Epitaxial Fe/Y2O3 interfaces as a model system for oxide-dispersion-strengthened ferritic alloys
Not Available
Engineering topics
Publications and source records attributed to Shutthanandan, V..
Not Available
We examine the structure and composition of phase-pure epitaxial α-(Fe{sub 1−x}V{sub x}){sub 2}O{sub 3} thin films deposited on α-Al{sub 2}O{sub 3}(0001) substrates by oxygen-plasma-assisted molecular beam epitaxy for 0 ≤ x ≤ ∼0.5. The films crystallize in the corundum lattice, with vanadium substituting for iron throughout. Vanadium cations exhibit the expected 3+ charge state in the bulk, but exhibit higher valences nearer to the surface, most likely because of excess oxygen in interstitial sites near the surface. The extent of vanadium oxidation beyond the 3+ state is inversely proportional to x. The gradation of vanadium valence with depth has an impact on local bonding geometries, and could be highly significant in this material's efficiency as a photocatalyst.
14YWT oxide dispersion strengthened (ODS) ferritic steel was irradiated with of 5 MeV Ni2+ ions, at 300 °C, 450 °C, and 600 °C to a damage level of 100 dpa. The stability of Ti–Y–O nanoclusters was investigated by applying atom probe tomography (APT) in voltage mode, of the samples before and after irradiations. The average size and number density of the nanoclusters was determined using the maximum separation method. These techniques allowed for the imaging of nanoclusters to sizes well below the resolution limit of conventional transmission electron microscopy techniques. The most significant changes were observed for samples irradiated at 300 °C where the size (average Guinier radius) and number density of nanoclusters were observed to decrease from 1.1 nm to 0.8 nm and 12 × 1023 to 3.6 × 1023, respectively. In this study, the nanoclusters are more stable at higher temperature.
14YWT oxide dispersion strengthened (ODS) ferritic steel was irradiated with of 5 MeV Ni2+ ions, at 300 C, 450 C, and 600 C to a damage level of 100 dpa. The stability of Ti–Y–O nanoclusters was investigated by applying atom probe tomography (APT) in voltage mode, of the samples before and after irradiations. The average size and number density of the nanoclusters was determined using the maximum separation method. These techniques allowed for the imaging of nanoclusters to sizes well below the resolution limit of conventional transmission electron microscopy techniques. The most significant changes were observed for samples irradiated at 300 C where the size (average Guinier radius) and number density of nanoclusters were observed to decrease from 1.1 nm to 0.8 nm and 12 1023 to 3.6 1023, respectively. In this study, the nanoclusters are more stable at higher temperature.
Tailored metal alloy thin film-oxide interfaces generated using molecular beam epitaxy (MBE) deposition of alloy thin films on a single crystalline oxide substrate can be used for detailed studies of irradiation damage response on the interface structure. However, the presence of nanoscale phase separation in the MBE grown alloy thin films can impact the metal-oxide interface structure. Due to nanoscale domain size of such phase separation, it is very challenging to characterize by conventional techniques. Therefore, laser assisted atom probe tomography (APT) was utilized to study the phase separation in epitaxial Cr{sub 0.61}Mo{sub 0.39}, Cr{sub 0.77}Mo{sub 0.23}, and Cr{sub 0.32}V{sub 0.68} alloy thin films grown by MBE on MgO(001) single crystal substrates. Statistical analysis, namely frequency distribution analysis and Pearson coefficient analysis of experimental data was compared with similar analyses conducted on simulated APT datasets with known extent of phase separation. Thus, the presence of phase separation in Cr-Mo films, even when phase separation was not clearly observed by x-ray diffraction, and the absence of phase separation in the Cr-V film were confirmed.
Moisture plays a significant role in influencing the mechanical behavior and long-term durability of polymer matrix composites (PMC’s). The common methods used to determine the moisture diffusion coefficients of PMCs are based on the solution of Fickian diffusion in the one-dimensional domain. Fick’s Law assumes that equilibrium between the material surface and the external vapor is established instantaneously. A time dependent boundary condition has been shown to improve correlation with some bulk diffusion measurements, but has not been validated experimentally. The surface moisture content in a Toray 800S/3900-2B toughened quasi-isotropic laminate system, [0/±60]s, was analyzed experimentally using Nuclear Reaction Analysis (NRA). It was found that the surface moisture content showed a rapid increase to an intermediate concentration C0, followed by a slow linear increase to the saturation level.
In0.20Ga0.80N/GaN multi-quantum wells grown on [0001]-oriented GaN substrates with and without an InGaN buffer layer were characterized using three-dimensional atom probe tomography. In all samples, the upper interfaces of the QWs were slightly more diffuse than the lower interfaces. The buffer layers did not affect the roughness of the interfaces within the quantum well structure, a result attributed to planarization of the surface of the 1st GaN barrier layer which had an average root-mean-square roughness of 0.177 nm. The In and Ga distributions within the MQWs followed the expected distributions for a random alloy with no indications of In clustering.
This special issue of Nuclear Instruments and Methods in Physics Research B contains the proceedings of the 21st International Conference on Ion Beam Analysis (IBA – 2013). This conference was held in Marriott Waterfront in Seattle, Washington, USA during June 23–28, 2013.
Titanium nitride (TiNx) coatings were grown by magnetron sputtering onto Si(1 0 0) substrates by varying time of deposition to produce coatings with variable thickness (dTiN) in the range of 20-120 nm. TiNx coatings were characterized by studying their structure, composition, and mechanical properties. Nuclear reaction analysis (NRA) combined with Rutherford backscattering spectrometry (RBS) analyses indicate that the grown coatings were stoichiometric TiN. Grazing incidence X-ray diffraction (GIXRD) measurements indicate that the texturing of TiN coatings changes as a function of dTiN. The (1 1 1) and (0 0 2) peaks appear initially; (1 1 1) becomes intense while (0 0 2) disappears with increasing dTiN. Dense, columnar grain structure was evident for all the coatings in electron microscopy analyses. The residual stress for TiN coatings with dTiN~120 nm was 1.07 GPa in compression while thinner samples exhibit higher values of stress.
The Stopping and Range of Ions in Matter (SRIM) code has been widely used to predict nuclear stopping power and angular distribution of ion-solid collisions. However, experimental validation of the predictions is insufficient for slow heavy ions in nonmetallic compounds. In this work, time-of-flight secondary ion mass spectrometry (ToF-SIMS) is applied to determine the angular distribution of 1 MeV Au ions after penetrating a Si 3 N 4 foil with a thickness of ~100 nm. The exiting Au ions are collected by a Si wafer located ~14 mm behind the Si 3 N 4 foil, and the resulting 2-dimensional distribution of Au ions on the Si wafer is measured by ToF-SIMS. The SRIM-predicted angular distribution of Au ions through the Si 3 N 4 thin foil is compared with the measured results, indicating that SRIM slightly overestimates the nuclear stopping power by up to 10%. In addition, thickness reduction of the suspended Si3N4 foils induced by 1 MeV Au ion irradiation is observed with an average loss rate of ~107 atom/ion.
Germanium oxide (GeO x ) films were grown on (1 0 0) Si substrates by reactive Direct-Current (DC) magnetron sputter-deposition using an elemental Ge target. The effects of oxygen gas fraction, Г = O 2 /(Ar + O 2 ), on the deposition rate, structure, chemical composition and optical properties of GeOx films have been investigated. The chemistry of the films exhibits an evolution from pure Ge to mixed Ge + GeO + GeO 2 and then finally to GeO 2 upon increasing Г from 0.00 to 1.00. Grazing incidence X-ray analysis indicates that the GeO x films grown were amorphous. The optical properties probed by spectroscopic ellipsometry indicate that the effect of Г is significant on the optical constants of the GeO x films. The measured index of refraction (n) at a wavelength (λ) of 550 nm is 4.67 for films grown without any oxygen, indicating behavior characteristic of semiconducting Ge. The transition from germanium to mixed Ge + GeO + GeO 2 composition is associated with a characteristic decrease in n (λ = 550 nm) to 2.62 and occurs at Г = 0.25. Finally n drops to 1.60 for Г = 0.50–1.00, where the films become GeO 2 . A detailed correlation between Г, n, k and stoichiometry in DC sputtered GeO x films is presented and discussed.
The structural properties of high-quality epitaxial (Fe1-xCrx)2O3 thin films are investigated across the composition range. Epitaxial films are deposited on a-Al2O3(0001) substrates by oxygen-plasma-assisted molecular beam epitaxy. Corundum (Fe1-xCrx)2O3 supercells relaxed by density functional theory confirm that the non-linear behavior of the bulk lattice parameters originates in the magnetic structure of the alloy films. High-resolution x-ray diffraction reveals the degree of epitaxial strain relaxation in the films, with Cr-rich films remaining partially strained to the Al2O3 substrate. For intermediate compositions, a lattice expansion and non-Poisson-like tetragonal distortion are found. Scanning transmission electron microscopy and electron energy loss spectroscopy reveal a columnar grain structure in the films, with uniform mixing of cations on the nanometer scale. Oxygen non-stoichiometry is quantified by non-Rutherford resonant elastic scattering measurements utilizing 3.04 MeV He+. Intermediate-composition films are found to be slightly over-stoichiometric, resulting in the observed lattice expansion. Cr-rich films, in contrast, appear to be slightly oxygen deficient. A model is proposed to explain these results based on the energetics of oxygen defect formation and rate of oxygen diffusion in the corundum lattice. Compressive biaxial strain is found to reduce the bandgap of epitaxial Cr2O3 relative to the bulk value. The relationships which are elucidated between epitaxial film structure and optical properties can be applied to bandgap optimization in the (Fe,Cr)2O3 system.
Molecular dynamics (MD) simulations were employed with empirical potentials to study the effects of multilayer interfaces and interface spacing in Al-Ti nanolayers. Several model interfaces derived from stacking of close-packed layers or face-centered cubic \{100\} layers were investigated. The simulations reveal significant and important asymmetries in defect production with $\sim$60\% of vacancies created in Al layers compared to Ti layers within the Al-Ti multilayer system. The asymmetry in the creation of interstitials is even more pronounced. The asymmetries cause an imbalance in the ratio of vacancies and interstitials in films of dissimilar materials leading to $>$90\% of the surviving interstitials located in the Al layers. While in the close-packed nanolayers the interstitials migrate to the atomic layers adjacent to the interface of the Al layers, in the \{100\} nanolayers the interstitials migrate to the center of the Al layers and away from the interfaces. The degree of asymmetry and defect ratio imbalance increases as the layer spacing decreases in the multilayer films. Underlying physical processes are discussed including the interfacial strain fields and the individual elemental layer stopping power in nanolayered systems. In addition, experimental work was performed on low-dose (10$^{16}$ atoms/cm$^2$) helium (He) irradiation on Al/Ti nanolayers (5 nm per film), resulting in He bubble formation $\sim$1 nm in diameter in the Ti film near the interface. The correlation between the preferential flux of displaced atoms from Ti films to Al films during the defect production that is revealed in the simulations and the morphology and location of He bubbles from the experiments is discussed.
The interfacial region between graphene and an imidazolium based ionic liquid is studied using spectroscopic analysis and computational modelling. This combined approach reveals that the molecular level structure of the interfacial region is significantly influenced by functional group defects on the graphene surface.The combined experimental and computational study reveals that the molecular structure at interfacial region between graphene and imidazolium based ionic liquid is defined by the hydroxyl functional groups on the graphene surface
Epitaxial thin films of CrxV1-x over the entire composition range were deposited on MgO(001) by molecular beam epitaxy. The films exhibited the expected 45° in-plane rotation with no evidence of phase segregation or spinodal decomposition. Pure Cr, with the largest lattice mismatch to MgO, exhibited full relaxation and cubic lattice parameters. As the lattice mismatch decreased with alloy composition, residual epitaxial strain was observed. For 0.2 ≤ x ≤ 0.4 the films were coherently strained to the substrate with associated tetragonal distortion; near the lattice-matched composition of x = 0.33, the films exhibited strain-free pseudomorphic matching to MgO. Unusually, films on the Cr-rich side of the lattice-matched composition exhibited more in-plane compression than expected from the bulk lattice parameters; this result was confirmed with both x-ray diffraction and Rutherford backscattering spectrometry channeling measurements. Although thermal expansion mismatch in the heterostructure may play a role, the dominant mechanism for this phenomenon is still unknown. High resolution transmission electron microscopy was utilized to characterize the misfit dislocation network present at the film/MgO interface. Dislocations were found to be present with a non-uniform distribution, which is attributed to the Volmer-Weber growth mode of the films. The CrxV1-x / MgO(001) system can serve as a model system to study both the fundamentals of defect formation in bcc films and the interplay between nanoscale defects such as dislocations and radiation damage.
Nanostructured yttria-stabilized hafnia (YSH) coatings were grown on α-Al2O3 substrates with variable coating thickness in a wide range of ~50 nm to 1 μm. Microstructure and thermal oxidation behavior of the grown YSH coatings were studied employing X-ray diffraction (XRD), Rutherford backscattering spectrometry (RBS), scanning electron microscopy (SEM) and isothermal furnace oxidation testing. The effect of coating thickness on the crystal structure, surface/interface morphology and thermal oxidation was investigated. X-ray diffraction analyses revealed the formation of monoclinic phase for relatively thin coatings (b100 nm) indicating that the interfacial phenomena play a dominant role in phase stabilization. The evolution towards stabilized cubic phase with increasing coating thickness is observed. The SEM results indicate the dense, columnar structure of YSH coatings as a function of thickness. Thermal oxidation measurements indicate the enhanced hightemperature oxidation resistance of cubic YSH coatings.
The interface between polar perovskite LaCrO3 (LCO) and non-polar SrTiO3(001) (STO), grown by molecular beam epitaxy, is examined using a combination of electron microscopy, spectroscopy, and Rutherford backscattering spectrometry. The LCO/STO(001) interface is insulating, a potential counter example for the claim that polar/nonpolar perovskite interfaces should be conductive by virtue of an electronic reconstruction to alleviate the polar discontinuity. The A-site cations of these ABO3 perovskites are found to diffuse across the interface to a greater extent than the B-site cations, based on high angle annular dark field scanning transmission electron microscopy (HAADF-STEM), energy dispersive x-ray spectroscopy (EDS) and electron energy loss spectroscopy (EELS). The B-site cation valences are shown to be partially reduced near the interface by analysis of EELS near-edge structures. The location and direction of these electronic modifications do not intuitively compensate the charge imbalance imposed by uneven cation inter-diffusion, and yet both the film and interface are insulating. These results highlight the importance of both the physical and electronic structure of such complex interfaces in determining their characteristics. Furthermore, the extent of inter-diffusion is shown to increase with increasing LCO film thickness, suggesting a potential mechanism behind the critical thickness for interfacial conductivity in other polar/non-polar oxide systems, and a fundamental limitation on the formation of abrupt interfaces in LCO/STO(001).
A novel write-once-read-many (WORM) optical stack on Mylar tape is proposed as a replacement for magnetic tape for archival data storage. This optical tape contains a cosputtered bismuth–tellurium–selenium (BTS) alloy as the write layer sandwiched between thin, protective films of reactively sputtered carbon. The composition and thickness of the BTS layer were confirmed by Rutherford Backscattering (RBS) and atomic force microscopy (AFM), respectively. The C/BTS/C stack on Mylar was written to/marked by 532 nm laser pulses. Under the same conditions, control Mylar films without the optical stack were unaffected. Marks, which showed craters/movement of the write material, were characterized by optical microscopy and AFM. The threshold laser powers for making marks on C/BTS/C stacks with different thicknesses were explored. Higher quality marks were made with a 60× objective compared to a 40× objective in our marking apparatus. Finally, the laser writing process was simulated with COMSOL.