Effect of Water Concentration in LiPF 6 -Based Electrolytes on the Formation, Evolution, and Properties of the Solid Electrolyte Interphase on Si Anodes

A trace amount of water in an electrolyte is one of the factors detrimental to the electrochemical performance of silicon (Si)-based lithium-ion batteries that adversely affect the formation and evolution of the solid electrolyte interphase (SEI) on Si-based anodes and change its properties. Thus far, a lack of fundamental and mechanistic understanding of SEI formation, evolution, and properties in the presence of water has inhibited efforts to stabilize the SEI for improved electrochemical performance. As such, we investigated the SEI formed in a Gen2 electrolyte (1.2 M LiPF6 in ethylene carbonate/ethyl methyl carbonate, 3:7 wt %, water content: <10 ppm) with and without additional water (50 ppm) at varying potentials (1.0, 0.5, 0.2, and 0.01 V vs Li/Li + ). The impact of additional water on the morphological, (electro)chemical, and structural properties of SEI was studied using microscopic (atomic force microscopy and scanning spreading resistance microscopy) and spectroscopic (X-ray photoelectron spectroscopy, attenuated total reflection Fourier-transform infrared spectroscopy, and time-of-flight secondary ion mass spectrometry) techniques. The SEI exhibits both potential- and water concentration-dependent trends in its morphology and chemical composition. The presence of additional water in the electrolyte causes parasitic reactions, which onset at ~1.0 V, resulting in a reduction of electrolyte components and result in the formation of an insulating, fluorophosphate-rich SEI. In addition, hydrolysis of LiPF 6 creates hydrofluoric acid, which reacts with the surface oxide layer on the Si electrode, leading to a pitted and inhomogeneous SEI structure.

36 MATERIALS SCIENCE↗

Evolution of solid electrolyte interphase and active material in the silicon wafer model system

Alloying anode materials for lithium-ion batteries, such as silicon (Si), are an important focus of materials research due to the demand for increased energy density for electric vehicles and stationary grid storage. However, progress towards next generation anode materials has been hindered by poor capacity retention due to the instability of the Si active material and the solid electrolyte interphase (SEI). Herein, the evolution of the active Si material and the SEI are simultaneously investigated from the perspective of chemical, structural, morphological, and electronic evolution in the Si wafer model system through its cycling life, using time-of-flight secondary ion mass spectrometry (TOF-SIMS), scanning transmission electron microscopy (STEM), atomic force microscopy (AFM), and scanning spreading resistance microscopy (SSRM). The results illustrate a dynamic evolution of the SEI and active Si material through cycling. Through an improved understanding of evolution of SEI and Si active material within the Si wafer model system, mitigation strategies may be designed to extend the lifetime of Si anodes.

25 ENERGY STORAGE↗

Enhanced Interfacial Stability of Si Anodes for Li-Ion Batteries via Surface SiO2 Coating

Silicon is a promising alloying anode for lithium-ion batteries owing to its high capacity and low cost. However, its use has been hampered by mechanical failure arising from the large volume change upon cycling and by an insufficiently stable solid-electrolyte interphase (SEI). SEI formation depends on the Si surface, which is often an oxide (SiO x ). In this study we compare three different Si surfaces using Si wafers: 1.3 nm native SiO x , 1.4 nm thermally grown SiO2, and a SiOx-free surface. The oxide-free surface showed the worst electrochemical performance, never exceeding 94% Coulombic efficiency (CE). Furthermore, it also exhibited the thickest SEI and the highest overpotential for lithiation, which correlated with uninhibited electrolyte reduction and the incorporation of P-F species into the SEI. The oxide-coated surfaces performed significantly better, demonstrating a CE above 99% beyond the second cycle, low overpotential for lithiation, and a thinner and more stable SEI. The oxides lower the onset potential for electrolyte reduction, and yield an SEI with fewer P-F species. However, it was found that the CE with the native oxide surface decays from the fifth cycle onwards and correlates with a resurgence of electrolyte reduction. A 1-2 nm thermal SiO 2 coating is optimum for achieving a stable SEI that minimizes side reactions and sustains efficient cycling.

25 ENERGY STORAGE↗

Surface SiO 2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid–electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiO x coatings of varying thicknesses that form the true surface of the electrode. Here, the lithiation of SiO 2 -coated Si is studied in a controlled manner using SiO 2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO 2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li + . Si lithiation is reversible, and SiO 2 lithiation is largely irreversible. Above 2 nm SiO 2 , voltammetric currents decrease exponentially with SiO 2 thickness. For 2–3 nm SiO 2 , SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO 2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO 2 coating is thicker than 3–4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO 2 /Si interface radially outward from an existing pinhole, followed by the lithiation of SiO 2 from the interface outward.

25 ENERGY STORAGE↗

Fabrication of high-performance gas-diffusion-electrode based membrane-electrode assemblies

This paper demonstrates the fabrication and processing steps required to produce high performance fuel cell membrane electrode assemblies (MEAs) based on spray-coated gas-diffusion electrodes (GDEs). It is demonstrated that coating the catalyst layer with a thin layer of ionomer and then hot pressing the GDEs to the membrane is required to achieve comparable catalyst activity and air performance to catalyst-coated-membrane MEAs. We show that there is a critical amount of ionomer required to achieve maximized performance. Using electron microscopy, we show that the combination of the ionomer overlayer and hot-pressing bonds the catalyst layer to the membrane, increasing the interfacial contact area and quality of this interface. We also find that the ionomer overlayer smooths the surface of the GDE and provides increased contact area between the GDE and the membrane. Additionally, we demonstrate that much less ionomer is required for high-performance than has been previously reported. Through model fitting of electrochemical impedance spectroscopy, we show that this improvement in the catalyst layer - membrane interface reduces the effective catalyst layer resistance, which reduces Ohmic losses and increases catalyst utilization.

33 ADVANCED PROPULSION SYSTEMS↗

Intrinsic Properties of Individual Inorganic Silicon–Electrolyte Interphase Constituents

Because of the complexity, high reactivity, and continuous evolution of the silicon-electrolyte interphase (SiEI), 'individual' constituents of the SiEI were investigated to understand their physical, electrochemical, and mechanical properties. For the analysis of these intrinsic properties, known SiEI components (i.e., SiO 2 , Li 2 Si 2 O 5 , Li 2 SiO 3 , Li 3 SiO x , Li 2 O, and LiF) were selected and prepared as amorphous thin films. The chemical composition, purity, morphology, roughness, and thickness of prepared samples were characterized using a variety of analytical techniques. On the basis of subsequent analysis we found, LiF shows the lowest ionic conductivity and relatively weak, brittle mechanical properties, while lithium silicates demonstrate higher ionic conductivities and greater mechanical hardness. This research establishes a framework for identifying components critical for stabilization of the SiEI, thus enabling rational design of new electrolyte additives and functional binders for the development of next-generation advanced Li-ion batteries utilizing Si anodes.

14 SOLAR ENERGY↗

Three-Dimensional Resistivity vs. Depth Profiling for Advanced Characterization of the Lithium-Ion Battery Solid Electrolyte Interphase

In this work, we investigate the evolution of SEI formed from a standard electrolyte (1.2 M LiPF6 in EC:EMC (3:7 wt%)) through various points in cycling on several model Si surfaces. We also examine the solubility of SEI by resting the anode in the cell at varied temperatures then characterizing the residual SEI. Evolution of the SEI surface is also analyzed with atomic force microscopy (AFM) measurements. AFM and SSRM-derived results are presented in combination with chemical characterization, including time-of-flight secondary ion mass spectrometry (TOF-SIMS).

25 ENERGY STORAGE↗

Temperature-Dependent Solubility of Solid Electrolyte Interphase on Silicon Electrodes

The lithium-ion batteries powering mass market electric vehicles must be capable of operating in a wide temperature range. Temperature variation has the possibility to greatly affect the stability of the solid electrolyte interphase (SEI) responsible for mitigating capacity fade due to electrolyte decomposition in the lithium-ion battery. Here, we explore the solubility of the SEI on the silicon (Si) electrode, an alternative anode material to the conventional graphite electrode, at temperatures ranging from -10 to 50 °C. Through use of an electrochemical protocol with a high cathodic cutoff voltage, we measure the evolution of the SEI independently of competing Si mechanical stress. We correlate the electrochemical data with three-dimensional resistivity versus depth profiling as well as atomic force microscopy to show that SEI dissolution occurs at significantly faster rates at higher temperatures.

25 ENERGY STORAGE↗

Three-dimensional electronic resistivity mapping of solid electrolyte interphase on Si anode materials

Silicon is a promising candidate for the lithium ion battery (LIB) anode because of the order-of-magnitude improvement in capacity over current state-of-the-art graphite anodes. In systems featuring both C and Si anodes, electronic resistivity of the solid-electrolyte interphase (SEI) layer is a critical factor for preventing continuous electrolyte-decomposition reactions at the electrode/electrolyte interface. However, the in-situ measurement of SEI electronic resistance has been complicated by ion transport and electronic contributions from other parts of the battery circuit. Ex-situ measurements of SEI resistivity at microscopic scales are also lacking. We report on a nanometer-resolution three-dimensional technique that enables ex-situ mapping of electronic resistivity of SEI formed on a model single-crystalline wafer Si anode. Our novel experimental approach uses scanning spreading-resistance microscopy resistance imaging and mechanical depth profiling. In addition to resistance mapping, this method also provides an alternative technique for locating buried interfaces, where mechanical or electronic properties differ sufficiently between layers. Further validation of this method was obtained by resistance mapping of a reference sample with a designed a-Si:H layer stack of different doping concentrations. The results show relatively uniform lateral resistivity distribution of the SEIs but steep decreases in resistivity in the vertical direction. Resistivity vs. depth profiles are highly dependent on cycling conditions, but they generally show a resistivity decrease from the most superficial levels of SEI and a thickness increase with continued cycling prior to SEI stabilization. The most prominent resistivity increase was observed on SEI formed in Gen2 electrolyte (EC:EMC [3:7 by wt.] + 1.2 M LiPF6) with 10 wt% fluoroethylene carbonate additive; this result may partially explain the significant improvements of sustained electrochemical cycling and coulombic efficiency observed with this electrolyte additive. Our approach provides a novel and unparalleled three-dimensional approach in characterizing electronic resistivity, which contributes significantly to understanding SEI formation and the intrinsic properties critical to battery performance.

25 ENERGY STORAGE↗

Mechanical Properties and Chemical Reactivity of Li x SiO y Thin Films

Silicon (Si) is a commonly studied candidate material for next-generation anodes in Li-ion batteries. A native oxide SiO 2 on Si is often inevitable. However, it is not clear if this layer has a positive or negative effect on the battery performance. This understanding is complicated by the lack of knowledge about the physical properties of the SiO 2 lithiation products and by the convolution of chemical and electrochemical effects during the anode lithiation process. In this study, Li x SiO y thin films as model materials for lithiated SiO 2 were deposited by magnetron sputtering at ambient temperature, with the goal of (1) decoupling chemical reactivity from electrochemical reactivity and (2) evaluating the physical and electrochemical properties of Li x SiO y . X-ray photoemission spectroscopy analysis of the deposited thin films demonstrate that a composition close to previous experimental reports of lithiated native SiO 2 can be achieved through sputtering. Our density functional theory calculations also confirm that the possible phases formed by lithiating SiO 2 are very close to the measured film compositions. Scanning probe microscopy measurements show that the mechanical properties of the film are strongly dependent on lithium concentration, with a ductile behavior at a higher Li content and a brittle behavior at a lower Li content. The chemical reactivity of the thin films was investigated by measuring the AC impedance evolution, suggesting that Li x SiO y continuously reacts with the electrolyte, in part because of the high electronic conductivity of the film determined from solid-state impedance measurements. The electrochemical cycling data of the sputter-deposited Li x SiO y /Si films also suggest that Li x SiO y is not beneficial in stabilizing the Si anode surface during battery operation, despite its favorable mechanical properties.

14 SOLAR ENERGY↗

Intrinsic Properties of Individual Constituents of Silicon-Electrolyte Interphase

The stabilization of a solid electrolyte interphase (SEI) is one of the great challenges to utilize superior theoretical capacity (about 3,600 mAh g-1, almost 10 times higher than that of graphite) of a silicon (Si) as an anode in a next-generation advanced lithium-ion battery (LIB). A SEI remains a poorly understood and hardly studied topic relative to the research devoted to battery components due to its intrinsic properties of complexity, reactivity and continuous evolution. However, the SEI plays a key role in prevention of further electrolyte reduction and desolvation of Li+ ions, which is directly related to electrochemical performance, lifetime and safety of batteries. For example, the unstable SEI on a Si anode leads to initial irreversible capacity losses, poor cycling stability and a limited cycle life. 2-4 In this study each 'individual' component of SEI on a Si anode was prepared as a thin film, and the physical, electrochemical, mechanical and structural properties of prepared films were characterized using a variety of analytical equipment including electrochemical impedance spectroscopy, operando X-ray photoelectron spectroscopy, atomic force microscope, Fourier-transform infrared spectroscopy, scanning spreading resistance microscopy and time-of-flight secondary ion mass spectrometry. This study can provide a strong guidance to aid in the development of new electrolytes, additives and binders to stabilize SEI layer on a silicon anode by identifying beneficial components and providing mechanical explanation of a variety of reactions and phenomena in a SEI.

14 SOLAR ENERGY↗