Ion-conductive organic networks for battery applications

An anode includes: (1) a current collector; and (2) an interfacial layer disposed over the current collector. The interfacial layer includes an ion-conductive organic network including anionic coordination units, organic linkers bonded through the anionic coordination units, and counterions dispersed in the ion-conductive organic network.

Bao, Zhenan↗

Resolving Current-Dependent Regimes of Electroplating Mechanisms for Fast Charging Lithium Metal Anodes

Poor fast-charge capabilities limit the usage of rechargeable Li metal anodes. Understanding the connection between charging rate, electroplating mechanism, and Li morphology could enable fast-charging solutions. In this report we develop a combined electroanalytical and nanoscale characterization approach to resolve the current-dependent regimes of Li plating mechanisms and morphology. Measurement of Li + transport through the solid electrolyte interphase (SEI) shows that low currents induce plating at buried Li||SEI interfaces, but high currents initiate SEI-breakdown and plating at fresh Li||electrolyte interfaces. The latter pathway can induce uniform growth of {110}-faceted Li at extremely high currents, suggesting ion-transport limitations alone are insufficient to predict Li morphology. At battery relevant fast-charging rates, SEI-breakdown above a critical current density produces detrimental morphology and poor cyclability. Thus, prevention of both SEI-breakdown and slow ion-transport in the electrolyte is essential. This mechanistic insight can inform further electrolyte engineering and customization of fast-charging protocols for Li metal batteries.

25 ENERGY STORAGE↗

Supercooled liquid sulfur maintained in three-dimensional current collector for high-performance Li-S batteries

In lithium-sulfur (Li-S) chemistry, the electrically/ionically insulating nature of sulfur and Li 2 S leads to sluggish electron/ion transfer kinetics for sulfur species conversion. Sulfur and Li 2 S are recognized as solid at room temperature, and solid-liquid phase transitions are the limiting steps in Li-S batteries. Here, we visualize the distinct sulfur growth behaviors on Al, carbon, Ni current collectors and demonstrate that (i) liquid sulfur generated on Ni provides higher reversible capacity, faster kinetics, and better cycling life compared to solid sulfur; and (ii) Ni facilitates the phase transition (e.g., Li 2 S decomposition). Accordingly, light-weight, 3D Ni-based current collector is designed to control the deposition and catalytic conversion of sulfur species toward high-performance Li-S batteries. This work provides insights on the critical role of the current collector in determining the physical state of sulfur and elucidates the correlation between sulfur state and battery performance, which will advance electrode designs in high-energy Li-S batteries.

25 ENERGY STORAGE↗

Tortuosity Effects in Lithium-Metal Host Anodes

Lithium (Li) metal is the ultimate anode material for Li batteries because of its highest capacity among all candidates. Recent research has focused on stable interphase and host materials to address its low stability and reversibility. Here, we discover that tortuosity is a critical parameter affecting the morphology and electrochemical performances of hosted Li anodes. In three types of hosts—vertically aligned, horizontally aligned, and random reduced graphene oxide (rGO) electrodes with tortuosities of 1.25, 4.46, and 1.76, respectively—we show that high electrode tortuosity causes locally higher current density on the top surface of electrodes, resulting in thick Li deposition on the surface and degraded cycling performance. Low electrode tortuosity in the vertically aligned rGO host enables homogeneous Li transport and uniform Li deposition across the host, realizing greatly improved cycling stability. Furthermore, using this principle of low tortuosity, the designed electrode shows through-electrode uniform morphology with anodic Coulombic efficiency of ~99.1% under high current and capacity cycling conditions.

25 ENERGY STORAGE↗

Electrochemical generation of liquid and solid sulfur on two-dimensional layered materials with distinct areal capacities

It has recently been shown that sulfur, a solid material in its elementary form S8, can stay in a supercooled state as liquid sulfur in an electrochemical cell. We establish that this newly discovered state could have implications for lithium–sulfur batteries. Here, through in situ studies of electrochemical sulfur generation, we show that liquid (supercooled) and solid elementary sulfur possess very different areal capacities over the same charging period. To control the physical state of sulfur, we studied its growth on two-dimensional layered materials. We found that on the basal plane, only liquid sulfur accumulates; by contrast, at the edge sites, liquid sulfur accumulates if the thickness of the two-dimensional material is small, whereas solid sulfur nucleates if the thickness is large (tens of nanometres). Correlating the sulfur states with their respective areal capacities, as well as controlling the growth of sulfur on two-dimensional materials, could provide insights for the design of future lithium–sulfur batteries.

36 MATERIALS SCIENCE↗

An ultrathin ionomer interphase for high efficiency lithium anode in carbonate based electrolyte

High coulombic efficiency and dendrite suppression in carbonate electrolytes remain challenges to the development of high-energy lithium ion batteries containing lithium metal anodes. Here we demonstrate an ultrathin (≤100 nm) lithium-ion ionomer membrane consisting of lithium-exchanged sulfonated polyether ether ketone embedded with polyhedral oligosilsesquioxane as a coating layer on copper or lithium for achieving efficient and stable lithium plating-stripping cycles in a carbonate-based electrolyte. Operando analyses and theoretical simulation reveal the remarkable ability of the ionomer coating to enable electric field homogenization over a considerably large lithium-plating surface. The membrane coating, serving as an artificial solid-electrolyte interphase filter in minimizing parasitic reactions at the electrolyte-electrode interface, enables dendrite-free lithium plating on copper with outstanding coulombic efficiencies at room and elevated (50 °C) temperatures. The membrane coated copper demonstrates itself as a promising current collector for manufacturing high-quality pre-plated lithium thin-film anode.

25 ENERGY STORAGE↗

Improving cyclability of Li metal batteries at elevated temperatures and its origin revealed by cryo-electron microscopy

Operations of lithium-ion batteries have long been limited to a narrow temperature range close to room temperature. At elevated temperatures, cycling degradation speeds up due to enhanced side reactions, especially when high-reactivity lithium metal is used as the anode. In this work, we demonstrate enhanced performance in lithium metal batteries operated at elevated temperatures. In an ether-based electrolyte at 60 °C, an average Coulombic efficiency of 99.3% is obtained and more than 300 stable cycles are realized, but, at 20 °C, the Coulombic efficiency drops dramatically within 75 cycles, corresponding to an average Coulombic efficiency of 90.2%. Cryo-electron microscopy reveals a drastically different solid electrolyte interface nanostructure emerging at 60 °C, which maintains mechanical stability, inhibits continuous side reactions and guarantees good cycling stability and low electrochemical impedance. Additionally, larger lithium particles grown at the elevated temperature reduce the electrolyte/electrode interfacial area, which decreases the per-cycle lithium loss and enables higher Coulombic efficiencies.

36 MATERIALS SCIENCE↗

Ultrathin, flexible, solid polymer composite electrolyte enabled with aligned nanoporous host for lithium batteries

The urgent need for safer batteries is leading research to all-solid-state lithium-based cells. To achieve energy density comparable to liquid electrolyte-based cells, ultrathin and lightweight solid electrolytes with high ionic conductivity are desired. However, solid electrolytes with comparable thicknesses to commercial polymer electrolyte separators (~10 μm) used in liquid electrolytes remain challenging to make because of the increased risk of short-circuiting the battery. In this work, we report on a polymer–polymer solid-state electrolyte design, demonstrated with an 8.6-μm-thick nanoporous polyimide (PI) film filled with polyethylene oxide/lithium bis(trifluoromethanesulfonyl)imide (PEO/LiTFSI) that can be used as a safe solid polymer electrolyte. The PI film is nonflammable and mechanically strong, preventing batteries from short-circuiting even after more than 1,000 h of cycling, and the vertical channels enhance the ionic conductivity (2.3 × 10 -4 S cm -1 at 30 °C) of the infused polymer electrolyte. Lastly, all-solid-state lithium-ion batteries fabricated with PI/PEO/LiTFSI solid electrolyte show good cycling performance (200 cycles at C/2 rate) at 60 °C and withstand abuse tests such as bending, cutting and nail penetration.

25 ENERGY STORAGE↗

Fast lithium growth and short circuit induced by localized-temperature hotspots in lithium batteries

Fast-charging and high-energy-density batteries pose significant safety concerns due to high rates of heat generation. Understanding how localized high temperatures affect the battery is critical but remains challenging, mainly due to the difficulty of probing battery internal temperature with high spatial resolution. Here we introduce a method to induce and sense localized high temperature inside a lithium battery using micro-Raman spectroscopy. We discover that temperature hotspots can induce significant lithium metal growth as compared to the surrounding lower temperature area due to the locally enhanced surface exchange current density. More importantly, localized high temperature can be one of the factors to cause battery internal shorting, which further elevates the temperature and increases the risk of thermal runaway. This work provides important insights on the effects of heterogeneous temperatures within batteries and aids the development of safer batteries, thermal management schemes, and diagnostic tools.

25 ENERGY STORAGE↗

Uniform High Ionic Conducting Lithium Sulfide Protection Layer for Stable Lithium Metal Anode

Artificial solid-electrolyte interphase (SEI) is one of the key approaches in addressing the low reversibility and dendritic growth problems of lithium metal anode, yet its current effect is still insufficient due to insufficient stability. Here, a new principle of “simultaneous high ionic conductivity and homogeneity” is proposed for stabilizing SEI and lithium metal anodes. Fabricated by a facile, environmentally friendly, and low-cost lithium solid-sulfur vapor reaction at elevated temperature, a designed lithium sulfide protective layer successfully maintains its protection function during cycling, which is confirmed by both simulations and experiments. Stable dendrite-free cycling of lithium metal anode is realized even at a high areal capacity of 5 mAh cm -2 , and prototype Li–Li 4 Ti 5 O 12 cell with limited lithium also achieves 900 stable cycles. These findings give new insight into the ideal SEI composition and structure and provide new design strategies for stable lithium metal batteries.

25 ENERGY STORAGE↗

Surface-engineered mesoporous silicon microparticles as high-Coulombic-efficiency anodes for lithium-ion batteries

High-capacity silicon anodes suffer from rapid capacity decay due to large volume expansion, which causes mechanical fracture, electrical contact loss and unstable solid electrolyte interphase (SEI). Nanostructuring has proved to be effective in addressing these problems over the past decade; however, new issues such as poor initial Coulombic efficiencies due to increased surface area remain unsolved. Here we develop a surface-engineering strategy by depositing a dense silicon skin onto each mesoporous silicon microparticle and further encapsulating it with a conformal graphene cage, which improves both the initial and later-cycle Coulombic efficiencies. The silicon skin lowers the unfavorable electrolyte/electrode contact area and minimizes SEI formation, resulting in an initial Coulombic efficiency over twice as high as that without silicon skin coating. Furthermore, the graphene cage combined with the inner void space of mesoporous silicon allow for silicon expansion, which guarantees structural integrity and SEI stability, resulting in high later-cycle Coulombic efficiencies (99.8–100% for later cycles) and impressive cycling stability.

25 ENERGY STORAGE↗

Amidoxime-Functionalized Macroporous Carbon Self-Refreshed Electrode Materials for Rapid and High-Capacity Removal of Heavy Metal from Water

Heavy metal pollution continues to be one of the most serious environmental problems which has attracted major global concern. Here, a rapid, high-capacity, yet economical strategy for deep cleaning of heavy metals ions in water is reported based on amidoxime-functionalized macroporous carbon electrode materials. The active sites of our material can be self-refreshed during the electrochemical removal process, which is different from traditional methods. The novel filter device in this work can purify contaminated water very rapidly (3000 L h –1 m –2 ), and can decrease heavy metal ion concentrations to below 5 ppb with a very short contact time (only 3 s). The original treatment efficiency of the device can be retained even after 1 week of continuous device operation. An extremely high removal capacity of over 2300 mg g –1 can be achieved with 2–3 orders of magnitude higher efficiency than that of surface adsorption-based commercial filters without any decay. Additionally, the cost of energy consumed in our method is lower than $6.67 × 10 –3 per ton of wastewater. We envision that this approach can be routinely applied for the rapid, efficient, and thorough removal of heavy metals from both point-of-use water and industrial wastewater.

36 MATERIALS SCIENCE↗

Composite lithium electrode with mesoscale skeleton via simple mechanical deformation

Lithium metal–based batteries are attractive energy storage devices because of high energy density. However, uncontrolled dendrite growth and virtually infinite volume change, which cause performance fading and safety concerns, have limited their applications. In this work, we demonstrate that a composite lithium metal electrode with an ion-conducting mesoscale skeleton can improve electrochemical performance by locally reducing the current density. In addition, the potential for short-circuiting is largely alleviated due to side deposition of mossy lithium on the three-dimensional electroactive surface of the composite electrode. Moreover, the electrode volume only slightly changes with the support of a rigid and stable scaffold. Therefore, this mesoscale composite electrode can cycle stably for 200 cycles with low polarization under a high areal current density up to 5 mA/cm 2 . Most attractively, the proposed fabrication process, which only involves simple mechanical deformation, is scalable and cost effective, providing a new strategy for developing high performance and long lifespan lithium anodes.

25 ENERGY STORAGE↗

Wrinkled Graphene Cages as Hosts for High-Capacity Li Metal Anodes Shown by Cryogenic Electron Microscopy

Lithium (Li) metal has long been considered the “holy grail” of battery anode chemistry but is plagued by low efficiency and poor safety due to its high chemical reactivity and large volume fluctuation, respectively. Here we introduce a new host of wrinkled graphene cage (WGC) for Li metal. Different from recently reported amorphous carbon spheres, WGC show highly improved mechanical stability, better Li ion conductivity, and excellent solid electrolyte interphase (SEI) for continuous robust Li metal protection. At low areal capacities, Li metal is preferentially deposited inside the graphene cage. Cryogenic electron microscopy characterization shows that a uniform and stable SEI forms on the WGC surface that can shield the Li metal from direct exposure to electrolyte. With increased areal capacities, Li metal is plated densely and homogeneously into the outer pore spaces between graphene cages with no dendrite growth or volume change. As a result, a high Coulombic efficiency (CE) of ~98.0% was achieved under 0.5 mA/cm 2 and 1–10 mAh/cm 2 in commercial carbonate electrolytes, and a CE of 99.1% was realized with high-concentration electrolytes under 0.5 mA/cm 2 and 3 mAh/cm 2 . Full cells using WGC electrodes with prestored Li paired with Li iron phosphate showed greatly improved cycle lifetime. With 10 mAh/cm 2 Li metal deposition, the WGC/Li composite anode was able to provide a high specific capacity of ~2785 mAh/g. Furthermore, with its roll-to-roll compatible fabrication procedure, WGC serves as a highly promising material for the practical realization of Li metal anodes in next-generation high energy density secondary batteries.

36 MATERIALS SCIENCE↗

Fast galvanic lithium corrosion involving a Kirkendall-type mechanism

Developing a viable metallic lithium anode is a prerequisite for next-generation batteries. However, the low redox potential of lithium metal renders it prone to corrosion, which must be thoroughly understood for it to be used in practical energy-storage devices. Here in this paper, we report a previously overlooked mechanism by which lithium deposits can corrode on a copper surface. Voids are observed in the corroded deposits and a Kirkendall-type mechanism is validated through electrochemical analysis. Although it is a long-held view that lithium corrosion in electrolytes involves direct charge-transfer through the lithium–electrolyte interphase, the corrosion observed here is found to be governed by a galvanic process between lithium and the copper substrate—a pathway largely neglected by previous battery corrosion studies. The observations are further rationalized by detailed analyses of the solid–electrolyte interphase formed on copper and lithium, where the disparities in electrolyte reduction kinetics on the two surfaces can account for the fast galvanic process.