Soiling, cleaning, and abrasion: The results of the 5-year photovoltaic glass coating field study
Not Available
Engineering topics
Publications and source records attributed to To, Bobby.
Not Available
External contamination ("soiling") of the incident surface is a major limiting factor for solar technologies. A 5-year field glass coupon study was conducted to better understand external contamination and its effects; compare cleaning methods and the use of preventative coatings; and explore the abrasion resulting from cleaning to advise on accelerated abrasion testing. Test sites included the cities of Dubai (UAE), Kuwait City (Kuwait), Mesa (AZ), Mumbai (India), and Sacramento (CA). Through the 5-year cumulative study, dry brush, water spray, and wet sponge and squeegee cleaning methods were compared to no cleaning. Optical microscopy was used to obtain images, including representative color images, grayscale images for object analysis, and oblique images for coating integrity assessment. A thresholding protocol was developed to analyze and distinguish specimens using the ImageJ software. Optical performance was quantified using a spectrophotometer, including comprehensive optical characterization (transmittance, reflectance, and absorptance in addition to forward- and back-scattering). Atomic force microscopy was used to verify the abrasion damage morphology, including the width and depth of surface scratches. Analysis of the results included correlation of optical performance and particle area coverage, rank order (by coating or location), and the acceleration factor for abrasion damage. The efficacy of external cleaning was more readily distinguished from the effectiveness of antisoiling coatings. The acceleration factor for dry brush cleaning of a porous silica coating was found to be on the order of unity.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector, and discrete fuse components. In this study, unused field-vintage specimens are examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for the C-AST chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen current, voltage, and temperature. A significant increase in operating temperature (~100 degrees C from ~40 degrees C) and a different failure mode were observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow for failure analysis, including the extraction of the internal convolute springs for morphological examination (optical and electron microscopy).
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector, and discrete fuse components. Previous papers and presentations have focused on the development of the test method using a benchtop prototype. This presentation covers the early results of C-AST aging of static and dynamic specimens.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include: offline-modules, -strings, -inverters; system shutdown; arc-faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector, and discrete fuse components. Unused field-vintage specimens are presently being examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for the C-AST chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen: current, voltage, and temperature. A significant increase in operating temperature, ~100 deg C from ~40 deg C, and a different failure mode was observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow failure analysis, including the extraction of the internal convolute springs for morphological examination (optical- and electron-microscopy).
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were, therefore, examined, consisting of cable connector, branch connector, and discrete fuse components. In this study, unused field-vintage specimens are examined using a benchtop prototype fixture to identify the most influential environmental stressors on BoS components as well as the effect of external mechanical perturbation. The prototype fixture was used to develop a perturbation capability for future use in the combined-accelerated stress testing chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen current, voltage, and temperature. A significant increase in operating temperature (~100 °C from ~40 °C) and a different failure mode (arcing at the metal pins rather than overheating of the fuse filament) were observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (measured for static specimens, with failure occurring in the fuses) to 15 A (for tests with mechanical perturbation, with failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow for failure analysis, including the extraction of the internal convolute springs for morphological examination (optical and electron microscopy). Chemical composition analysis included energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include: offline-modules, -strings, -inverters; system shutdown; arc-faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector and discrete fuse components. Unused field-vintage specimens are presently being examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for C-AST. The benchtop experiments were also used to develop the in-situ data acquisition of specimen: current, voltage, and temperature. A significant increase in operating temperature, ~100 deg C from ~40 deg C, and a different failure mode was observed immediately once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure occurring in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow failure analysis, including the extraction of the internal convolute springs for morphological examination (optical- and electron-microscopy). Chemical composition analysis included: energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.
IEC 62788-7-3 was published on February 22, 2022. This presentation will discuss and try to understand how and why the methods became prescribed, and gather feedback on abrasives and characterization used with abrasion tests. The presentation will also cover the methods of linear brush test, rotary brush test, falling sand test, and forced sand impingement test.
Not Available
Natural soiling and the subsequent requisite cleaning of photovoltaic (PV) modules result in abrasion damage to the cover glass. The durability of the front glass has important economic consequences, including determining the use of anti-reflective and/or anti-soiling coatings as well as the method and frequency of operational maintenance (cleaning). Artificial linear brush abrasion using Nylon 6/12 bristles was therefore examined to explore the durability of representative PV first-surfaces, i.e., the surface of a module incident to direct solar radiation. Specimens examined include silane surface functionalized-, roughened (etched)-, porous silica-coated-, fluoropolymer-coated-, and ceramic (TiO2 or ZrO2/SiO2/ZrO2/SiO2)-coated-glass, which are compared to monolithic-poly(methyl methacrylate) and -glass coupons. Characterization methods used in this study include: optical microscopy, ultraviolet-visible-near-infrared (UV-VIS-NIR) spectroscopy, sessile drop goniometry, white-light interferometry, atomic force microscopy (AFM), and depth-profiling X-ray photoelectron spectroscopy (XPS). The corresponding characteristics examined include: surface morphology, transmittance (i.e., optical performance), surface energy (water contact angle), surface roughness, scratch width and depth, and chemical composition, respectively. The study here was performed to determine coating failure modes; identify characterization methods that can detect nascent failures; compare the durability of popular contemporary coating materials; identify their corresponding damage characteristics; and compare slurry and dry-dust abrasion. This study will also aid in developing an abrasion standard for the PV industry.
We describe advances on procedures used for the coring of silicon photovoltaic modules. These procedures involve coring specific locations, starting from the back of the modules, and removing selected parts of the cell structure, while preserving the front tempered glass. The standard coring procedures had to be modified from case to case due to the different cell structures and measurement requirements. We provide examples of the characterization of the cored samples by scanning electron microscopy and energy-dispersive X-ray spectroscopy. Finally, we describe a simple process to create small openings at specific locations on the back of photovoltaic modules to allow for efficiency-related measurement of individual cells and groups of cells.
Entropy stabilization has garnered significant attention as a new approach to designing novel materials. Much of the work in this area has focused on bulk ceramic processing, leaving entropy-stabilized thin films relatively under-explored. Following an extensive multi-variable investigation of polycrystalline (Mg 0.2 Co 0.2 Ni 0.2 Cu 0.2 Zn 0.2 )O thin films deposited via pulsed laser deposition (PLD), it is shown here that substrate temperature and deposition pressure have strong and repeatable effects on film texture and lattice parameter. Further analysis shows that films deposited at lower temperatures and under lower oxygen chamber pressure are 40x less electrically resistive than otherwise identical films grown at higher temperature and pressure. Annealing these films in an oxygen-rich environment increases their electrical resistivity to match that of the films grown at higher temperatures and pressures. Because of this, the electric conductivity is hypothesized to be the result of polaron hopping mediated by transition metal valence changes which compensate for oxygen off-stoichiometry.
Nanoparticle silicon–graphite composite electrodes are a viable way to advance the cycle life and energy density of lithium-ion batteries. However, characterization of composite electrode architectures is complicated by the heterogeneous mixture of electrode components and nanoscale diameter of particles, which falls beneath the lateral and depth resolution of most laboratory-based instruments. In this work, we report an original laboratory-based scanning probe microscopy approach to investigate composite electrode microstructures with nanometer-scale resolution via contrast in the electronic properties of electrode components. Applying this technique to silicon-based composite anodes demonstrates that graphite, SiOx nanoparticles, carbon black, and LiPAA binder are all readily distinguished by their intrinsic electronic properties, with measured electronic resistivity closely matching their known material properties. Resolution is demonstrated by identification of individual nanoparticles as small as ~20 nm. Our technique presents future utility in multiscale characterization to better understand particle dispersion, localized lithiation, and degradation processes in composite electrodes for lithium-ion batteries.
Hybrid materials of metal chalcogenide colloidal quantum dots (QDs) embedded in metal halide perovskites (MHPs) have led to composites with synergistic properties. Here, we investigate how QD size, surface chemistry, and MHP film formation methods affect the resulting optoelectronic properties of QD/MHP “dot-in-matrix” systems. We monitor the QD absorption and photoluminescence throughout synthesis, ligand exchange, and transfer into the MHP ink, and we characterize the final QD/MHP films via electron microscopy and transient absorption. In addition, we are the first to globally map how PbS QDs are distributed on the micrometer scale within these dot-in-matrix systems, using three-dimensional (3D) tomography time-of-flight secondary ion mass spectrometry. The surface chemistry imparted during synthesis directly affects the optical properties of the dot-in-matrix composites. Pb-halide passivation leads to QD/MHP dot-in-matrix samples with optical properties that are well-described by a theoretical model, based on a Type I finite-barrier heterostructure between the PbS QD and the MHP matrix. Samples without Pb-halide passivation show complicated size-dependent behavior, indicating a transition from a Type I heterostructure between the PbS QD wells and MHP barriers for small-sized QDs to PbS QDs that are electronically decoupled from the MHP matrix for larger QDs. Furthermore, the choice in perovskite antisolvent crystallization method leads to a difference in the spatial QD distribution within the perovskite matrix, differences in carrier lifetime, and photoluminescence shifts of up to 180 meV for PbS in methylammonium lead iodide. This work establishes an understanding of such emerging synergistic systems relevant for technologies such as photovoltaics, infrared emitters and detectors, and other unexplored technological applications.
Natural soiling and the subsequent necessary cleaning of photovoltaic (PV) modules result in abrasion damage to the cover glass. The durability of the front glass has important economic consequences, including determining the use of anti-reflective and/or anti-soiling coatings as well as the method and frequency of operational maintenance (cleaning). Artificial linear brush abrasion using Nylon 6/12 bristles was therefore examined to explore the durability of representative PV first-surfaces, i.e., the surface of a module incident to direct solar radiation. Specimens examined include silane surface functionalized-, roughened (etched)-, porous silica-coated-, fluoropolymer-coated-, and ceramic (TiO 2 or ZrO 2 /SiO 2 /ZrO 2 /SiO 2 )-coated-glass, which are compared to monolithic-poly(methyl methacrylate) and -glass coupons. Characterization methods used in this study include: optical microscopy, ultraviolet–visible–near-infrared (UV-VIS-NIR) spectroscopy, sessile drop goniometry, white-light interferometry, atomic force microscopy (AFM), and depth-profiling X-ray photoelectron spectroscopy (XPS). The corresponding characteristics examined include: surface morphology, transmittance (i.e., optical performance), surface energy (water contact angle), surface roughness, scratch width and depth, and chemical composition, respectively. The study here was performed to determine coating failure modes; identify characterization methods that can detect nascent failures; compare the durability of popular contemporary coating materials; identify their corresponding damage characteristics; and compare slurry and dry-dust abrasion. This study will also aid in developing an abrasion standard for the PV industry.
Various processes lead to degradation of cathodes in lithium-ion batteries. Questions remain regarding mechanisms of many of these processes. Probe microscopy methods including scanning electrochemical microscopy (SECM) are capable of directly probing processes at the cathode/electrolyte interface. SECM uses a small electrode to perform rapid electrochemical analysis of transient species generated at an active cathode/electrolyte interface. This paper discusses the background of the SECM instrument and its application to lithium-ion battery research. We also describe the application of SECM methods to the study of cathode degradation processes observed in lithium-ion batteries. Specifically, we focus on characterizing the dissolution of manganese from LiMn2O4 (LMO) based on recent debate in the literature. We describe experiments to observe and characterize the electrochemical properties of manganese complexes emerging from degrading LMO electrode materials.