Investigating the effect of B T direction on W source-to-core pathways during the SAS-VW campaign on DIII-D

Experiments using the V-shaped closed slot tungsten (W) coated SAS-VW divertor in DIII-D studied the effects of the BT direction on core contamination of eroded tungsten from a closed slot divertor configuration. Core W content is inferred using soft-X ray tomography (SXR) and vacuum ultraviolet spectroscopy (SPRED), while W divertor erosion is inferred from visible spectroscopy of W emission (400.9 nm) measured by in-slot filterscopes (filtered photo-multipliers). Post-mortem analysis from the campaign discovered tile misalignment leading to suspected pronounced leading-edge erosion in the unfavorable BT direction (ion B ⃗×∇B ⃗ drift away from divertor) likely not captured by diagnostics. However, empirical findings show up to ~2-3x larger core contamination in the favorable BT direction even considering no additional W erosion from leading edges. A “source-to-core efficiency factor” is derived to estimate the effects of leading-edge erosion and compare W contamination for two pairs of H-mode discharges in opposite BT directions. While having differing absolute parameters, similar core impurity density gradients suggest comparable core impurity transport. These results show that favorable BT may have stronger source-to-core pathways for W impurities sourced from the outer divertor region. Possible explanations could include the effects of E ⃗×B ⃗ drifts on W transport in the scrape-off-layer (SOL) as well as previously determined fast SOL inner target directed flows in favorable BT.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Recent DIII-D progress toward validating models of tungsten erosion, re-deposition, and migration for application to next-step fusion devices

Abstract Fundamental mechanisms governing the erosion and prompt re-deposition of tungsten impurities in tokamak divertors are identified and analyzed to inform the lifetime of tungsten plasma-facing components in ITER and other future devices. Various experiments conducted at DIII-D to benchmark predictive models are presented, leveraging the DiMES removable sample exposure probe capability and the Metal Rings Campaign, in which toroidally symmetric rows of tungsten-coated tiles were installed in the DIII-D divertor. In tokamak divertors, the width of the electric sheath is of the order of the main ion Larmor radius, and a vast majority of sputtered tungsten impurities are typically ionized within the sheath. Therefore, W prompt redeposition is mainly governed by the ratio of the characteristic ionization mean-free path of neutral tungsten to the width of the sheath. In-situ monitoring of the prompt redeposition of tungsten impurities in divertors is demonstrated via the use of WII/WI line ratios and the ionizations/photon (S/XB) method in L-mode discharges. Even with this relatively limited set of emission measurements, net erosion measurements were found to be a consistent upper bound to an analytic scaling based on the ratio of the W ionization length, λ iz , and the width of the magnetic sheath rather than the ratio of λ iz and the W + gyro-radius. In the far-scrape-off layer (SOL) of the ITER divertor, however, it is calculated that the measurement of photon emissions associated with the ionization of tungsten impurities up to W 5 + may be required. Finally, W deposition patterns on DiMES collector probes, interpreted via DIVIMP-WallDYN modelling, reveal the key roles of progressive W erosion/re-deposition staps and E × B drifts in regulating long-range high-Z material migration.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Direct measurement of the electron turbulence-broadening edge transport barrier to facilitate core–edge integration in tokamak fusion plasmas

Abstract The integration of a high-performance core and a dissipative divertor, or the so-called ‘core–edge integration,’ has been widely identified as a critical gap in the design of future fusion reactors. In this letter, we report, for the first time, direct experimental evidence of electron turbulence at the DIII-D H-mode pedestal that correlates with the broadening of the pedestal and thus facilitates core–edge integration. In agreement with gyrokinetic simulations, this electron turbulence is enhanced by high η e ( η e = L n / L T e , where L n is the density scale length and L T e is the electron temperature scale length), which is due to a strong shift between the density and temperature pedestal profiles associated with a closed divertor. The modeled turbulence drives significant heat transport with a lower pressure gradient that may broaden the pedestal to a greater degree than the empirical and theoretically predicted pedestal width scalings. Such a wide pedestal, coupled with a closed divertor, enables us to achieve a good core–edge scenario that integrates a high-temperature low-collisionality pedestal (pedestal top temperature T e,ped > 0.8 keV and a pedestal top collisionality ν * ped < 1) under detached divertor conditions. This paves a new path toward solving the core–edge integration issue in future fusion reactors.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Study on divertor detachment and pedestal characteristics in the DIII-D upper closed divertor

Abstract Experiments performed in DIII-D demonstrate that higher plasma current and heating power combined with impurity seeding facilitate the achievement of divertor detachment with a higher pedestal pressure and higher plasma performance in H-mode plasmas with a baffled closed divertor compared with an open divertor. Dedicated experiments were carried out to study the impact of power, plasma current and impurity seeding on divertor detachment with ion B × ∇ B directed into the divertor favorable for the L–H transition. With a factor of three variation in heating power and with only D 2 puffing, no significant difference in the separatrix density at detachment onset was found. The higher heating power leads to higher impurity concentration and wider scrape-off layer (SOL) width, and reduces the detachment onset density to one similar to that in lower-power plasmas. Higher current requires higher pedestal and line-averaged densities to achieve divertor detachment; however, the increase in separatrix density at increasing plasma current is found to be less pronounced. Initial calculations found that both power scan and plasma current scan datasets are qualitatively consistent with theory after considering the change in impurity concentration and heat flux width. This also motivates the future extensive study of transport and divertor impurity behavior in order to have a quantitative comparison between experiment and theory. Compared with an open divertor, a closed divertor facilitates detachment onset at ∼40% lower line-averaged plasma density. Additional N 2 seeding facilitates the achievement of detachment at a lower separatrix density and thus a higher pedestal temperature, which is beneficial for advanced tokamak scenarios. Higher heating power requires a higher N 2 puffing rate to achieve the same degree of detachment, while a higher N 2 puffing rate leads to lower detachment onset line-averaged density, both of which agree with theory. In contrast to the narrower pedestal in an open divertor approaching detachment, the pedestal density width in a closed divertor increases with density. The density gradient increases with line-averaged density at higher plasma current, but remains nearly unchanged at lower plasma current. In particular, compared with discharges with low power, at high heating power the pedestal density gradient is much weaker, while the SOL density is significantly higher and wider. At the same plasma current, both pedestal pressure gradient and temperature gradient decrease linearly with the line-averaged density but remain similar across different heating powers. Even with different plasma current and heating power, the normalized pressure gradient remains identical. As a result, achievement of divertor detachment with a higher pedestal pressure and higher plasma performance is shown in a closed divertor, which is important for improving core–edge integration as one of the critical issues for future tokamak fusion reactors.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Predicting tungsten erosion and leakage properties for the new V-shaped small angle slot divertor in DIII-D

Impurity transport modeling of the new tungsten (W)-coated, V-shaped small angle slot (SAS) divertor in the DIII-D tokamak was conducted using the SOLPS-ITER plasma edge code package and the DIVIMP impurity tracking code. The inboard baffle of the current SAS divertor will be shifted closer to the outboard baffle, creating a V-corner at the slot vertex. In addition, the outboard baffle will be coated with 10–15 μm of W for experiments studying high-Z sourcing and leakage in a closed divertor. Modeling of the 'SAS-VW' divertor predicts that these changes to the inner baffle will reduce W gross erosion by 40× relative to the existing SAS divertor when the outer strike point (OSP) is at the V-corner and the ion B × ∇B drift is towards the divertor, driven primarily by significant cooling near the slot vertex. Most W erosion in SAS-VW is expected to occur near the slot entrance, which may pose a higher risk to core contamination than W eroded deeper in the slot. Furthermore, adding a new sheath-based prompt redeposition model increases the sensitivity of redeposition estimates to near-target plasma conditions and may provide more accurate predictions of net erosion. Moving the OSP outboard from the slot vertex ~4 cm onto the W-coated region yields a 40× increase in the gross erosion rate and a 50% decrease in the core leakage fraction. Thus slight variations in strike point location may counteract the potential benefits of the tightly-baffled V slot on minimizing erosion. This impurity transport modeling provides useful guidance for future experiments on the SAS-VW divertor focused on high-Z erosion/redeposition, scrape-off layer transport, and core leakage.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Developing solid-surface plasma facing components for pilot plants and reactors with replenishable wall claddings and continuous surface conditioning. Part A: concepts and questions

Abstract It is estimated that pilot plants and reactors may experience rates of net erosion and deposition of solid plasma facing component (PFC) material of 10 3 –10 5 kg yr −1 . Even if the net erosion (wear) problem can be solved, the redeposition of so much material has the potential for major interference with operation, including disruptions due to so-called ‘unidentified flying objects (UFOs)’ and unsafe dust levels. The potential implications appear to be no less serious than for plasma contact with the divertor target: a dust explosion or a major UFO-disruption could be as damaging for an actively-cooled deuterium-tritium (DT) tokamak as target failure. It will therefore be necessary to manage material deposits to prevent their fouling operation. This situation appears to require a fundamental paradigm shift with regard to meeting the challenge of taming the plasma–material interface: it appears that any acceptable solid PFC material will in effect be flow-through , like liquid–metal PFCs, although at far lower mass flow rates. Solid PFC material will have to be treated as a consumable , like brake pads in cars. ITER will use high-Z (tungsten) armor on the divertor targets and low-Z (beryllium) on the main walls. The ARIES-AT reactor design calls for a similar arrangement, but with SiC cladding on the main walls. Non-metallic low-Z refractory materials such as ceramics (graphite, SiC, etc) used as in situ replenishable, relatively thin—of order mm—claddings on a substrate which is resistant to neutron damage could provide a potential solution for the main walls, while reducing the risk of degrading the confined plasma. Separately, wall conditioning has proven essential for achieving high performance. For DT devices, however, standard methods appear to be unworkable, but recently powder droppers injecting low-Z material ∼continuously into discharges have been quite effective and may be usable in DT devices as well. The resulting massive generation of low-Z debris, however, has the same potential to seriously disrupt operation as noted above. Powder droppers provide a unique opportunity to carry out controlled studies on the management of low-Z slag in all current tokamaks, independent of whether their protection tiles use low-Z or high-Z material.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Developing solid-surface plasma facing components for pilot plants and reactors with replenishable wall claddings and continuous surface conditioning. Part B: required research in present tokamaks

Abstract The companion part A paper (Stangeby et al 2022) reports a number of independent estimates indicating that high-duty-cycle DT tokamaks starting with pilot plants will likely experience rates of net erosion and deposition of solid PFC, plasma facing component, material in the range of 10 3 to 10 4 kg yr −1 , regardless of the material used. The subsequent redeposition of such large quantities of material has the potential for major interference with tokamak operation. Similar levels and issues will be involved if ∼continuous low-Z powder dropping is used for surface conditioning of DT tokamaks, independent of the material used for the PFC armor. In Stangeby et al (2022) (part A) it is proposed that for high-duty-cycle DT tokamaks, non-metallic low-Z refractory materials such as ceramics (graphite, SiC, etc) used as in situ replenishable, relatively thin—of order mm—claddings on a substrate which is resistant to neutron damage could provide a potential solution for protecting the main walls, while reducing the risk of degrading the confined plasma. Assessment of whether such an approach is viable will require information, much of which is not available today. Section 6 of part A identifies a partial list of major physics questions that will need to be answered in order to make an informed assessment. This part B report describes R&D needed to be done in present tokamaks in order to answer many of these questions. Most of the required R&D is to establish better understanding of low-Z slag generation and to identify means to safely manage it. Powder droppers provide a unique opportunity to carry out controlled studies on the management of low-Z slag in current tokamaks, independent of whether their protection tiles use low-Z or high-Z material.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Design and physics basis for the upcoming DIII-D SAS-VW campaign to quantify tungsten leakage and transport in a new slot divertor geometry

A set of experiments are planned to exploit the high SOL collisionality enabled by a tightly baffled slot divertor geometry to suppress tungsten leakage in DIII-D. A toroidal row of graphite tiles from the Small Angle Slot (SAS) divertor is being coated with 10–15 μ m of tungsten. New spectroscopic viewing chords with in-vacuo optics will measure the W gross erosion source from the divertor surface with high spatial and temporal resolution. In parallel, the bottom of the SAS divertor is changed from a flat to a ‘V’ shape. New SOLPS-ITER/DIVIMP simulations conducted with drifts using the planned ‘V’ shape predict a substantial reduction in W sourcing and SOL accumulation in either B × ∇B direction relative to either the old SAS divertor shape or the open, lower divertor. Dedicated studies are planned to carefully characterize the level of W sourcing, leakage, and scrape-off-layer (SOL) accumulation in DIII-D over a wide range of plasma scenarios. Various actuators will be assessed for their efficacy in further reducing high-Z impurity sources and leakage from the slot divertor geometry. Finally, this coupled code-experiment validation effort will be used to stress-test physics models and build confidence in extrapolations to advanced, high-Z divertor geometries for next-step devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Numerical assessment of the new V-shape small-angle slot divertor on DIII-D

The small-angle slot (SAS) divertor of the DIII-D tokamak, and its upcoming upgrade, the V-shape small-angle slot (SAS-V) divertor, are numerically investigated using the SOLPS-ITER code package, including the effect of particle drifts, for a range of plasma density, heating power, strike point position in the slot, and for both magnetic field directions. The simulations show that the electron temperature near the strike point is reduced in SAS-V compared to SAS, for both magnetic field directions, such that SAS-V achieves divertor detachment at a lower value of the outboard mid-plane separatrix electron density. The detachment threshold is lower because the V-shape focuses recycling neutrals on the V-end, densifying and cooling the plasma in the slot. At sufficiently high density, the V-shape also reduces the radial gradient of the temperature profile at the target, which in turns reduces the radial electric field and the E x B drift velocities, further densifying and cooling the plasma in the slot and leading to detachment. The V-shape effect, however, is reduced for higher heating power. With more heating power, the detachment density increases, reducing the ionization mean free path of recycled neutrals, which therefore become less sensitive to target shape changes. Furthermore, this suggests that in a fusion reactor, where the heating power is high, optimization of the divertor target shape needs to be combined with other strategies to lower the detachment density, such as in-slot injection of low-Z impurities.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effects of divertor electrical drifts on particle distribution and detachment near the divertor target plate in DIII-D

Strong impacts of drifts on the divertor plasma in–out asymmetry and detachment are demonstrated in DIII-D with an open divertor configuration. For forward toroidal field, B T , i.e., with the ion B × ∇B drift toward the divertor, the particle flux to the inner divertor, as represented by the Langmuir probe measured ion saturation current (J sat ), exhibits a double peak structure, with electron temperature, lower at the inner target. Reversing the B T direction reverses both the radial and poloidal E × B flows, leading to a broad particle flux profile in the outboard scrape-off layer (SOL) with a similar double-peak structure to that observed at the inner target with forward B T . The correlation of a double peak structure with divertor temperature profiles confirms physical coupling between the drift flow and sheath boundary condition and their strong impact on divertor profiles. In addition, under reversed B T conditions, increasing the density flattens the target temperature profile. However, J sat remains high away from the strike point, rendering it difficult to achieve an “effective” detached plasma, i.e., with effective reduction in both peak heat flux and peak temperature (in the far SOL). In contrast, divertor detachment with a cold and flat temperature profile can be achieved at both target plates with the forward B T .

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Observation of fully detached divertor integrated with improved core confinement for tokamak fusion plasmas

Integration of divertor detachment with a high-performance (β N ~ 3, β p > 2, H 98 ~ 1.5) core plasma has been demonstrated in DIII-D high-β p (poloidal beta) plasmas associated with a sustained core internal transport barrier (ITB) and an H-mode edge transport barrier (ETB). Such good core-edge integration has been achieved for both neon and nitrogen seeding, for both favorable and unfavorable B-field directions, independently from the impurity puffing locations, though these variations play important roles on divertor characteristics. Compared to the standard H-mode plasmas, the high-β p plasma exhibits a much wider window of detachment compatible with high confinement core. Fully detached divertor plasmas with low plasma temperature (Te < 5 eV), low particle flux, and low heat flux across the entire divertor target plate were obtained by using nitrogen seeding. This detached high-β p plasma is compatible with a newly developed detachment control system which can help optimize the nitrogen gas flow rate. Several features, i.e., the high edge safety factor in the high-β p scenario, impurity injection, closed divertor and reduced heating power requirement due to the high confinement, facilitate the achievement of full divertor detachment at lower density. Instead of degrading global performance, the divertor detachment facilitates the access to an even stronger ITB at large radius with a relatively weak ETB through self-organized synergy between ITB and ETB, leading to sustained high confinement. The strengthening of the large-radius ITB compensates for the ETB degradation associated with divertor detachment. In addition, a weak ETB naturally has smaller edge localized modes (ELMs). In particular, with neon injection, a long-period no-ELM H-mode phase has been achieved simultaneously with high-performance core and partially detached divertor plasmas. Furthermore, these results demonstrate the possibility of integrating excellent core plasma performance with an effective divertor solution, an essential step toward steady-state operation of reactor-grade plasmas.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Evaluation of silicon carbide as a divertor armor material in DIII-D H-mode discharges

Silicon carbide (SiC) represents a promising but largely untested plasma-facing material (PFM) for next-step fusion devices. In this work, an analytic mixed-material erosion model is developed by calculating the physical (via SDTrimSP) and chemical (via empirical scalings) sputtering yield from SiC, Si, and C. The Si content in the near-surface SiC layer is predicted to increase during D plasma bombardment due to more efficient physical and chemical sputtering of C relative to Si. Silicon erosion from SiC thereby occurs primarily from sputtering of the enriched Si layer, rather than directly from the SiC itself. SiC coatings on ATJ graphite, manufactured via chemical vapor deposition, were exposed to repeated H-mode plasma discharges in the DIII-D tokamak to test this model. The qualitative trends from analytic modeling are reproduced by the experimental measurements, obtained via spectroscopic inference using the S/XB method. Quantitatively the model slightly under-predicts measured erosion rates, which is attributed to uncertainties in the ion impact angle distribution, as well as the effect of edge-localized modes. After exposure, minimal changes to the macroscopic or microscopic surface morphology of the SiC coatings were observed. Compositional analysis reveals Si enrichment of about 10%, in line with expectations from the erosion model. Extrapolating to a DEMO-type device, an order-of-magnitude decrease in impurity sourcing, and up to a factor of 2 decrease in impurity radiation, is expected with SiC walls, relative to graphite, if low C plasma impurity content can be achieved. Furthermore, these favorable erosion properties motivate further investigations of SiC as a low-Z, non-metallic PFM.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Integration of full divertor detachment with improved core confinement for tokamak fusion plasmas

Divertor detachment offers a promising solution to the challenge of plasma-wall interactions for steady-state operation of fusion reactors. Here, we demonstrate the excellent compatibility of actively controlled full divertor detachment with a high-performance (β N ~ 3, H 98 ~ 1.5) core plasma, using high-β p (poloidal beta, β p > 2) scenario characterized by a sustained core internal transport barrier (ITB) and a modest edge transport barrier (ETB) in DIII-D tokamak. The high-β p high-confinement scenario facilitates divertor detachment which, in turn, promotes the development of an even stronger ITB at large radius with a weaker ETB. This self-organized synergy between ITB and ETB, leads to a net gain in energy confinement, in contrast to the net confinement loss caused by divertor detachment in standard H-modes. These results show the potential of integrating excellent core plasma performance with an efficient divertor solution, an essential step towards steady-state operation of reactor-grade plasmas.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

First Evidence of Local E × B Drift in the Divertor Influencing the Structure and Stability of Confined Plasma near the Edge of Fusion Devices

The structure of the edge plasma in a magnetic confinement system has a strong impact on the overall plasma performance. Here we uncover for the first time a magnetic-field-direction dependent density shelf, i.e., local flattening of density radial profile near the magnetic separatrix, in high confinement plasmas with low edge collisionality in the DIII-D tokamak. The density shelf is correlated with a doubly peaked density profile near the divertor target plate, which tends to occur for operation with the ion BX∇B drift direction away from the X-point, as currently employed for DIII-D advanced tokamak scenarios. This double-peaked divertor plasma profile is connected via the EXB drifts, arising from a strong radial electric field induced by the radial electron temperature gradient near the divertor target. The drifts lead to the reversal of the poloidal flow above the divertor target, resulting in the formation of the density shelf. The edge density shelf can be also enhanced at higher heating power, preventing large, periodic bursts of the plasma, i.e. Edge-localized Modes, in the edge region, consistent with ideal magnetohydrodynamics calculations.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗