Engineering Papers⌕ Search

Engineering topics

Moore, T. J.

Publications and source records attributed to Moore, T. J..

48 records · Page 3

State-of-technology for joining TD-NiCr sheet

At the current state-of-technology there are many joining processes that can be used to make sound welds in TD-NiCr sheet. Some of these that are described in this report are electron beam welding, gas-tungsten arc welding, diffusion welding, resistance spot welding, resistance seam welding, and brazing. The strengths of the welds made by the various processes show considerable variation, especially at elevated temperatures. Most of the fusion welding processes tend to give weak welds at elevated temperatures (with the exception of fusion-type resistance spotwelds). However, solid-state welds have been made with parent metal properties. The process used for a specific application will be dictated by the specific joint requirements. In highly stressed joints at elevated temperatures, one of the solid-state processes, such as DFW, RSW (solid-state or fusion), and RSEW, offer the most promise.

Holko, K. H.↗

Practical method of diffusion-welding steel plate in air

Method is ideal for critical service requirements where parent metal properties are equaled in notch toughness, stress rupture and other characteristics. Welding technique variations may be used on a variety of materials, such as carbon steels, alloy steels, stainless steels, ceramics, and reactive and refractory materials.

Holko, K. H.↗

Exploratory study of friction welds in Udimet 700 and TD-Nickel bar

Friction welded butt joints were made in both Udimet 700 and TD-Nickel bar. Also, dissimilar metal friction welds were made between these materials. Friction welding of Udimet 700 shows great promise because the welds were found to be as strong as the parent metal in stress rupture and tensile tests at 760 and 980 C. The weld line was not detectable metallographically in the heat treated condition. Friction welding for TD-Nickel, however, holds little if any promise. TD-Nickel friction weldments could support only 9 percent as much stress as the base metal for a 10-hour stress-rupture life at 1090 C. Dissimilar Udimet 700/TD-Nickel friction welds could sustain only 15 percent as much stress as the TD-Nickel parent metal for a 10-hour rupture life at 930 C.

Moore, T. J.↗

Fabrication of hollow ball bearings by diffusion welding

Two steel hemispheres are diffusion welded in an atmosphere of 0.00002 torr at a temperature of 2130 degrees F for 4 hours with a pressure of 4 psi holding the hemispheres together. Weld is accomplished with only microdeformation.

Moore, T. J.↗