Direct Feed High-Level Waste APPS Model Glass Testing (DFHLW APPS) Matrix

This report summarizes the data collected during the batching and melting of the Direct Feed High-Level Waste APPS Model Glass Matrix (DFHLW APPS) to serve as a quality-assured validation of the Aspen Process Performance Simulation (APPS) formulation method. Of 15 glasses tested, 12 satisfied all target property constraints. Two glasses, APPS-05 and -06, formed nepheline on canister centerline cooling heat-treatment and failed the Product Consistency Test response limits. Glass APPS-07-2 formed unacceptably high concentrations of crystals (primarily Na3Nd(PO4)2) when heat treated at 950 °C. All other glasses were found to be satisfactory. The measured property values were compared to predicted values from a set of current models. In many cases the current models were found to be inadequate for design of DFHLW glasses. These models are being adjusted to correct for mispredictions. Other models, e.g., density, toxicity characteristic leaching procedure, and sulfur solubility, are adequate for formulation of DFHLW glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Enhanced Hanford Low-Activity Waste Glass Property Data Development: Phase 5 and Phase 6

This report summarizes the data collected on two test matrices of low-activity waste (LAW) glass compositions intended to expand the composition-property database: Low-Activity Waste (LAW) Phase 5: Expansion of LAW Glass Composition Boundaries and LAW Phase 6: High PCT and VHT Response Glass Matrix. Both matrix glass compositions were statistically designed to expand the LAW glass composition region. The analyses performed on these glasses include chemical composition (for target compositional verification), density, viscosity, electrical conductivity, crystal fraction, container centerline cooling with crystal identification, the product consistency test (PCT) response, the vapor hydration test (VHT) response, and sulfur solubility. Because of the slightly different scope of the two matrices, not all methods were applied to both matrices. Specifically, the following measurements were taken only on the LAW Phase 5: Expansion of LAW Glass Composition Boundaries glasses: crystal fraction as a function of temperature, density (ρ), viscosity (η), and electrical conductivity (EC, e). Combined, these data contribute a significant amount, 51 glasses, to the database for high LAW loaded enhanced waste glasses. Most of these data are focused near the boundaries of acceptable PCT and VHT responses, where prediction uncertainties are most impactful.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Product Consistency Test and Vapor Hydration Test Comparisons of a Radioactive Hanford Waste Glass with its Non-Radioactive Simulant Glass

Product Consistency Tests (PCT) and Vapor Hydration Tests (VHT) were performed on a radioactive glass made from Hanford tank AP-107 waste (i.e., R-AP-107) and its non-radioactive equivalent glass made from simulated tank waste (i.e., S-AP-107). The radioactive and non-radioactive experiments were conducted in parallel with identical equipment, protocols, and staff to remove additional experimental uncertainties. PCT and VHT results are reported for all samples and are shown in Table S.1. Average normalized mass loss of B ( NL B ) and Na ( NL Na ) calculated from the three replicate test results for each glass with their respective standard deviations (SD) are presented for PCT results while individual VHT rates ( r VHT ) with their propagated errors ( σ r prop ) from individual thickness measurements on each sample are presented for the VHT results. Some VHT samples experienced more than 50% evaporation loss during the experiments. However, no visible alteration was detected on any VHT samples regardless on the amount of evaporation loss detected as shown in Table S.1.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Review and Experimental Comparison of the Durability of Iodine Waste Forms in Semi-Dynamic Leach Testing

To ensure the safe disposal of radioiodine-containing nuclear wastes, a durable iodine waste form (IWF) is required. Many IWFs have been developed and evaluated for chemical durability using a wide range of test methods, making direct comparisons difficult as highlighted in this work through a review of available IWF corrosion data. To move toward a common dataset, a semi-dynamic leach test suite was experimentally demonstrated using several IWF types, providing standard comparisons. The results highlighted clear differences in corrosion resistance between various IWFs. This test suite is suggested for future studies to generate comparable data for a common dataset.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of Al:Si and (Al+Na):Si Ratios on the Properties of the International Simple Glass, Part II: Structure

High-alumina containing high-level waste (HLW) will be vitrified at the Waste Treatment Plant at the Hanford Site. The resulting glasses, high in alumina, will have distinct composition-structure-property (C-S-P) relationships compared to previously studied HLW glasses. These C-S-P relationships determine the processability and product durability of glasses and therefore must be understood. The main purpose of this study is to understand the detailed structural changes caused by Al:Si and (Al+Na):Si substitutions in a simplified nuclear waste model glass (ISG, International Simple Glass) by combining experimental structural characterizations and molecular dynamics (MD) simulations. The structures of these two series of glasses were characterized by neutron total scattering and 27Al, 23Na, 29Si, and 11B solid-state nuclear magnetic resonance (NMR) spectroscopy. Additionally, MD simulations were used to generate atomistic structural models of the borosilicate glasses and simulation results were validated by the experimental structural data. Short-range (e.g., bond distance, coordination number, etc.) and medium-range (e.g., oxygen speciation, network connectivity, polyhedral linkages) structural features of the borosilicate glasses were systematically investigated as a function of the degree of substitution. The results show that bond distance and coordination number of the cation-oxygen pairs are relatively insensitive to Al:Si and (Al+Na):Si substitutions with the exception of the B-O pair. Additionally, the Al:Si substitution results in an increase of tri-bridging oxygen species, while (Al+Na):Si substitution creates non-bridging oxygen species. Charge compensator preferences were found for Si-[NBO] (Na+), [3]B-[NBO] (Na+), [4]B (mostly Ca2+), [4]Al (nearly equally split Na+ and Ca2+), and [6]Zr (mostly Ca2+). The network former-BO-network former linkages preferences were also tabulated; Si-O-Al and Al-O-Al were preferred at the expense of lower Si-O-[3]B and [3]B-O-[3]B linkages. These results provide insights on the structural origins of property changes such as glass transition temperature caused by the substitutions, providing a basis for future improvements of theoretical and computer simulation models.

Lu, Xiaonan↗

Effects of Al:Si and (Al + Na):Si ratios on the properties of the international simple glass, part I: Physical properties

Understanding composition-structure-property relationships of high-alumina nuclear waste glasses are important for vitrification of nuclear waste at the Hanford Site. Two series of glasses were designed, one with varying Al:Si ratios and the other with (Al+Na):Si ratios based on the International Simple Glass (ISG, a simplified nuclear waste model glass), with Al2O3 ranging from 0 to 23 mol % (0 to 32 wt. %). The glasses were synthesized and characterized using electron probe microanalysis, X-ray photoelectron spectroscopy, small angle X-ray scattering, high temperature oxide melt solution calorimetry, and infrared spectroscopy. Glasses were crystal free, and the lowest Na2O and Al2O3 glass formed an immiscible glass phase. Evolution of various properties - glass transition temperature, percentage of 4-coordinated B, enthalpy of glass formation - and infrared spectroscopy results indicate that structural effects differ based on the glass series.

Nuclear Waste Glass↗

Acceleration of Glass Alteration Rates Induced by Zeolite Seeds at Controlled pH

As the glass-water reaction proceeds, certain glass compositions undergo a delayed acceleration in the alteration rate – a phenomenon that is commonly referred to as Stage III behavior – which generally coincides with zeolite formation. However, studying Stage III in the laboratory is difficult because the time scale required to observe Stage III behavior can vary from months to several years, and the solution conditions that initiate this acceleration remain poorly understood. Consequently, the development of a corrosion test method capable of quantifying Stage III rates in a timely manner would be of great benefit to both the scientific community and policy makers concerned with nuclear waste disposal. In this work, we induced and measured the acceleration in the corrosion rate of the AFCI glass by seeding static corrosion tests with zeolite Na-P2 at fixed pH90°C values ranging from 9.5 to 11.5. The induced Stage III rates increased linearly with increasing pH and were measured to be between the forward and residual rates of AFCI. Tests designed to compare induced Stage III rates obtained for different seeding times showed that the induced Stage III rates were faster in the absence of an alteration layer. In summary, the use of the seeded test method allows for a conservative quantification of Stage III rates in a relatively short, one-month time period.

Neeway, James J.↗