Effects of Hydrogen Bonding and Molecular Chain Flexibility of Substituted n-Alkyldimethylsilanes On Impact Ice Adhesion Shear Strength

The effects of hydrogen bonding and molecular flexibility upon ice adhesion shear strength were investigated using aluminum substrates coated with substituted n-alkyldimethylalkoxysilanes. The location of the chemical group substitution was on the opposing end of the linear n-alkyl chain with respect to silicon. Three hydrogen-bonding characteristics were evaluated: 1) non-hydrogen bonding, 2) donor/acceptor, and 3) acceptor. Varying the length of the n-alkyl chain provided an assessment of molecular chain flexibility. Coated and uncoated aluminum surfaces were characterized by receding water contact angle and surface roughness. Ice adhesion shear strength was determined in the Adverse Environment Rotor Test Stand facility from -16 to -8°C that simulated aircraft in-flight icing conditions within the FAR Part 25/29 Appendix C icing envelope. Surface roughness of the coatings was similar allowing for comparison of the test results. An adhesion reduction factor, based on the ice adhesion shear strength data with respect to uncoated aluminum obtained at the same temperature, was calculated to compare the data. The results revealed complex interactions with impacting supercooled water droplets that were interdependent upon ice accretion temperature, surface energy characteristics of water and ice, hydrogen bonding characteristic of the substituent, and length of the n-alkyl chain. To aid in explaining the results, 1) changes in the surface energy component (i.e., non-polar and polar) values that water undergoes during its’ phase change from liquid to solid that arise from the freezing of impacting supercooled water droplets on the surface depended upon the temperature during accretion were taken into account and 2) the physical properties (i.e., water solubility and melting point) of small compounds analogous to the substituted n-alkyldimethylalkoxysilanes used in this study were compared.

Smith, Joseph G.

Development and Validation of Physics Based Models for Ice Shedding

Calculations for ice accretion and shedding are presented for a model scale rotor in hover. The aerodynamic characteristics of the rotor are first computed using a combined blade element-momentum theory. The effective angles of attack, and the local flow velocity are used within the NASA Glenn solver LEWICE to estimate the collection efficiency. The computed convection efficiency and the surface pressure distribution from a panel method within LEWICE are used to estimate the ice accretion over the rotor blades over an elapsed time interval. Finally, a force balance approach is used to establish shedding events where the centrifugal force over the ice mass exceeds the adhesive forces at the rotor surface and the cohesive forces between adjacent masses of ice. Preliminary comparisons with test data acquired at the Pennsylvania State Icing Research Tunnel are presented. Sensitivity of the ice shedding events to surface roughness, adhesive strength, cohesive strength, and ambient conditions is discussed.

Gupta, Avani

Design and Development of a Laboratory-Scale Ice Adhesion Testing Device

When an aircraft traverses through clouds containing supercooled water droplets, in-flight icing can occur that negatively affects vehicle performance by increasing weight and drag leading to loss of lift. Super-cooled water droplets present in clouds that impact vehicle surfaces can lead to inflight icing any time during the year.1 Most events occur at temperatures ranging from 0 to -20degC. Ice generated on the aircraft can vary between clear/glaze, rime, and mixed (Fig. 1) depending on air temperature (-5 to -20degC), liquid water content (0.3-0.6 g/m3), and droplet size (median volumetric diameter of 15-40 μm). Current strategies to remove ice are based on active technologies such as pneumatic boots, heated surfaces, and deicing agents (i.e., ethylene- and propylene-based glycols). The latter have potential environmental concerns. A passive approach to mitigate accreting ice that is actively being investigated are protective coatings. An ice mitigating coating could potentially be used as a stand-alone material, but more likely in combination with an active approach. In the latter scenario, potential reduction in power consumption by the active approach may be realized. To determine the ice adhesion strength of impact ice that is representative of the aircraft environment is not a trivial matter. Test methods utilizing slowly formed ice (i.e., freezer ice) do not accurately simulate this environment. Likewise, some testing methodologies involve sample relocation from the icing environment to the test chamber that can result in thermal shock to the sample, thus affecting the results. The Adverse Environment Rotor Test Stand (AERTS) located at Pennsylvania State University (PSU) has been demonstrated to simulate impact icing conditions within the icing envelope for the determination of ice adhesion shear strength (IASS) without removal/relocation of the sample.2 Due to the confidence in results obtained from AERTS, this instrument is in high demand and requires a significant amount of lead time and capital investment to obtain IASS results. As a solution for quickly and economically screening coatings in a controlled manner under impact icing conditions, a laboratory-scale ice adhesion test and dead blades were then removed from the rotor/blade assembly to obtain the final mass. The IASS of the live blade was determined from the difference in mass (before and after testing) of the live and dead blades, the ice shed area, and the rpm of the shed event. The same live blade sample was tested in triplicate at all three test temperatures. Surface roughness was determined using a Bruker Dektak XT Stylus Profilometer. Measurements were conducted using a 12.5 μm tip at a vertical range of 65.5 μm with an applied force of 3 mg. Data were collected over a 1.0 mm length at a resolution of 0.056 μm/point. Five single line scans at different locations were collected and processed using a two-point leveling subtraction. The resultant Ra (arithmetic roughness) and Rq (root mean square roughness) average values were calculated.

Smith, Joseph G., Jr.

Mechanism of Supercooled Water Droplet Breakup near the Leading Edge of an Airfoil

This work presents the results of an experimental study on supercooled droplet deformation and breakup near the leading edge of an airfoil. The results are compared to prior room temperature droplet deformation results to explore the effects of droplet supercooling. The experiments were conducted in the Adverse Environment Rotor Test Stand (AERTS) at The Pennsylvania State University. An airfoil model placed at the end of the rotor blades mounted onto the hub in the AERTS chamber was moved at speeds ranging between 50 and 80 m/sec. The temperature of the chamber was set at -20˚C. A monotonic droplet generator was used to produce droplets that fell from above, perpendicular to the path of the airfoil. The supercooled state of the droplets was determined by measurement of the temperature of the drops at various locations below the droplet generator exit. A temperature prediction code was also used to estimate the temperature of the droplets based on vertical velocity and the distance traveled by droplets from the droplet generator to the airfoil stagnation line. High speed imaging was employed to observe the interaction between the droplets and the airfoil. The high speed imaging provided droplet deformation information as the droplet approached the airfoil near the stagnation line. A tracking software program was used to measure the horizontal and vertical displacement of the droplet against time. It was demonstrated that to compare the effects of water supercooling on droplet deformation, the ratio of the slip velocity and the initial droplet velocity must be equal. A case with equal slip velocity to initial velocity ratios was selected for room temperature and supercooled droplet conditions. The airfoil velocity was 60 m/s and the slip velocity for both sets of data was 40 m/s. In these cases, the deformation of the weakly supercooled and warm droplets did not present different trends. The similar behavior for both environmental conditions indicates that water supercooling has no effect on particle deformation for the limited range of the weak supercooling of the droplets tested and the selected impact velocity. The assumption of a constant surface tension value was further supported by the equal trend of the Bond number obtained for supercooled and room temperature droplets.

in-flight icing

Effect of Molecular Flexibility upon Ice Adhesion Shear Strength

Ice formation on aircraft surfaces effects aircraft performance by increasing weight and drag leading to loss of lift. Current active alleviation strategies involve pneumatic boots, heated surfaces, and usage of glycol based de-icing fluids. Mitigation or reduction of in-flight icing by means of a passive approach may enable retention of aircraft capabilities, i.e., no reduction in lift, while reducing the aircraft weight and mechanical complexity. Under a NASA Aeronautics Research Institute Seedling activity, the effect of end group functionality and chain length upon ice adhesion shear strength (IASS) was evaluated with the results indicating that chemical functionality and chain length (i.e. molecular flexibility) affected IASS. Based on experimental and modeling results, diamine monomers incorporating molecular flexibility as either a side chain or in between diamine functionalities were prepared, incorporated into epoxy resins that were subsequently used to fabricate coatings on aluminum substrates, and tested in a simulated icing environment. The IASS was found to be lower when molecular flexibility was incorporated in the polymer chain as opposed to a side chain.

Smith, Joseph G.

The Effect of Surface Chemical Functionality Upon Ice Adhesion

In nature, anti-freeze proteins present in fish utilize specific organic functionalities to disrupt ice crystal formation and propagation. Based on these structures, surfaces with controlled chemical functionality and chain length were evaluated both experimentally and computationally to assess the effect of both parameters in mitigating ice formation. Linear aliphatic dimethylethoxysilanes terminated with methyl or hydroxyl groups were prepared, characterized, and used to coat aluminum. The effect upon icing using a microdroplet freezing apparatus and the Adverse Environment Rotor Test Stand found hydroxyl-terminated materials exhibited a greater propensity for ice formation and adhesion. Molecular dynamics simulations of a silica substrate bearing functionalized species of similar composition were brought into contact with a pre-equilibrated ice crystal. Several parameters including chain mobility were monitored to ascertain the size of a quasi-liquid layer. The studies suggested that chain mobility affected the interface between ice and the surface more than terminal group chemical composition.

Smith, Joseph G., Jr.

Ice Particle Impacts on a Moving Wedge

This work presents the results of an experimental study of ice particle impacts on a moving wedge. The experiment was conducted in the Adverse Environment Rotor Test Stand (AERTS) facility located at Penn State University. The wedge was placed at the tip of a rotating blade. Ice particles shot from a pressure gun intercepted the moving wedge and impacted it at a location along its circular path. The upward velocity of the ice particles varied from 7 to 12 meters per second. Wedge velocities were varied from 0 to 120 meters per second. Wedge angles tested were 0, 30, 45, and 60. High speed imaging combined with backlighting captured the impact allowing observation of the effect of velocity and wedge angle on the impact and the post-impact fragment behavior. It was found that the pressure gun and the rotating wedge could be synchronized to consistently obtain ice particle impacts on the target wedge. It was observed that the number of fragments increase with the normal component of the impact velocity. Particle fragments ejected immediately after impact showed velocities higher than the impact velocity. The results followed the major qualitative features observed by other researchers for hailstone impacts, even though the reduced scale size of the particles used in the present experiment as compared to hailstones was 4:1.

Impacts

Ice Particle Impacts on a Moving Wedge

This work presents the results of an experimental study of ice particle impacts on a moving wedge. The experiment was conducted in the Adverse Environment Rotor Test Stand (AERTS) facility located at Penn State University. The wedge was placed at the tip of a rotating blade. Ice particles shot from a pressure gun intercepted the moving wedge and impacted it at a location along its circular path. The upward velocity of the ice particles varied from 7 to 12 meters per second. Wedge velocities were varied from 0 to 120 meters per second. Wedge angles tested were 0 deg, 30 deg, 45 deg, and 60 deg. High speed imaging combined with backlighting captured the impact allowing observation of the effect of velocity and wedge angle on the impact and the post-impact fragment behavior. It was found that the pressure gun and the rotating wedge could be synchronized to consistently obtain ice particle impacts on the target wedge. It was observed that the number of fragments increase with the normal component of the impact velocity. Particle fragments ejected immediately after impact showed velocities higher than the impact velocity. The results followed the major qualitative features observed by other researchers for hailstone impacts, even though the reduced scale size of the particles used in the present experiment as compared to hailstones was 4:1.

Roughness

Experimental Measurement of Frozen and Partially Melted Water Droplet Impact Dynamics

High-speed video of single frozen water droplets impacting a surface was acquired. The droplets diameter ranged from 0.4 mm to 0.9 mm and impacted at velocities ranging from 140 m/sec to 309 m/sec. The techniques used to freeze the droplets and launch the particles against the surfaces is described in this paper. High-speed video was used to quantify the ice accretion area to the surface for varying impact angles (30 deg, 45 deg, 60 deg), impacting velocities, and break-up angles. An oxygen /acetylene cross-flow flame used to ensure partial melting of the traveling frozen droplets is also discussed. A linear relationship between impact angle and ice accretion is identified for fully frozen particles. The slope of the relationship is affected by impact speed. Perpendicular impacts, i.e. 30 deg, exhibited small differences in ice accretion for varying velocities, while an increase of 60% in velocity from 161 m/sec to 259 m/sec, provided an increase on ice accretion area of 96% at an impact angle of 60 deg. The increase accretion area highlights the importance of impact angle and velocity on the ice accretion process of ice crystals. It was experimentally observed that partial melting was not required for ice accretion at the tested velocities when high impact angles were used (45 and 60 deg). Partially melted droplets doubled the ice accretion areas on the impacting surface when 0.0023 Joules were applied to the particle. The partially melted state of the droplets and a method to quantify the percentage increase in ice accretion area is also described in the paper.

Impact Dynamics