performance

Unstable electrode/electrolyte interface is the major cause of degradation for silicon (Si)-based anodes for lithium (Li)-ion batteries. Development of functional electrolyte additives can provide a viable path toward stabilizing the dynamic Si/electrolyte interface, which will benefit the development of high energy density Li-ion batteries. Here, we evaluate polymerizable electrolyte additives with varying functional groups (fluorocarbon, thiophosphate, and fluorophosphazene). The additives are examined using LiNi 0.6 Mn 0.2 Co 0.2 O 2 /Si full cells where the cycle performance and impedance are measured. Electrochemical tests show that the fluorine-containing additives provide better passivation at the Si electrode, leading to enhanced full cell performance. Here, among the three additives examined, best electrochemical performance is observed from the fluorocarbon-containing compound, followed by fluorophosphazene- and thiophosphate-containing compounds. Characterization of the solid electrolyte interphase (SEI) on cycled electrodes using Auger electron spectroscopy (AES), X-ray photoelectron spectroscopy (XPS), and attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR) reveal that higher concentration of fluorine and lithium oxide, and lower concentration of carbonate and organic species correlate with enhanced electrochemical performance.

25 ENERGY STORAGE↗

A Comprehensive Understanding of the Aging Effects of Extreme Fast Charging on High Ni NMC Cathode

As the battery industry shifts toward high Ni content cathodes, such as LiNi 0.8 Mn 0.1 Co 0.1 O 2 [NMC811], a complete understanding of the degradation mechanisms of NMC811 under extreme fast charging (XFC) (XFC, ≤10–15 min charging) conditions is needed. Such comprehensive understanding would identify the most critical materials gaps that need to be addressed for enabling XFC long-life cells for electric vehicles. This study maps out the key aging mechanisms for NMC811 cycled at different XFC conditions (between 1C and 9C) for up to 1000 cycles. To acquire a fundamental understanding of utilization and degradation, cells are evaluated using a range of electrochemical techniques, and multimodal and multiscale microscopy techniques to quantify chemical, structural, and crystallographic degradation as a function of cycling conditions for the NMC cathode. When comparing NMC811 to NMC532, it is observed that NMC811 has a greater subsurface crystallographic degradation and displays a similar magnitude of subparticle cracking. However, the NMC811 maintains superior performance despite those advanced degradations. Here, the superior cycle life performance is attributed to the NMC811 particles having radially oriented grains and improved transport properties. NMC811 shows between 4.6× and 3.15× reduction in capacity fade than NMC532 for charging rates between 4C (e.g., 15-min charging) and 6C (10-min charging).

25 ENERGY STORAGE↗

Concealed Cathode Degradation in Lithium-Ion Cells with a Ni-Rich Oxide

Difficulties with sourcing cobalt and the interest in increasing cell energy have motivated the development of Ni-rich oxide materials for lithium-ion battery cathodes. Despite the intense research on the topic, there is limited information available on the long-term performance of novel cathode formulations. Here, we evaluate the stability of LiNi 0.9 Mn 0.05 Co 0.05 O 2 in full-cells tested for over five months, assessing how cycling, voltage and electrolyte additives impact cathode aging. We use differential voltage analysis to extract insights about the cathode from the full-cell data and identify the isolation of cathode particles in the delithiated (charged) state as a relevant mode of aging. Importantly, this particular mechanism of cathode aging does not cause immediate cell capacity fade, causing the simple analysis of cell capacity retention to overestimate the cathode stability under the investigated conditions. So, our observations serve as cautionary tale indicating that careful analysis of data from extended testing may be required for assessing the performance of Ni-rich cathodes and for evaluating how these materials are affected by electrolyte additives.

25 ENERGY STORAGE↗

Understanding the Effect of Cathode Composition on the Interface and Crosstalk in NMC/Si Full Cells

Crosstalk between the cathode and the anode in lithium-ion batteries has a great impact on performance, safety, and cycle lifetime. Still, no report exists for a systematic investigation on crosstalk behavior in silicon (Si)-based cells as a function of transition metal composition in cathodes. We studied the effect of crosstalk on degradation of Si-rich anodes in full cells with different cathodes having the same crystal structure but different transition metal compositions, such as LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NM111), LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532), and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811). We found that the transition metal composition in cathodes, especially Mn ion concentration, significantly affects electrolyte decomposition reactions, even from very early cycles. This change causes differences in the solid electrolyte interphase (SEI) chemistry of each aged Si sample. As a result, each of the aged Si samples has a different electrochemistry, in terms of initial Coulombic efficiency and the mechanism of capacity fade.

25 ENERGY STORAGE↗

Evaluating the roles of electrolyte components on the passivation of silicon anodes

A protocol was recently developed to compare calendar life using a constant potential while monitoring the electrical current required to maintain the potential. Here, this calendar life protocol is used with electrolyte formulations containing various mole fractions of ethylene carbonate (EC), ethyl methyl carbonate (EMC), and LiPF 6 to elucidate the role each component plays in passivation for high silicon anodes. Together, EC and LiPF 6 lead to higher currents, and thus poorer passivation, whereas EMC acts as a spectator. The variation of the components' mole fraction also changes the solid-electrolyte interphase (SEI) composition, as measured by x-ray photoelectron spectroscopy. Importantly, higher LiPF 6 content leads to increased LiF as well as increased current, indicating that higher LiF content does not enhance the passivation of the silicon surface. Finding that EC did not yield a passivating SEI, instead ethylene sulfite, sulfolane, and propylene carbonate (PC) were used in place of EC. Using ethylene sulfite and sulfolane resulted in poorer passivation compared to EC, whereas PC resulted in superior passivation. As a result, the superior passivation may be related to more stable lithium-solvent complexes.

25 ENERGY STORAGE↗

Influence of metallic contaminants on the electrochemical and thermal behavior of Li-ion electrodes

Emerging nondestructive (direct) recycling techniques for lithium-ion batteries may introduce metallic impurities into recycled electrodes. In the present work, the impact of such nonionic contaminants on the practical performance of both anode and cathode materials is evaluated using a synergistic combination of electrochemical and thermal analysis. The impurities under study have been selected through evaluation of industrially shredded batteries, and include Fe0, Al0, Mg0, Cu0, and Si0. The electrochemical behavior of materials containing each individual contaminant at either the anode or the cathode is evaluated in both half-cell and full-cell format. Further, the first-cycle thermal signatures of full cells are used to validate and complement electrochemical signatures, and the two techniques are used in conjunction to suggest distinct mechanisms of electrochemical reactivity for the various impurities. At the anode, metallic contaminants are found to disrupt performance through direct reaction with Li and may serve as weak catalysts to accelerate electrolyte degradation. At the cathode, metallic contaminants show evidence of crossover during formation cycling to disrupt SEI formation. We suggest that coupled electrochemical and thermal analysis may be used to both identify the presence of contaminants and to elucidate specific mechanisms of reactivity for metallic impurities under anodic and cathodic conditions.

Contaminant↗

Extreme fast charge aging: Correlation between electrode scale and heterogeneous degradation in Ni-rich layered cathodes

Extreme fast charging (XFC) is a key requirement for the adoption of battery-based electric vehicles by the transportation sector. However, XFC has been shown to accelerate degradation, causing the capacity, life, and safety of batteries to deteriorate. There are no systematic studies in the open literature regarding aging modes in Ni-rich Li y Ni 0.a Mn 0.b Co 0.c O 2 (NMCabc) cathodes caused by fast charging. Herein, we report the effects of cathode composition and electrode loading in pouch cells containing NMC532, 622 and 811 paired with graphite and cycled under XFC conditions. The relative anisotropic volume change in the unit cell increases with Ni content in low-loading cells, while it levels up for all three NMC cathodes in high-loading cells because of substantial Li plating. The amounts of lithium plating and heterogeneity on the anode, determined by crystallographic phase quantification, were found to be correlated with electrode loading and cathode heterogeneity. The concentrations of the transition metals deposited on the anodes depend on NMCabc composition in a complex way. More particle cracking and surface degradation was found in NMC811. Here, the findings in this work provide a new understanding of the failure mechanisms and their practical implications for compositional tuning of future high-Ni NMCabc cathode materials during fast charging.