Accelerated Corrosion Testing of Cold Spray Coatings on 304L in Chloride Environments.
Abstract not provided.
Engineering topics
Publications and source records attributed to Ross, Kenneth A..
Abstract not provided.
Here, friction surfacing (FS) was investigated as a method for sealing 50 μm wide thru-cracks in 3-mm-thick 304L stainless steel (304L) plate. Friction surfacing was performed using two sizes of 304L consumable rod, with diameters of 9.52 mm and 12.7 mm, on two substrate conditions (clean and oxidized). Friction surfacing was able to deposit a 600 μm thick coating and repair cracks to a depth of 100 μm - 200 μm below the original surface, when using the 12.7-mm-diameter consumable rod for both substrate conditions. Helium leak rates of 10 -10 atm-cc/s were achieved on crack repairs, designating them as leak-tight by the ANSI N14.5 standard. Optical and scanning electron microscopy were used to investigate the coating microstructure and bond interfaces. In this study, the 12.7-mm-diameter rod performed better with disruption of the oxide layer on the oxidized substrate and providing a more homogenous coating. Mechanical properties of the coated samples were evaluated by performing micro-indentation, tensile, bending, and adhesion testing. Higher hardness in the coatings was observed due to the fine equiaxed grains resulting from dynamic recrystallization. Complete consolidation of plastically deformed material on the substrate and a strong diffusion bond across the interface was observed. This was reflected in tensile and bending properties of the FS coatings being comparable to those of uncoated specimen. No delamination of the FS coating was observed during adhesion testing. The results demonstrate that friction surfacing is a viable option to seal cracks in stainless steels.
The microstructural evolution under the extreme environments imposed during cold spray deposition of cermet coatings and the microstructural recovery during post-processing annealing treatments is rather complex and not well understood. Here, Ni-Yttria cermet coatings on an SS304 substrate were produced using cold spray technique, resulting in a bimodal grain structure. The grain growth, phase stability, hardness, and wear properties are observed in as-deposited and annealed (at 400 °C) Ni-Yttria and pure Ni coatings. A multimodal microstructural characterization using electron microscopy, and atom probe tomography shows the structural and compositional stability of yttria particles and Ni grains. A fragmentation of Y-rich particles and dispersion in Ni was observed, however, no forced mixing/dissolution of Y in Ni is detected. Nano-yttria dispersed within the Ni grains slowed the grain growth during annealing. After annealing, Yttria reinforced coating was 1.5 times harder and showed better thermal and mechanical stability compared to the Ni coating.
The purpose of this work is to investigate the use of cold spray for repair and mitigation of chloride-induced stress corrosion cracking (CISCC) in dry cask storage system (DCSS) canisters to ensure their integrity far beyond their original license period. This report provides a viability analysis of cold spray for repair and mitigation of CISCC in DCSS canisters to extend canister life.
This report provides an overview of cold spray (CS) technology as it relates to repair and fabrication of metal alloys in the nuclear power industry. CS is a relatively new technology with applications established in other industries (e.g., aerospace, defense), and greater use of CS is anticipated within the nuclear power industry. This report is prepared in support of the United States Nuclear Regulatory Commission (NRC) Action Plan for Advanced Manufacturing Technologies (AMTs) Rev. 1, which includes objectives to identify the AMTs most likely to be used for nuclear power applications that require NRC approval, and to prepare NRC staff to review regulatory submittals containing components manufacturing using AMTs. In addition to providing an overview of CS technology, this report highlights engineering and scientific knowledge gaps of CS and rates the size of the knowledge gaps. It also assesses importance rankings of the knowledge gaps as they relate to several application categories. The application categories considered in this exercise include factory-applied CS for chloride induced stress corrosion cracking (CISCC) mitigation, field CISCC repair, light water reactor (LWR) factory structural fabrication, and LWR field dimensional restoration and corrosion protection. The combination of a knowledge gap size rating and importance ranking for an application can be used to prioritize additional data or information gathering efforts.
Thick plate and lower temperature friction stir welding results in good post-weld properties by welding at very low tool rotational speeds. Low speeds cause large variations in the measured shoulder temperature, making temperature control difficult. This paper describes a computationally light method to correct for oscillating measured temperatures. Data is collected over the previous two revolutions and used to build a compensation table and calculate a derivative. In simulation, measured temperature variations are reduced by a factor of five to ten. Temperature data is preserved and not cornered, nor is any time delay induced by this method, unlike with filtering methods.
There is an urgent need for repair of hydropower components that have undergone damage due to cavitation. Conventional repair methods involve melting of materials and can deteriorate material properties and cause distortion. This study investigated the relevant properties of different materials using solid phase processing—cold spray technology. Stainless steel (SS) 316, Inconel 625 and CrC-NiCr materials were cold spray deposited onto base metal SS 316, respectively. Cold spray achieved dense uniform deposits with low level porosity, and intimate contact between the deposit and the base metal was observed. Severe plastic deformation imparted during the cold spray process resulted in significant grain size refinement, nanostructured regions were observed in the deposits across the interfacial area. Cold sprayed deposits exhibited elevated hardness in contrast to that of the base metal SS 316. The cavitation erosion resistance of the deposits was evaluated with a cavitation erosion jet adhering to ASTM G134. Both SS 316 and Inconel 625 achieved better cavitation erosion resistance when compared to that of the SS 316 base metal, with the former exhibiting close to a 4 times improvement.
The lack of a permanent spent nuclear fuel repository means utilities are faced with extending licenses for dry cask storage systems (DCSS) canisters far beyond their original 20-year license period. DCSS canisters are made from austenitic stainless steels (SSs) and fabricated using fusion welds. High heat input and melting associated with fabrication welds causes material around the weld to be susceptible to chloride-induced stress corrosion cracking (CISCC). The purpose of the work reported here is to investigate the use of cold spray for repair and mitigation of CISCC in DCSS canisters to ensure integrity far beyond their original license period. This report presents an analysis of cold spray for canister life extension, a summary of related efforts, relevant technology down selections, work accomplished, and future efforts relative to use of cold spray for repair and mitigation of CISCC in DCSS canisters.
A feasibility study of the cold spray deposition process of 304L stainless steel on 304L stainless steel substrates as a mitigation method for chloride-induced stress corrosion cracking (CISCC) has been investigated under various substrate conditions. The study is aimed at the application of this technology to mitigate CISCC that may potentially occur in or nearthe fusion welded regions of stainless steel canisters in Dry Cask Storage System (DCSS) for used nuclear fuels. Spherical gas-atomized 304L stainless steel powder, in the size range of 25 µm to 44 µm, was used as a feedstock powder for the cold spray process. The powder was deposited on four types of 304L substrates with various surface conditions: as-polished, oxidized, cold-rolled, plates with prototypical CISCC. The effects of cold spray parameters on quality of cold spray coatings were investigated. Thickness, porosity, and phases in the as-deposited materials were evaluated using scanning electron microscopy (SEM) and X-ray diffraction (XRD), and correlated with microhardness and adhesion strength measured via micro-indentation and ASTM C633 pulling test, respectively. XRD analysis of the coatings was also conducted to examine the effects of cold spray condition on residual stress state in the coating. Detailed cross-sectional examination of coating/substrate interfaces was performed with transmission electron microscopy (TEM) equipped with energy dispersive spectroscopy (EDS). Dense and continuous coatings with good adhesion strength and hardness were produced for the various substrate conditions by adjusting cold spray parameters. The results demonstrate that cold spray stainless steel coating is a viable option to provide a physical barrier against CISCC in fusion weld regions of stainless steel in corrosive chloride salt-bearing environments.
Friction stir dovetailing (FSD) is a new dissimilar material joining process that simultaneously forms a mechanical interlock and metallurgical bond at the dissimilar material interface. This work presents development of a modeling and simulation approach to predict mechanical performance of FSD thick section aluminum to steel joints. A finite element analysis (FEA) was carried out in order to predict the load-carrying capacity and failure location for aluminum thicknesses between 12.7 mm and 50.8 mm with different numbers of dovetails. The numerical results and corresponding experimental investigation are in agreement and suggest that the developed methods can be used effectively for design and analysis of FSD joints using standard FEA tools.
The purpose of this work is to investigate the use of cold spray and friction stir welding or processing (FSW/P) for repair and mitigation of chloride-induced stress corrosion cracking (CISCC) in dry cask storage system (DCSS) canisters to ensure integrity far beyond their original license period. This report provides a viability analysis of cold spray and friction stir welding for repair and fabrication of DCSS canisters. This report presents experimental work and a research strategy to optimize and evaluate cold spray and FSW/P for CISCC resistance. The literature reports that the following three conditions must exist for CISCC to occur: tensile stress, corrosive environment, and susceptible material. These conditions must be understood and accounted for while evaluating CISCC susceptibility. Furthermore, non-obvious factors, such as surface conditions and geometric confinement, can dramatically increase the intensity of one or more of the three listed conditions for CISCC. Arc welding should be considered for either temporary or permanent repair when combined with a mitigation technology. It is known that alloys used in the existing inventory of spent nuclear fuel storage canisters become sensitized in areas around fusion welds. Technologies, such as cold spray or FSW, can mitigate the sensitization caused by fusion welds. FSW/P and cold spray, potential alternatives for fabrication and repair, are solid-phase processes. No melting occurs and the energy input can be controlled such that no harm is done to the base metal during these processes. FSW/P should be considered for use in new fabrication of canisters and repair of existing canisters. Low heat input and grain refinement result in material with improved mechanical properties and comparable generalized corrosion performance relative to base metal. FSW/P offers the potential of through-thickness CISCC resistance. Cold spray should be considered for production, mitigation, and repair of canisters. Cold spray has demonstrated the ability to deposit stainless steel, Inconel alloys, and other alloys on stainless steel 304L such that galvanic potential is matched and resistance to pitting is improved. The technical basis for cold spray mitigation and repair within the overpack using remote robotic equipment is established. A non-obvious application to the research community is the sealing of crevices. All reported instances of CISCC in the fielded nuclear applications were associated with crevice corrosion. This can be avoided by cold spraying to seal crevices. The bulk of the work planned for FY 2020 will be generating coupons for CISCC testing by collaborative projects at Pacific Northwest National Laboratory and Sandia National Laboratories. First an exploratory study will be executed that will include screening studies and process optimization. This task will identify the effect of process parameters on microstructure and CISCC resistance. Optimized parameters will be used to produce a smaller number of coupons for full testing and evaluation. Test methods for evaluating CISCC resistance must meet the following criteria: (1) normalized surface geometry and exposed process microstructure, (2) account for residual stresses, (3) be in a controlled and appropriate test environment, and (4) be numerically quantifiable and repeatable. Failure to meet these criteria could lead to results that cannot be used for comparative analysis of processes and materials.
A method for solid state joining of dissimilar materials using a friction stir welding device wherein a pin is inserted through an aperture defined in a first material and a second material to hold the materials together and then held in place by friction stir welding a portion of the pin to a material adjacent said pin, or by friction stir welding a cap or plug that holds the pin in place to the adjacent material. The result is a connection or join wherein the central portion of the pin is not friction stir welded but the portions holding the pin in place (the ends or caps) generally are.
Lightweighting of vehicles and portable structures is an important undertaking. Multi-material design is required to achieve conflicting design targets such as cost, stiffness, and weight. Friction stir welding (FSW) variants, such as friction stir dovetailing and friction stir scribe, are enabling technologies for joining of dissimilar metals. This work shows that FSW variants are capable of joining aluminum to steel. Characteristics of metallurgical bonding at the dissimilar material interface are strongly affected by weld temperature. Control of FSW process temperature enables metallurgical bonding with suppressed formation of intermetallics at the dissimilar material interface resulting in improved mechanical properties relative to competing techniques. Temperature control is a powerful tool for process development and to ensure weld quality of dissimilar material welds.
Friction stir dovetailing (FSD) was used to join 0.5 inch (12.7 mm) AA7099 to 0.5 inch (12.7 mm) Ni-Cr-Mo steel in a lap configuration. Two new FSD approaches are reported that significantly reduce zinc embrittlement of Fe-Al intermetallic compounds (IMCs) which form during conventional friction stir welding (FSW). The first method uses the general FSD approach where a custom designed tool is employed to extrude the AA7099 into the pre-machined dovetail groove of underlying steel by forming mechanical interlocking and metallurgical bonding simultaneously. The second method uses a two-step approach where FSD of AA6061 is first used to form a silicon-rich Fe-Al IMC within the dovetail groove. AA7099 plate is then joined to the AA6061 within the dovetail using conventional FSW. A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.
Ultrasound sensors and inspection systems are frequently used to generate acoustic waves in metal structures capable of detecting and characterizing cracks, pits, erosion, inclusions, weld anomalies, and other material and structural features. One significant problem with piezoelectric transducers is the difficulty to achieve good coupling between the transducer and the surface being examined. This is particularly true in harsh conditions with high temperatures, cyclical hot and cold temperatures, highly radioactive fields found near nuclear reactors or spent nuclear fuel, caustic or corrosive fluids, and other extreme environmental conditions, as well as in long-term monitoring applications where repair or replacement of the sensor is difficult or expensive. Typically, coupling between the surface and the transducer is achieved with water, gel, grease, viscous shear coupling material, or pressure, which might not be possible or appropriate for long-term applications in which the impedance -matching materials wear away, evaporate, or simply stop functioning due to changes in surface conditions. Fluid couplings can evaporate or drain away from the transducer-substrate interface; glue- based couplings may foul or fail and are notoriously unreliable at high temperatures and in radioactive environments. This work explores the behavior of a magnetostrictive cold-spray patch that is metallurgically bonded to a stainless steel inspection target surface, and compares it to the performance of a standard adhesively-bonded ferrous-cobalt magnetostrictive strip solution. Cold-spray is a coating process where 10 –100 micron diameter powdered metal is accelerated to Mach 2 to Mach 3 (2–3 × speed of sound) and impacted on the surface to be coated. Each powder particle forms a kinetic bond with the substrate or other coating particles to produce a metallurgically bonded layer. If the powder is nickel or cobalt with high magnetostrictive coefficients, this surface can serve as the base of a magnetostrictive sensor suitable for crack or pitting-damage inspection and monitoring that is not subject to temporal or environmental degradation.
This paper describes a technology review of non-destructive examination (NDE) methods that can be applied to cold spray coatings. Cold spray is a process for depositing metal powder at high velocity so that it bonds to the substrate metal without significant heating that would be likely to cause additional residual tensile stresses. Coatings in the range from millimeters to centimeters are possible at relatively high deposition rates. Cold spray coatings that may be used for hydroelectric components that are subject to erosion, corrosion, wear, and cavitation damage are of interest. The topic of cold spray NDE is treated generally however and may be considered applicable to virtually any cold spray application except where there are constraints of the hydroelectric component application that bear special consideration. Hydroelectric turbine components are primarily made from low carbon and austenitic stainless steels. They are typically very large components that are partially assembled on-site. Transport of these components within the hydroelectric facility and away from the hydroelectric facility is challenging due to the component’s size and weight, high cost of disassembly, and the confined space of the dam. One method for prolonging component life is application of cold spray and thermal powder metal coatings to the components most susceptible to erosion, corrosion, cracking, and mechanical wear. Process controls and visual inspections have historically been applied to cold spray application; however, quantitative NDE could detect anomalies not readily apparent from such a visual examination. Optical profilometry, Eddy current, ultrasound, and hardness tests are shown for one set of good, fair, and poor Nickle-Chrome (NiCr) on 304 stainless steel (304SS) cold spray samples to demonstrate inspection possibilities. The primary indicator of cold spray quality is the cold spray porosity that is most directly measured with witness-sample destructive examinations (DE) – mostly photo-micrographs. These DE generated porosity values are correlated with optical profilometry, eddy current, ultrasound, and hardness test NDE methods to infer the porosity and other Information of interest. These parameters of interest primarily include: • Porosity primarily caused by improper process conditions (temperature, gas velocity, spray standoff, spray angle, powder size, condition, surface cleanliness, surface oxide, etc.). • Presence/absence of the cold spray coating including possible over-sprayed voids • Coating thickness Optical profilometry measurements of surface roughness trended with porosity plus if compared with a reference measurement or reference drawing would provide information on the coating thickness. Ultrasound could provide similar surface profile information plus attenuation measurements trended with porosity. The ultrasound measurements however may be limited to geometries where the substrate back-wall is normal to the cold spray surface and not too thick. Eddy current showed a strong correlation with porosity. Eddy currents can also be sensitive to cracks and do not need fluid coupling to make measurements. Eddy currents however are not sensitive to coating thicknesses in most cases. Vickers hardness measurements also tracked well with porosity. These types of hardness measurements however are also not sensitive to coating thickness. An NDE program may include multiple measurements. Acknowledgement: This work is sponsored by Bonneville Power Administration (BPA) under their technology innovation project program. Such support does not constitute BPA endorsement of views expressed in this work.
Maintaining consistent tool depth relative to the part surface is a critical requirement for many Friction stir processing (FSP) applications. Force control is often used with the goal of obtaining a constant weld depth. When force control is used, if weld temperature decreases, flow stress increases and the tool is pushed up. If weld temperature increases, flow stress decreases and the tool dives. These variations in tool depth and weld temperature cause various types of weld defects. Robust temperature control for FSP maintains a commanded temperature through control of the spindle axis only. Robust temperature control and force control are completely decoupled in control logic and machine motion. This results in stable temperature, force and tool depth despite the presence of geometric and thermal disturbances. Performance of this control method is presented for various weld paths and alloy systems.
The Nuclear Regulatory Commission has identified chloride-induced stress corrosion cracking (CISCC) of austenitic stainless steel dry cask storage systems (DCSS) as an area of great concern. Friction Stir Processing (FSP) was used to repair laboratory-generated stress corrosion cracking (SCC) in representative stainless steel 304 coupons. Results of this study show FSP is a viable method for repair and mitigation CISCC. This paper highlights lessons learned and developed techniques relative to FSP development for crack repair in sensitized thick section stainless steel 304. These include: development of process parameters, welding at low spindle speed, use of weld power and temperature control and optimization of these controls. NDE and destructive analysis are also presented to demonstrate effectiveness of the developed methods for SCC crack repair.