Containerless Liquid to Solid Nucleation Pathways in Two Representative Grades of Commercially Available Zirconium
Experimental measurements were conducted to determine the solid metal nucleation pathways of radiatively cooling, molten zirconium spheres of two different commercially available purity grades in a high-vacuum, high-temperature electrostatic levitator. The ensemble distribution of maximum undercooling temperatures was interpreted using Poisson statistics to determine the temperature dependence of the solid metal nucleation rate. For a sample of nominally 99.95% pure zirconium, the results are consistent with heterogeneous solid metal nucleation either on static catalyst particles at least approx. 30 nm diameter or on a surface coating. For a sample of nominally 99% pure zirconium, however, it appears that heterogeneous solid metal nucleation occurred either on a polydispersion of approx. 10 nm (mean diameter) static catalyst particles or on dynamic catalyst particles that precipitated from a solution that became supersaturated as the melt cooled.