Advanced Manufacturing and Materials Technologies for Gasification
Presented by LRST at the 2020 Gasification Project Review Meeting, 9/2
Engineering topics
Publications and source records attributed to Nakano, Anna.
Presented by LRST at the 2020 Gasification Project Review Meeting, 9/2
Coal ash slag as a waste by-product, is generated from commercial processes that include gasification facilities, power plants, and steelmaking industries. Some is recycled into construction materials, insulation fibers, and used as a soil neutralizer, but the majority is still discarded. Coal ash slag exhibit trace amounts of critical materials including rare earth elements (REEs). An economically viable extraction of REEs from the coal ash would lower the production costs, addressing the availability and environmental concerns. In nature, most REEs exist as phosphate such as monazite but its synthetic evolution in coal ash slag has never been reported. In industrial processes, P may originate from coal, additives, and/or refractory liners. REEs may be extracted by first concentrating REEs into phosphates, sulphide, or fluorides [1], or carbonates [2]. In this work, P-enriched coal ash slag bearing REEs was first melted above 1600 °C, then crystallization behaviors in the melt during controlled cooling was studied. REE phosphate coprecipitated with mullite and hematite with mullite being the first crystal to form on cooling. The REEs were rejected from the molten slag, mullite, and hematite, and tended to segregate only to the phosphate phase with REE concentration as high as 58 wt.% in the structure.
Presented by NETL at TMS 2020, 02/20
Presented by NETL at UNITECR 2019, 10/19
The disclosure relates to a method for concentrating rare earth elements (REEs) from a coal byproduct. The method includes mixing the coal byproduct input with aluminum phosphate, sulfur and/or other compounds used as an additive; heating the coal byproduct input in air for a period of 3 minutes or longer at a temperature above a liquid starting temperature of the coal byproduct input, forming a molten coal byproduct; cooling the molten coal byproduct at a rate slower than critical glass transition cooling rate of the melt, forming REE phosphate product; heating the coal byproduct input above the liquid starting temperature of the coal byproduct after REE phosphate product is formed; and cooling the coal byproduct input at a rate faster than the critical glass transition cooling rate of the melt, minimizing forming unwanted solids.
A single-heating stage method for reclaiming or recovering metals like nickel and vanadium from a petroleum waste byproduct has three steps: melting the petroleum waste byproduct in a reducing atmosphere, generating agglomerated metal in the melted byproduct, and lifting the agglomerated metal to an exposed surface of the melted byproduct. The metal precipitates out of the molten byproduct, agglomerates into a separate portion, and rises to an exposed surface of the melted petroleum waste byproduct even though the metal may have greater density than the molten petroleum waste byproduct. The original petroleum waste byproduct stratifies into a byproduct remnant and the agglomerated metal disk. The agglomerated metal disk is separable from the byproduct remnant and may be additionally separated into constituent metals in those embodiments with multiple metals in the disk.
Embodiments relate to methods, systems And apparatus tor generating lithium from brine. The brine is heated in a first vessel to greater than 260° C. and CO2 gas is injected mixing with the brine such that the CO2/P is greater than 18 g/atm. The brine is held at greater than 18 g/atm for longer than 20 minutes so that any impurities precipitate as solids leaving only lithium ions and chlorine ions. The brine is moved to a second vessel screening out solid precipitates leaving a brine containing only chlorine and lithium. CO2 gas is injected and mixed with the brine at 260° C. so that the CO2/P is greater than 200 g/atm. The brine is held at greater than 200 g/atm for longer than 20 minutes suppressing the chlorine as dissolved ions while lithium precipitates out as lithium carbonate. The lithium carbonate precipitate is removed from the brine solution.
Presented by NETL at UNITECR 2019, 10/19
Presented by NETL at UNITECR 2019, 10/19
Presented by NETL at The 44th International Technical Conference on Clean Energy, 06/19
Presented by NETL at The 44th International Technical Conference, 06/19
Presented by NETL at UNITECR 2019, 10/19
Presented by NETL at Materials Science and Technology, 09/19
Presented by NETL at TMS 2019 Conference, 03/19
High temperature corrosion of a Pt-30 wt.% Rh alloy in a phosphorizing gas was isothermally investigated at 1285 K using a gas switching technique. Diffusion of P into the alloy created an outer layer of Pt-rich liquid and blocky (Pt, Rh) 2 P precipitates along with an inner layer of fcc and (Pt, Rh) 2 P plates in a cellular microstructure. Concentration profiles measured by SEM-WDS and EPMA across the layers at room temperature showed that there were three fcc phases: first was a 12 at.% Rh phase in the outer layer; second was a 37 at.% Rh phase in the cellular microstructure; and third was the initial 43 at.% Rh alloy. Also, the EPMA data registered approximately 0.1 at.% P in fcc of these layers. Based on the surrounding binary phase diagrams and the experimental data obtained in this study, a partial Pt-Rh-P phase diagram was constructed. A diffusion path for the corrosion microstructure was drawn on the partial phase diagram to help develop a step by step model for how the microstructure evolved. In conclusion, growth kinetics of the inner layer were used to calculate a P diffusivity of about 10 –12 m 2 /s in the Pt-Rh alloy at 1285 K, suggesting rapid diffusion by either an interstitial or interstitialcy mechanism.
Presented by NETL at the Minerals, Metals, and Materials Society 148th Annual Meeting and Exhibition, 3/19