Durability of YSZ Coated Ti2AlC in 1300 °C Mach 0.3 Burner Rig Tests

A thermal barrier coating system survived burner rig testing at 1300 °C for 500 h. A 160 µm thick yttria stabilized zirconia (YSZ) coating was applied to a Ti2AlC MAX phase bar sample by plasma spray physical vapor deposition (PS-PVD) and tested face-on in an atmospheric Mach 0.3 jet fuel burner, using 5-h thermal cycles. No thermal barrier coating (TBC) spallation or recession was observed, only a 2.4 mg/cm2 mass gain. The modest weight gain precluded severe volatility losses under high velocity burner conditions. The coating surface exhibited colonies of (111)flourite fiber-textured columns separated by craze patterns, with no visible moisture attack. The metastable tetragonal t' YSZ phase was obtained initially, transitioning to equilibrium teq and cubic YSZ, but with little detrimental monoclinic. The thickness of the alumina TGO was ~21 to 23 μm under the heated YSZ face and ~13 to 15 μm on the uncoated, cooler backside. The backside exhibited removal of initial transient TiO2 nodules and partial etching of the underlying Al2O3 scale by volatile hydroxides formed in high temperature, high velocity water vapor. Aerodynamic forces produced some bending of the cantilevered sample via creep. The test indicated exceptional stability of YSZ coatings on Ti2AlC under turbine conditions, with thermal expansion matching playing a key role. The purpose of this study was to demonstrate long term durability of YSZ/MAX phase system in aggressive high temperature burner rig testing. MAX phases have been keenly studied because of their unique crystal structure and intriguing properties (Refs. 1 and 2). Having Mn+1(Al,Si)(C,N)n general composition, they are defined as ceramics, but possess unusual desirable attributes such as high conductivity, thermal shock resistance, easy machinability, and deformation tolerance. The mechanical properties derive from weak M-(Al,Si) bonding in the basal plane that leads to sliding and kinking in preference to catastrophic crack growth. Like most ceramics they are phase stable at high temperatures, generally up to 1500 °C. High temperature oxidation resistance is excellent for alumina-forming Ti3AlC2, Ti2AlC, and Cr2AlC, as reviewed by Tallman, et al. (Ref. 3). Compatibility with α-Al2O3 scales is further enhanced in cyclic exposures by a close matching of thermal expansion coefficients, (Ref. 4) i.e., (~9.3, 10.2, 11.3×10–6/K for Al2O3, Ti2AlC, and YSZ, to be discussed). Turbine environments generally contain 10 percent water vapor in the combustion gases, therefore moisture effects can be a concern for some materials (Ref. 5). Furnace tests of MAX phases in high temperature steam generally showed little effect on Al2O3 scale growth (Ref. 6). However, high velocity and high pressure gas can influence scale losses by the formation of volatile reaction products, such as TiO(OH)2 and Al(OH)3 (Refs. 7 to 10). This phenomenon had been discussed for 1100 to 1300 °C high pressure burner rig tests of Ti2AlC (Ref. 11). A single cubic growth rate parameter kcubic was measurably lower than comparable furnace TGA data, but it could be matched reasonably well if corrected for a slight volatility term. In general, a two-parameter cubic-linear growth-volatility law was believed to apply. Corresponding scale volatility loss rates, directly measured at 1300 °C on a pre-oxidized sample, were moderate (0.012 mg/cm2/h) and largely attributed to removal of the initial TiO2 transient scale. A related CH4 burner study of high purity Cr2AlC MAX phase demonstrated 1200 °C durability after 500 rapid (5 min. heat and 2 min. cool) thermal shock cycling (29 h hot time) (Ref. 12). Heating and cooling rates were ~1000 and 500 °C per minute, with a gas velocity of 5 m/s, producing a 75 °C/mm gradient. A 7 μm Al2O3 surface scale and a 13 μm Cr7C3 depletion zone formed with no signs of failure. No evidence of scale volatility was evident, although weight change was not provided, the velocity was moderate, and the total hot time was not extensive. The same high gradient BRT was used to produce 1400 °C surface temperatures for a YSZ/Cr2AlC/IN738 system in the first study of MAX phases used as bond coats for thermal barrier coatings (TBC) (Ref. 25). Here TBC failure was reported after 745 cycles, with only a 1.5 μm Al2O3 scale entrained within a porous, Cr7C3 bondcoat depletion phase. YSZ thermal barrier coatings have been considered to be a compatible complement to Al-MAX phases because of thermal expansion matching and extremely low volatility in water vapor. Initial studies showed superior oxidative stability up to 1300 °C, for long times (at least 500 h) for Ti2AlC substrates and less (268 h) for Cr2AlC, while withstanding large alumina TGO scale thickness (~35 to 40 μm) (Refs. 13 and 14). By comparison, typical superalloy systems can only survive 1150 °C maximum interface temperatures for extended periods, with a maximum sustained TGO below 10 μm (Ref. 15). High temperature SiC based systems are known to form slow-growing SiO2 scales. But these are subject to rate enhancement and volatile Si(OH)4 products in the presence of water vapor, as described comprehensively by Opila, et al. (Refs. 5, 16 to 19). Net weight losses are generally observed in high velocity, high pressure burner rig studies (e.g., 0.084 mg/cm2/h at 1300 °C) (Ref. 20). Furthermore, the loss rates have been shown from chemical physics to scale with v1/2 and pH2O 2 (Ref. 16). Low activity, moisture-resistant environmental barrier coatings (EBC), such as rare earth silicates, are needed to prevent substrate recession under turbine conditions (Refs. 21 to 23).

Smialek, James L.

Revisiting the Birth of 7YSZ Thermal Barrier Coatings: Steve Stecura

Thermal barrier coatings are widely used in all turbine engines, typically using a 7 wt% Y2O3-ZrO2 formulation. Extensive research and development over many decades have refined the processing and structure of these coatings for increased durability and reliability. New compositions demonstrate some unique advantages and are gaining in application. However, the "7YSZ" formulation predominates and is still in widespread use. This special composition has been universally found to produce nanoscale precipitates of metastable t' tetragonal phase, giving rise to a unique toughening mechanism via ferro-elastic switching under stress. This note recalls the original study that identified superior properties of 6 to 8 wt% YSZ plasma sprayed thermal barrier coatings, published in 1978. The impact of this discovery, arguably, continues in some form to this day. At one point, 7YSZ thermal barrier coatings were used in every new aircraft and ground power turbine engine produced worldwide. It is a tribute to its inventor, Dr. Stephan J. Stecura, NASA retiree.

turbine blades

Unusual Oxidative Limitations for Al-MAX Phases

Alumina-forming MAX phases are well-known for their excellent oxidation resistance, rivaling many metallic NiAl, NiCrAl, and FeCrAl counterparts and with upper temperature capability possible to approximately1400C. However a number of limitations have been emerging that need to be acknowledged to permit robust performance in demanding applications. Ti2AlC and Ti3AlC2 possess excellent scale adhesion, cyclic oxidation/moisture/volatility resistance, and TBC compatibility. However they are very sensitive to Al content and flux in order to maintain an exclusive Al2O3 scale without runaway oxidation of ubiquitous TiO2 transient scales. Accelerated oxidation has been shown to occur for Al-depleted, damaged, or roughened surfaces at temperatures less than 1200C. Conversely, Cr2AlC is less sensitive to transients, but exhibits volatile losses at 1200C or above if common Cr7C3 impurity phases are present. Poor scale adhesion is exhibited after oxidation at 1150C or above, where spallation occurs at the Cr7C3 (depletion zone) interface. Delayed spallation is significant and suggests a moisture-induced phenomenon similar to non-adherent metallic systems. Re-oxidation of this surface does not reproduce the initial pure Al2O3 behavior, but initiates a less-protective scale. Cr2AlC has also been shown to have good long term bonding with superalloys at 800C, but exhibits significant Beta-NiAl + Cr7C3 diffusion zones at 1100C and above. This may set limits on Cr2AlC as a high temperature TBC bond coat on Ni-based superalloys, while improving corrosion resistance in lower temperature applications.

oxidation resistance

Extreme Oxidative Durability of TBCs on Ti2AlC MAX Phases

APS and PS-PVD YSZ thermal barrier coatings, applied directly to oxidation resistant Ti2AlC substrates, were oxidized in interrupted furnace tests. Temperature was advanced in 50C intervals from 1100 to 1300C, each 500 h long with eleven cooling cycles. Damage only initiated on the APS coating at 1300C after 15 h, with complete delamination after 500 h. The PS-PVD coating survived all testing. Weight change and metallographic analyses indicate that the YSZ-Ti2AlC systems sustained alumina scale growth of 30-40 m. In comparison, widely used Pt-aluminide bondcoats on single crystal superalloy turbine blades exhibit TBC lives equivalent to alumina scale growth up to 7 m, equivalent to just 200 h at 1200C. It is demonstrated that 25x TBC life improvement (or 180C temperature increase) resulted from the close CTE match of Ti2AlC with those of alumina and YSZ.

protective coating

Alumina-Forming MAX Phases in Turbine Material Systems

Coatings for high temperature turbine components are based on low conductivity YSZ thermal barriers and protective NiAl, NiCoCrAlY bond coats. Good oxidation hot corrosion resistance, intermediate CTE, and strain tolerance of Ti2AlC and Cr2AlC MAX phases are thus of special interest. Their alumina scale growth follows a cubic law in accord with FeCrAlY alloys, with oxygen grain boundary diffusivity: Dgb 1.8 x 10-10 exp(-375 kJmole) m3s. Protective cubic kinetics are also found in high pressure burner rig (6 atm., 25 ms) and TGA tests of MAXthal 211Ti2AlC. The initial portion (0.1 hr) is dominated by fast TiO2 growth (with little evidence of scale volatility in high pressure water vapor, as found for SiO2 scales). Bulk Ti2AlC and Cr2AlC substrates show promise as potential bond coats for YSZ TBCs in 1000-1200 C furnace life (500 h) tests. Cr2AlC is proving to be very resistant to 700-900 C Na2SO4 hot corrosion and is of interest for disk alloys. Preliminary diffusion bonded Cr2AlC-superalloy hybrid couples have survived 1000 hr interrupted furnace tests at 800C with no indication of cracking or debonding. Diffusion zones of -NiAl+Cr7C3 were produced in these above 1000 C, but did not grow to any great extent after 1000 hr at 800 C. Processing as coatings presents challenges, however the basic properties of MAX phases provide novel opportunities for high temperature turbine components.

MAX phase

Diffusivity in Alumina Scales Grown on Al-MAX Phases

Ti3AlC2, Ti2AlC, and Cr2AlC are oxidation resistant MAX phase compounds distinguished by the formation of protective Al2O3 scales with well controlled kinetics. A modified Wagner treatment was used to obtain interfacial grain boundary diffusivity, deltaD(sub gb,O,int.), from scale growth rates and corresponding grain size. It is based on the p(O2)(exp -1/6) dependency of the double charged oxygen vacancy and oxygen diffusivity, coupled with the effective diffusion constant for short circuit grain boundary paths. Data from the literature for MAX phases was analyzed accordingly, and deltaD(sub gb,O,int.) was found to nearly coincide with the Arrhenius line developed for Zr-doped FeCrAl, where: deltaD(sub gb,O,int.) = 1.8x10(exp -10) exp(-375 kJ/RT) cubic meters/s. Furthermore, this oxidation relation suggests the more general format applicable to bulk samples under ambient conditions: deltaD(sub gb,O) = 7.567x10(exp -8) exp(-544 kJ/RT) p(O2)(exp -1/6) cubic meters/[s x Pa(exp -1/6)]. Data from many other FeCrAl(X) studies were similarly assessed to show general agreement with the relation for deltaD(sub gb,O,int.). This analysis reinforces the view that protective alumina scales grow by similar mechanisms for these Al-MAX phases and oxidation resistant FeCrAl alloys.

aluminum oxide

Microstructure and Oxidation of a MAX Phase/Superalloy Hybrid Interface

Corrosion resistant, strain tolerant MAX phase coatings are of interest for turbine applications. Thin Cr2AlC MAX phase wafers were vacuum diffusion bonded to an advanced turbine disk alloy, LSHR, at 1100 C. The interface, examined by optical and scanning electron microscopy, revealed a primary diffusion zone consisting of ~ 10 micrometers of beta-Ni(Co)Al, decorated with various NiCoCrAl, MC and M3B2 precipitates. On the Cr2AlC side, an additional ~40 micrometers Al-depletion zone of Cr7C3 formed in an interconnected network with the beta-Ni(Co)Al. Oxidation of an exposed edge at 800 C for 100 h produced a fine-grained lenticular alumina scale over Cr2AlC and beta-Ni(Co)Al, with coarser chromia granules over the Cr7C3 regions. Subsequent growth of the diffusion layers was only ~ 5 micrometers in total. A residual stress of ~ 500 MPa was estimated for the MAX phase layer, but no interfacial damage was observed. Subsequent tests for 1000 h reveal similar results.

heat resistant alloys

Oxygen Permeability and Grain-Boundary Diffusion Applied to Alumina Scales

High-temperature oxygen permeability measurements had determined grain-boundary diffusivities (deltaD(sub gb)) in bulk polycrystalline alumina (Wada, Matsudaira, and Kitaoka). They predict that oxygen deltaD(sub gb,O) varies with oxygen pressure as P(O2)(sup -1/6) at low pressure whereas aluminum deltaD(sub gb),Al varies with P(O2)(sup +3/16) at high pressure. These relations were used to evaluate alumina scale growth in terms of diffusivity and grain size. A modified Wagner treatment for dominant inward oxygen growth produces the concise solution: П(sub i) = k(sub p,i)×G(sub i) = 12 deltaD(sub gb,O,int), where П(sub i) is a constant and k(sub p,i) and G(sub i) refer to instantaneous values of the scale parabolic growth constant and grain size, respectively. A commercial FeCrAl(Zr) alloy was oxidized at 1100 to 1400 degC to determine k(sub p,i), interfacial grain size, П, and thus deltaD(sub gb,O,int). The deltaD(sub gb,O,int) values predicted from oxidation at (375 kJ/mole) were about 20 times less than those obtained above (at 298 kJ/mole), but closer than extrapolations from high-temperature bulk measurements. The experimental oxidation results agree with similar FeCrAl(X) studies, especially where both k(sub p,i) and G(sub i) were characterized. This complete approach accounts for temperature-sensitive oxidation effects of grain enlargement, equilibrium interface pressure variation, and grain-boundary diffusivity.

Smialek, James L.

Oxide Scales Formed on NiTi and NiPtTi Shape Memory Alloys

Ni-49Ti and Ni-30Pt-50Ti (at.%) shape memory alloys were oxidized isothermally in air over the temperature range of 500 to 900 C. The microstructure, composition, and phase content of the scales were studied by SEM, EDS, XRD, and metallography. Extensive plan view SEM/EDS identified various features of intact or spalled scale surfaces. The outer surface of the scale was a relatively pure TiO2 rutile structure, typified by a distinct highly striated and faceted crystal morphology. Crystal size increased significantly with temperature. Spalled regions exhibited some porosity and less distinct features. More detailed information was obtained by correlation of SEM/EDS studies of 700 C/100 hr cross-sections with XRD analyses of serial or taper-polishing of plan surfaces. Overall, multiple layers exhibited graded mixtures of NiO, TiO2, NiTiO3, Ni(Ti) or Pt(Ni,Ti) metal dispersoids, Ni3Ti or Pt3Ti depletion zones, and substrate, in that order. The NiTi alloy contained a 3 at.% Fe impurity that appeared in embedded localized Fe-Ti-rich oxides, while the NiPtTi alloy contained a 2 v/o dispersion of TiC that appeared in lower layers. The oxidation kinetics of both alloys (in a previous report) indicated parabolic growth and an activation energy (250 kJ/mole) near those reported in other Ti and NiTi studies. This is generally consistent with TiO2 existing as the primary scale constituent, as described here.

Smialek, James L.

Moisture-Induced TBC Spallation on Turbine Blade Samples

Delayed failure of TBCs is a widely observed laboratory phenomenon, although many of the early observations went unreported. "The weekend effect" or "DeskTop Spallation" (DTS) is characterized by initial survival of a TBC after accelerated laboratory thermal cycling, then failure by exposure to ambient humidity or water. Once initiated, failure can occur quite dramatically in less than a second. To this end, the water drop test and digital video recordings have become useful techniques in studies at NASA (Smialek, Zhu, Cuy), DECHMA (Rudolphi, Renusch, Schuetze), and CNRS Toulouse/SNECMA (Deneux, Cadoret, Hervier, Monceau). In the present study the results for a commercial turbine blade, with a standard EB-PVD 7YSZ TBC top coat and Pt-aluminide diffusion bond monitored by weight change and visual appearance. Failures were distributed widely over a 5-100 hr time range, depending on temperature. At some opportune times, failure was captured by video recording, documenting the appearance and speed of the moisture-induced spallation process. Failure interfaces exhibited alumina scale grains, decorated with Ta-rich oxide particles, and alumina inclusions as islands and streamers. The phenomenon is thus rooted in moisture-induced delayed spallation (MIDS) of the alumina scale formed on the bond coat. In that regard, many studies show the susceptibility of alumina scales to moisture, as long as high strain energy and a partially exposed interface exist. The latter conditions result from severe cyclic oxidation conditions, which produce a highly stressed and partially damaged scale. In one model, it has been proposed that moisture reacts with aluminum in the bond coat to release hydrogen atoms that 'embrittle' the interface. A negative synergistic effect with interfacial sulfur is also invoked.

Smialek, James L.

Moisture-Induced Alumina Scale Spallation: The Hydrogen Factor

For some time the oxidation community has been concerned with interfacial spallation of protective alumina scales, not just upon immediate cool down, but as a time-delayed phenomenon. Moisture-induced delayed spallation (MIDS) and desktop spallation (DTS) of thermal barrier coatings (TBCs) refer to this process. It is most apparent for relatively adherent alumina scales that have survived initial cool down in a dry environment, have built up considerable thickness and strain energy, and have been somewhat damaged, such as by cyclic oxidation cracking. Indeed, a "sensitive zone" can be described that maximizes the observed effect as a function of all the relevant factors. Moisture has been postulated to serve as a source of interfacial hydrogen embrittlement. Hydrogen is derived from reaction with aluminum in the alloy at an exposed interface. The purpose of this monograph is to trace the close analogy of this phenomenon to other hydrogen-induced effects, such as embrittlement of aluminides and blistering of alloys and anodic alumina films. A formalized, top-down, logic-tree structure is presented as a guide to this discussion. A theoretical basis for interfacial weakening by hydrogen is first cited, as are demonstrations of hydrogen detection as a reaction product or interfacial species. Further support is provided by critical experiments that recreate the moisture effect, but by isolating hydrogen from other potential causative factors. These experiments include tests in H 2-containing atmospheres or cathodic hydrogen charging. Accordingly, they strongly indicate that interfacial hydrogen, derived from moisture, is the key chemical species accounting for delayed alumina scale spallation.

Smialek, James L.

A Compendium of Scale Surface Microstructures: Ni(pt)al Coatings Oxidized at 1150 C for 2000 1-h Cycles

The surface structure of scales formed on Ni(Pt)Al coatings was characterized by SEM/EDS/BSE in plan view. Two nominally identical {100} samples of aluminide coated CMSX4 single crystal were oxidized at 1150 C for 2000 1-h cycles and were found to produce somewhat disparate behavior. One sample, with less propensity for coating grain boundary ridge deformation, presented primarily alpha-Al2O3 scale structures, with minimal weight loss and spallation. The original scale structure, still retained over most of the sample, consisted of the classic theta-alpha transformation-induced ridge network structure, with approx. 25 nm crystallographic steps and terraces indicative of surface rearrangement to low energy alumina planes. The scale grain boundary ridges were often decorated with a fine, uniform distribution of (Hf,Ti)O2 particles. Another sample, producing steady state weight losses, exhibited much interfacial spallation and a complex assortment of different structures. Broad areas of interfacial spalling, crystallographically-faceted (Ni,Co)(Al,Cr)2O4 spinel, with an alpha-Al2O3 base scale, were the dominant features. Other regions exhibited nodular spinel grains, with fine or (Ta,Ti)-rich (rutile) particles decorating or interspersed with the spinel. While these features were consistent with a coating that presented more deformation at extruded grain boundaries, the root cause of the different behavior between the duplicate samples could not be conclusively identified.

Smialek, James L.

A New Approach of Designing Superalloys for Low Density

New low-density single-crystal (LDS) alloy, have bee. developed for turbine blade applications, which have the potential for significant improvements in the thrust-to-weight ratio over current production superalloys. An innovative alloying strategy was wed to achieve alloy density reductions, high-temperature creep resistance, microstructural stability, and cyclic oxidation resistance. The alloy design relies on molybdenum as a potent. lower-density solid-solution strengthener in the nickel-based superalloy. Low alloy density was also achieved with modest rhenium levels tmd the absence of tungsten. Microstructural, physical mechanical, and environmental testing demonstrated the feasibility of this new LDS superalloy design.

MacKay, Rebecca A.

Alloy Design Challenge: Development of Low Density Superalloys for Turbine Blade Applications

New low density single crystal (LDS) alloys have been developed for turbine blade applications, which have the potential for significant improvements in the thrust to weight ratio over current production alloys. An innovative alloying strategy was identified to achieve high temperature creep resistance, alloy density reductions, microstructural stability, and cyclic oxidation resistance. The approach relies on the use of molybdenum (Mo) as a potent solid solution strengthener for the nickel (Ni)-base superalloy; Mo has a density much closer to Ni than other refractory elements, such as rhenium (Re) or tungsten (W). A host of testing and microstructural examinations was conducted on the superalloy single crystals, including creep rupture testing, microstructural stability, cyclic oxidation, and hot corrosion. The paper will provide an overview of the single crystal properties that were generated in this new superalloy design space. The paper will also demonstrate the feasibility of this innovative approach of low density single crystal superalloy design. It will be shown that the best LDS alloy possesses the best attributes of three generations of single crystal alloys: the low density of first-generation single crystal alloys, the excellent oxidation resistance of second-generation single crystal alloys, and a creep strength which exceeds that of second and third generation alloys.

MacKay, Rebecca A.

Moisture-Induced Alumina Scale Spallation: The Hydrogen Factor

For some time our community has been concerned with interfacial spallation of protective alumina scales, not just upon immediate cooldown, but as a time-delayed phenomenon. Moisture-induced delayed spallation (MIDS) and desktop spallation (DTS) of TBC's refer to this process. It is most apparent for relatively adherent alumina scales that have survived cool down in a dry environment, built up considerable thickness and strain energy, and have been somewhat damaged, such as by cyclic oxidation cracking. Indeed, a "sweet zone" can be defined that maximizes the observed effect as a function of all the relevant factors. Moisture has been postulated to serve as a source of interfacial hydrogen embrittlement derived from reaction with aluminum in the alloy at an exposed interface. The purpose of this monograph is to trace the close analogy of this phenomenon to other hydrogen effects, such as embrittlement of aluminides and blistering of alloys and anodic alumina films. A formalized, top-down, logic tree structure is presented as a guide to this discussion. A theoretical basis for interfacial weakening by hydrogen is first cited, as are demonstrations of hydrogen as a reaction product or detected interfacial species. Further support is provided by critical experiments that produce the same moisture effect, but by isolating hydrogen from other potential causative factors. These experiments include tests in H2-containing atmospheres or cathodic hydrogen charging.

Smialek, James L.

Moisture-Induced Delayed Alumina Scale Spallation on a Ni(Pt)Al Coating

Delayed interfacial scale failure takes place after cooling for samples of a Ni(Pt)Al-coated CMSX4 single crystal superalloy, cycled at 1150 C for up to 2000 hr. One sample exhibited premature coating grain boundary wrinkling, alumina scale spallation to bare metal, and a final weight loss of 3.3 mg/cm2 . Spallation under ambient conditions was monitored with time after cooldown and was found to continue for 24 hr. This produced up to 0.05 mg/cm2 additional loss for each hold, accumulating 0.7 mg/cm 2 (20 percent of the total) over the course of the test. After test termination, water immersion produced an additional 0.15 mg/cm2 loss. (A duplicate sample produced much less wrinkling and time dependent spalling, maintaining a net weight gain.) The results are consistent with the general phenomena of moisture-induced delayed spallation (MIDS) of mature, distressed alumina scales formed on oxidation resistant M-Al alloys. Relative ambient humidity is discussed as the factor controlling adsorbed moisture, reaction with the substrate, and hydrogen effects on interface strength.

Smialek, James L.

Environmental Barrier Coatings for Turbine Engines: A Design and Performance Perspective

Ceramic thermal and environmental barrier coatings (TEBC) for SiC-based ceramics will play an increasingly important role in future gas turbine engines because of their ability to effectively protect the engine components and further raise engine temperatures. However, the coating long-term durability remains a major concern with the ever-increasing temperature, strength and stability requirements in engine high heat-flux combustion environments, especially for highly-loaded rotating turbine components. Advanced TEBC systems, including nano-composite based HfO2-aluminosilicate and rare earth silicate coatings are being developed and tested for higher temperature capable SiC/SiC ceramic matrix composite (CMC) turbine blade applications. This paper will emphasize coating composite and multilayer design approach and the resulting performance and durability in simulated engine high heat-flux, high stress and high pressure combustion environments. The advances in the environmental barrier coating development showed promise for future rotating CMC blade applications.

Zhu, Dongming

Enigmatic Moisture Effects on Al2O3 Scale and TBC Adhesion

Alumina scale adhesion to high temperature alloys is known to be affected primarily by sulfur segregation and reactive element additions. However, adherent scales can become partially compromised by excessive strain energy and cyclic cracking. With time, exposure of such scales to moisture can lead to spontaneous interfacial decohesion, occurring while the samples are maintained at ambient conditions. Examples of this Moisture-Induced Delayed Spallation (MIDS) are presented for NiCrAl and single crystal superalloys, becoming more severe with sulfur level and cyclic exposure conditions. Similarly, delayed failure or Desk Top Spallation (DTS) results are reviewed for thermal barrier coatings (TBCs), culminating in the water drop failure test. Both phenomena are discussed in terms of moisture effects on bulk alumina and bulk aluminides. A mechanism is proposed based on hydrogen embrittlement and is supported by a cathodic hydrogen charging experiment. Hydroxylation of aluminum from the alloy interface appears to be the relevant basic reaction.