Generating multi-scale Li-ion battery cathode particles with radial grain architectures using stereological generative adversarial networks

Abstract Understanding structure-property relationships of Li-ion battery cathodes is crucial for optimizing rate-performance and cycle-life resilience. However, correlating the morphology of cathode particles, such as in LiNi0.8Mn0.1Co0.1O2 (NMC811), and their inner grain architecture with electrode performance is challenging, particularly, due to the significant length-scale difference between grain and particle sizes. Experimentally, it is not feasible to image such a high number of particles with full granular detail. A second challenge is that sufficiently high-resolution 3D imaging techniques remain expensive and are sparsely available at research institutions. Here, we present a stereological generative adversarial network-based model fitting approach to tackle this, that generates representative 3D information from 2D data, enabling characterization of materials in 3D using cost-effective 2D data. Once calibrated, this multi-scale model can rapidly generate virtual cathode particles that are statistically similar to experimental data, and thus is suitable for virtual characterization and materials testing through numerical simulations. A large dataset of simulated particles with inner grain architecture has been made publicly available.

25 ENERGY STORAGE↗

Chemo-Mechanical Instabilities in Lithium Cobalt Oxide at Higher State-Of-Charge in Li-Ion Batteries

Transition metal oxide cathodes are widely used in commercial Li-ion batteries. However, their practical charge capacity is limited due to severe chemo-mechanical instabilities at higher charge voltage, and state-of-charge condition. Here, in situ stress and strain measurements were synchronized to probe mechanical deformations in the lithium cobalt oxide (LCO) cathode via a multi-beam stress sensor and digital image correlation, respectively. In situ mechanical measurements revealed how Li removal from the electrode structure induces deformations on the LCO composite cathodes during cycling. The structure and morphology of the LCO cathodes were further investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM) studies. Two distinct electrochemical and mechanical behaviors were identified when the LCO was charged up to 4.65 V. The LCO undergoes a compressive stress generation when charged up to 4.2 V and surface fractures on the LCO particles were detected by SEM. LCO cathode experienced significantly large contractions (negative strains) when charged up to 4.65 V, where intergranular crack formation and phase transformation were detected on the LCO particles via SEM and XRD, respectively. Overall, the study bridges complicated structural deformations with in situ analysis of mechanical degradations in LCO cathodes charged at higher voltages. The correlation is vital to understanding instability mechanisms in transition metal oxides at high voltages for alkali metal ion batteries.

higher state-of-charge↗

Direct reuse of graphite and lithium nickel manganese cobalt oxide (NMC) recovered from ultrafast-laser ablation debris in Li-ion battery electrodes

Here we demonstrate that debris collected from the ultrafast-laser ablation of graphite anodes can be directly reused in a lithium-ion battery with little to no negative effects on electrochemical performance. Further, we show that while post-ablation NMC (LiNi 0.33 Mn 0.33 Co 0.33 O) cathode debris will require additional processing before being incorporated into an electrode, its critical materials (nickel, manganese, and cobalt) are not lost during ablation and can be recovered for recycling. Pre- and post-ablation materials are characterized with a suite of diagnostics, including SEM, TEM, X-ray CT, EDS, and XRD, to study changes in material morphology, composition and crystal structure. Graphite exhibited little to no morphological or compositional changes and a slight annealing of its crystal structure. NMC underwent profound morphological and crystallographic changes, but retained its elemental composition. Finally, post-ablation materials were re-manufactured into electrodes and cycled vs lithium metal. Graphite showed equal or better capacity and Coulombic efficiency compared to pre-ablation electrodes, while the post-ablation NMC exhibited severely reduced electrochemical performance. Furthermore, we discuss the outlook for application of this work to advanced manufacturing lines that produce next-generation, laser-patterned electrodes.

25 ENERGY STORAGE↗

Probing the Formation of Cathode-Electrolyte Interphase on Lithium Iron Phosphate Cathodes via Operando Mechanical Measurements

Interfacial instabilities in electrodes control the performance and lifetime of Li-ion batteries. While the formation of solid-electrolyte interface (SEI) on anodes has received much attention, there is still lack of understanding about the formation of cathode-electrolyte interface (CEI) on the cathodes. To fill this gap, we report on dynamic deformations on lithium iron phosphate, LiFePO 4 cathodes during charge / discharge by utilizing in-operando digital image correlation, impedance spectroscopy and Cryo X-ray photoelectron spectroscopy. LiFePO4 cathodes were cycled in either LiPF 6 , LiClO 4 or LiTFSI- containing organic liquid electrolytes. Beyond the first cycle, Li-ion intercalation results in a nearly linear correlation between electrochemical strains and the state of (dis)-charge, regardless of the electrolyte chemistry. However, during the first charge in LiPF 6 - containing electrolyte, there is a distinct irreversible positive strain evolution at the onset of anodic current rise as well as current decay at around 4.0V. Impedance studies show the increase in surface resistance in the same potential window, suggesting the formation of CEI layers on the cathode. The chemistry of the CEI layer was characterized by X-ray photoelectron spectroscopy. LiF is detected in CEI layer starting as early as 3.4 V and Li $x$ PO $y$ F $z$ appeared at voltages higher than 4.0 V during the first charge. In conclusion, our approach offers new insights into the formation mechanism of CEI layers on the cathode electrodes, which is crucial for the development of robust cathode and electrolyte chemistries for higher performance batteries.

25 ENERGY STORAGE↗

The Role of Transition Metals on Chemo-Mechanical Instabilities in Prussian Blue Analogues For K-Ion Batteries: The Case Study on KNHCF Versus KMHCF

Prussian blue analogues (PBAs) cathodes can host diverse monovalent and multivalent metal ions due to their tunable structure. However, their electrochemical performance suffers from poor cycle life associated with chemo-mechanical instabilities. This study investigates the driving forces behind chemo-mechanical instabilities in Ni- and Mn-based PBAs cathodes for K-ion batteries by combining electrochemical analysis, digital image correlation, and spectroscopy techniques. Capacity retention in Ni-based PBA is 96% whereas it is 91.5% for Mn-based PBA after 100 cycles at C/5 rate. During charge, the potassium nickel hexacyanoferrate (KNHCF) electrode experiences a positive strain generation whereas the potassium manganese hexacyanoferrate (KMHCF) electrode undergoes initially positive strain generation followed by a reduction in strains at a higher state of charge. Overall, both cathodes undergo similar reversible electrochemical strains in each charge–discharge cycle. There is ~0.80% irreversible strain generation in both cathodes after 5 cycles. XPS studies indicated richer organic layer compounds in the cathode-electrolyte interface (CEI) layer formed on KMHCF cathodes compared to the KNHCF ones. Faster capacity fades in Mn-based PBA, compared to Ni-based ones, is attributed to the formation of richer organic compounds in CEI layers, rather than mechanical deformations. In conclusion, understanding the driving forces behind instabilities provides a guideline to develop material-based strategies for better electrochemical performance.

25 ENERGY STORAGE↗

Mechanistic Elucidation of Electronically Conductive PEDOT:PSS Tailored Binder for a Potassium‐Ion Battery Graphite Anode: Electrochemical, Mechanical, and Thermal Safety Aspects

Potassium-ion batteries (KIBs) are considered more appropriate for grid-scale storage than lithium-ion batteries (LIBs) due to similar operating chemistry, abundant precursors, and compatibility with low-cost graphite anodes. However, a larger ion reduces rate capabilities and exacerbates capacity fading from volumetric expansion. In this report, conductive polymer, poly(3,4-ethylenedioxythiophene) polystyrene sulfonate (PEDOT:PSS), is substituted for standard insulating polyvinylidene fluoride (PVDF). Half-cells using carbon black (CB) in continuously conductive PEDOT:PSS/CB binder outperforms PVDF/CB by mitigating electrically isolated “dead” graphite, improving 100 cycle capacity retention at C/10 from 63 to 80%. Enhanced electrical contact with PEDOT:PSS/CB also reduces ion impedance and improves rate capabilities. Without CB however, PEDOT:PSS binder performs poorly in electrochemical studies despite promising ex situ electronic conductivity. This discrepancy is mechanistically elucidated through identification of redox activity between PEDOT:PSS and K + which results in high impedances in the anode operating voltage window. Additionally, the impact of conducting binder on mechanical properties and thermal safety of the anode is investigated. Brittleness and poor wettability of PEDOT:PSS are identified as issues, but greater stability against reactive KC 8 reduces overall heat generation. Binder substitution offers a promising means of mitigating issues with current KIB anodes regardless of active material, and the work herein addresses issues towards further improvement.

electrochemical impedance spectroscopy↗

Elucidating Cycling Rate-Dependent Electrochemical Strains in Sodium Iron Phosphate Cathodes for Na-ion Batteries

Battery electrodes materials undergo significant mechanical instabilities which affects their longevity and exert rate-limitations during the cycling process. In this study, we investigate the rate-dependent mechanical response of sodium iron phosphate (NaFePO4, NFP) cathodes during Na intercalation via galvanostatic cycling at different rates by employing digital image correlation, electrochemical methods, and mathematical model. The mechanical behaviour of the electrode shows strong dependance on the applied scan rate. At slower rates, electrode shows asymmetrical strain generation between anodic and cathodic cycles, which is attributed to the formation of cathode-electrolyte interface layers. The electrode undergoes smaller strain generation when cycled at slower rates when the same amount of Na ions is removed or inserted into the electrode. A mathematical model was developed to predict strain evolution in the composite electrode as well as the concentration profile of the Na ions in the electrode particles. Rate-dependent and time dependent factors on the strain generation in the electrode are attributed to the capacity-dependent intercalation strains, rate-dependent mismatch strains, and time-dependent irreversible strains. The combination of in situ strain measurements with the analytical model provided new insight into the electrochemically induced mechanical deformations in Na-ion cathode electrodes.

Ozdogru, Bertan↗

In Situ Probing Potassium-ion Intercalation-induced Amorphization in Crystalline Iron Phosphate Cathode Materials

Na-ion and K-ion batteries are promising alternatives for large-scale energy storage applications due to their abundance and low cost. Intercalation of these large ions could cause irreversible structural deformation and partial to complete amorphization in the crystalline electrodes. The designing of new amorphous electrodes is another route to develop electrodes to store these ions reversibly. Lack of understanding of dynamic changes in the amorphous nanostructures during battery operation is the bottleneck for further developments. Here, we report the utilization of in situ digital image correlation and in-operando X-ray diffraction (XRD) techniques to probe dynamic changes in the amorphous phase of iron phosphate during potassium intercalation. In-operando XRD demonstrates amorphization in the electrode’s nanostructure during the first charge/discharge cycle. Additionally, the ex-situ high-resolution transmission electron microscopy further confirms the amorphization after potassium insertion. In situ strain analysis detects the reversible deformation associated with redox reactions in the amorphous phases. Our approach offers new insights on the mechanisms of ion intercalation in the amorphous nanostructures which are highly potent for development of next-generation batteries.