Liquid metal walls

Here, the plasma performance of fusion devices depends strongly on the chosen wall materials. Solid plasma-facing components (PFCs) are predominantly used in present devices, and are the most investigated candidates for fusion designs. High-Z materials such as tungsten (W) are the leading solid PFC material candidates. To date, a material choice that scales to steady-state reactor conditions has not been identified. Moreover, if plasma transient events such as edge-localized modes and disruptions cannot be altogether avoided or sufficiently mitigated, the projected peak heat and particle loads far exceed the power exhaust capabilities of solids. Liquid metal (LM) PFCs represent an intrinsic self-healing boundary that are both resilient to surface damage from transients, and that could handle high steady-state heat and particle fluxes. Flowing LM PFCs can be designed to remove “slag,” the buildup of material erosion due to plasma-material interactions, including charge exchange sputtering in the main chamber. Further, LM offer the prospect to manage hydrogenic species otherwise retained in the PFCs, which is important from a safety and inventory standpoint. The two most promising LMs are lithium (Li) and tin (Sn), although Sn–Li eutectics may be considered. While Sn offers a higher temperature window with low vapor pressure and low hydrogen retention, Li offers the prospect of enhanced energy confinement and higher acceptable core contamination limits, and this section focuses on Li PFCs. An LM PFC development research program developed LM PFC concepts for a nuclear fusion device via engineering design calculations, single-effect experiments, and staged prototypical experiments. A self-consistent design window was identified with liquid Li flow speeds ~5–10 m/s; plasma contamination was negligible for predicted Li evolution rates. While these preconceptual designs hold promise, there is substantial R&D needed to advance the technical readiness levels of LM PFCs for application to fusion power plants.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Initial design concepts for solid boron injection in ITER

As part of ITER’s consideration to change its first wall material from beryllium to tungsten, the ITER Organization has proposed studying the feasibility of real-time solid boron injection (SBI) into the plasma to coat the walls and divertor to supplement glow discharge boronization (GDB). Boron deposits getter oxygen and reduce sputtering of tungsten from plasma facing components (PFCs). Particularly in areas with significant plasma wall interactions, boron coatings are expected to be short-lived under high performance plasma conditions. The proposed SBI system aims to maintain boron layers in these areas to avoid excessive radiation from tungsten in the plasma as a risk mitigation to ensure ITER will be able to reach and sustain Q = 10 conditions. The system will be used sparingly, as redeposition of boron can lead to significant tritium retention, which must be minimized in ITER to comply with nuclear safety concerns. SBI is proposed to limit and precisely control the amount of boron injected in real-time during plasma operation. Here, some of the design requirements and initial concepts for an SBI system in ITER are presented based on previous results carried out with SBI systems on a number of tokamaks and stellarators around the world. Previous results using SBI systems installed by PPPL have injected boron particles from 5 µm–2 mm diameter at calibrated rates of 2–200 mg/s in real-time during plasma operation on AUG, DIII-D, EAST, KSTAR, LHD, TFTR, WEST, and W7-X, leading to improved wall conditions with reduced plasma impurity concentrations and radiated power and improved plasma performance. The boron is ionized in the plasma edge and then deposited on plasma-wetted surfaces. On AUG, EAST and WEST reduced tungsten sputtering sources were observed following several discharges with SBI. Extrapolation of these SBI results are presented to estimate the amount of boron needed for wall conditioning in ITER. Real-time SBI control requirements and plasma operation scenarios for ITER are also described.

36 MATERIALS SCIENCE↗

Divertor heat load estimates on NSTX and DIII-D using new and open-source 2D inversion analysis code

A thermography inversion algorithm has been developed in the open-source Python-based computer code, HYPERION, to calculate the heat flux incident on plasma-facing components (PFCs) in axisymmetric tokamaks. The chosen mesh size at the surface significantly affects the calculated transient heat flux results. The calculated transient heat flux will exceed the real value when the mesh size tends to zero but will underestimate the real value when the mesh size is large. A criterion for determining the appropriate mesh size for the transient heat flux calculation will be discussed. The numerical scheme for HYPERION uses a 2D fully implicit finite-difference approach, allowing temperature-dependent thermal properties of PFC materials. The inversion algorithm is benchmarked against established heat flux calculation codes, TACO and THEODOR, based on thermography data from NSTX and DIII-D respectively. The primary benefits of HYPERION compared to TACO and THEODOR are that it is open-source and it allows for the optimization of mesh thickness along the substrate. The algorithm also accounts for the thermal properties of thin surface layers that characteristically form on PFCs due to plasma-material interactions. The agreement between HYPERION and THEODOR is excellent, as the percent difference between the codes is ~5% on average in the case of the DIII-D data for moderate to high heat flux. Verification tests with TACO show slightly higher average percent differences of 8% and 12%. In using HYPERION to study filaments in heat flux, the initial results indicate that small ELMs filaments significantly broaden the divertor heat flux, and decrease divertor peak flux. Compared to the inter-ELM, the small ELM filaments decrease the divertor peak surface temperature. With intermittent divertor filaments, the divertor heat flux width is comparable with that found in L-mode.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Optimization of lithium vapor box divertor evaporator location on NSTX-U using SOLPS-ITER

Commercial fusion reactors will be faced with extremely high divertor target heat fluxes that will require mitigation. Simulations of detachment in an NSTX-U scenario projected to have 92 MW/m 2 unmitigated peak target heat flux are presented, which reaches sub-10 MW/m 2 target heat flux using a highly dissipating lithium vapor box divertor design. The lithium vapor box is a detached divertor design which employs lithium vapor evaporation and condensation to contain lithium below the X-point. Previous SOLPS modeling has indicated a lithium vapor box can reduce the heat flux down to 10 MW/m 2 via simultaneous evaporation from the Private Flux Region (PFR) and the Common Flux Region (CFR) sides of the vapor box. It is found here that PFR evaporation has improved access to the separatrix leading to significantly more efficient power dissipation than CFR evaporation. Simulations of target evaporation with an evaporation distribution that is self-consistent with the temperature of a Capillary Porous System with Fast flowing liquid lithium (CPSF) could reach n Li / n e ~ 0.025-0.030 at the Last Closed Flux Surface (LCFS) depending on the liquid metal flow speeds and lithium sputtering yield, while PFR-side evaporation can reach acceptable heat fluxes with n Li / n e ~ 0.038 at the LCFS. However, PFR evaporator performance can be improved if the target is allowed to be hot enough such that it reflects lithium, reaching n Li / n e ~ 0.028 and reducing required lithium evaporation. Ultimately PFR evaporation and target evaporation are found to have similar ability to produce acceptable heat flux solutions with minimal upstream concentration.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Deuterium recycling and wall retention characteristics during boron powder injection in EAST

Boron (B), as a low-Z material, is widely employed for wall conditioning to enhance plasma performance in fusion devices. In the Experimental Advanced Superconducting Tokamak, a series of experiments involving real-time B powder injection has been conducted to investigate fuel particle behavior. It was observed that fuel particle recycling decreased with an increase in the amount of B powder injected, resulting in an increase in short-term fuel retention. The fuel recycling decreased by up to 80%, as indicated by divertor neutral pressure and D α line emission. Furthermore, each B atom exhibited a trapping capacity of 0.3 D particles during B powder injection at a typical flow rate. The real-time B injection had no wall hysteresis effect on D retention, implying that cumulative B injection and deposited film did not affect long-term D retention. The possible mechanism for D retention is the formation of B-C-O-D compounds and co-deposition between B and D particles during discharges. This investigation would be valuable for evaluating T retention when B is used as wall conditioning material in future fusion reactor devices.

36 MATERIALS SCIENCE↗

Long-pulse high-performance H-mode plasmas achieved on EAST

A record duration of a 310 s H-mode plasma (H 98y2 ~ 1.3, n e /n GW ~ 0.7, f BS > 50%) has been recently achieved on experimental advanced superconducting tokamak (EAST) with metal walls, exploiting the device's improved long-pulse capabilities. The experiment demonstrates good control of tungsten concentration, core/edge MHD stability, and particle and heat exhaust with an ITER-like tungsten divertor and zero injected torque, establishing a milestone on the path to steady-state long-pulse high-performance scenarios in support of ITER and CFETR. Important synergistic effects are leveraged toward this result, which relies purely on radio frequency (RF) powers for heating and current drive (H&CD). On-axis electron cyclotron heating enhances the H&CD efficiency from lower hybrid wave injection, increasing confinement quality and enabling fully non-inductive operation at high density (n e /n GW ~ 70%) and high poloidal beta (β P ~ 2.5). A small-amplitude grassy edge localized mode regime facilitates the RF power coupling to the H-mode edge and reduces divertor sputtering/erosion. The high energy confinement quality (H 98y2 ~ 1.3) is achieved with the experimental and simulated results pointing to the strong effect of Shafranov shift on turbulence. Transport analysis suggests that trapped electron modes dominate in the core region during the record discharge. The detailed physics processes (RF synergy, core-edge integration, confinement properties, etc.) of the steady-state operation will be illustrated in the content. In the future, EAST will aim at accessing more relevant dimensionless parameters to develop long-pulse high-performance plasma toward ITER and CFETR steady-state advanced operation.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Overview of Liquid-Metal PFC R&D at the University of Illinois Urbana-Champaign

The design and implementation of future flowing liquid-lithium plasma-facing components (LLPFCs) will be dependent on several factors. Of course, one of the most important is the need to be able to deal with high heat fluxes incident on the surface of the LLPFCs, but there are also several other important liquid-metal behaviors that have been identified for their critical impact on the feasibility of a LLPFC. One of these is the ability to constantly wet 100% of the plasma-facing component area and the best way to achieve that. Another key point is knowing and understanding the erosion and corrosion of the surfaces subject to a flowing liquid-lithium system and the ability for hydrogen and helium uptake by the system. The Center for Plasma Material Interactions (CPMI) has been tasked with looking at these various issues. The Mock-up Entry module for EAST device was used to investigate wetting and erosion effects and to design a suitable distribution and collection system with a liquid-lithium loop. The vapor shielding effects of lithium on the surface were also modeled and studied. A model coupling CRANE, an open-source global reaction network solver, and Zapdos, a plasma transport solver, is being developed to better understand the dynamics of the vapor cloud. Experiments on the Magnum-PSI at the Dutch Institute for Fundamental Energy Research have been carried out to study the vapor shielding effect and obtain experimental benchmarks to verify the model. Also, initial experiments using the Hybrid Illinois Device for Research and Applications have been performed to understand the pumping effects of lithium on helium. Experiments with a drop of liquid lithium (~100 mg) into a helium plasma have shown the ability of lithium to take out the cold recycling helium gas as well as hydrogen and oxygen impurity gases. The improvement in plasma performance was significant, and further understanding of this effect will have impacts on how future LLPFCs will be designed. Further investigation into the exact mechanism for helium pumping by lithium needs to be performed in the future. Finally, this paper presents a summary of the results obtained at the CPMI.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Active wall conditioning through boron powder injection compatible $\mathrm{ELM}$ control in $\mathrm{EAST}$

Real-time wall conditioning and edge-localized mode (ELM) suppression through real-time boron powder injection into high-confinement mode discharges of the Experimental Advanced Superconducting Tokamak (EAST) have been investigated. The boron powder injection effectively conditioned the plasma-facing components, as shown by the reductions in low-Z and high-Z impurities and the global recycling level in the whole inner vessel, and suppressed the strong magnetohydrodynamic (MHD) activity in the plasma core. The improved wall conditions also resulted in an earlier transition from L- to H-mode. Boron powder injection also effectively suppressed ELM in the lower single null configuration with BT in the favorable direction while leaving the plasma density and stored energy largely unaffected.

36 MATERIALS SCIENCE↗

Mitigation of plasma–wall interactions with low-Z powders in DIII-D high confinement plasmas

Experiments with low-Z powder injection in DIII-D high confinement discharges demonstrated increased divertor dissipation and detachment while maintaining good core energy confinement. Lithium (Li), boron (B), and boron nitride (BN) powders were injected in H-mode plasmas (I p = 1 MA, B t = 2 T, P NB = 6 MW, < n e > = 3.6–5.0 · 10 19 m –3 ) into the upper small-angle slot divertor for 2 s intervals at constant rates of 3–204 mg s –1 . The multi-species BN powders at a rate of 54 mg s –1 showed the most substantial increase in divertor neutral compression by more than an order of magnitude and lasting detachment with minor degradation of the stored magnetic energy W mhd by 5%. Rates of 204 mg s –1 of boron nitride powder further reduce edge localized mode-fluxes on the divertor but also cause a drop in confinement performance by 24% due to the onset of an n = 2 tearing mode. The application of powders also showed a substantial improvement of wall conditions manifesting in reduced wall fueling source and intrinsic carbon and oxygen content in response to the cumulative injection of non-recycling materials. Furthermore, the results suggest that low-Z powder injection, including mixed element compounds, is a promising new core-edge compatible technique that simultaneously enables divertor detachment and improves wall conditions during high confinement operation.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K

Here, in this study, the corrosion behaviours of molybdenum (Mo) and a Mo-based alloy (TZM) were investigated using a static immersion corrosion technique. Weight loss, surface microstructure, and corrosion depth of Mo and the TZM alloy were correlated with elements. The compatibility of Mo and the TZM alloy in static liquid Li was suitable. Mo demonstrated uniform corrosion with a homogenous dissolution of free C and Mo, and TZM alloy exhibited a nonuniform corrosion behaviour with a preferential grain boundary attack caused by the selective dissolution of free C, Ti, and Zr. When the surface oxidation layer of the samples was consumed, free C from Mo and TZM diffused into molten Li to form Li 2 C 2 and then was captured by Zr, Ti, and Mo to form thermodynamically stable carbides, which resulted in the enrichment of the C layer near the sample surfaces. In addition, Ti and Zr acted as N-trappers in liquid Li; the formation of Zr and Ti nitrides resulted in the enrichment of N, Ti, and Zr elements on the surface and led to TZM corrosion increase. Thus, Zr and Ti depletion, pitting, and grain boundary corrosion were problematic for TZM under long-term exposure to liquid Li. Reducing the content of free C and nonmetallic N and increasing the amount of Ti and Zr carbides on the surface of and inside the raw TZM alloy helped improve the corrosion resistance of TZM in liquid Li.

36 MATERIALS SCIENCE↗

Fusion pilot plant performance and the role of a sustained high power density tokamak

Here, recent U.S. fusion development strategy reports all recommend that the U.S. should pursue innovative science and technology to enable construction of a fusion pilot plant (FPP) that produces net electricity from fusion at low capital cost. Compact tokamaks have been proposed as a means of potentially reducing the capital cost of a FPP. However, compact steady-state tokamak FPPs face the challenge of integrating a high fraction of self-driven current with high core confinement, plasma pressure, and high divertor parallel heat flux. This integration is sufficiently challenging that a dedicated sustained-high-power-density (SHPD) tokamak facility is proposed by the U.S. community as the optimal way to close this integration gap. Performance projections for the steady-state tokamak FPP regime are presented and a preliminary SHPD device with substantial flexibility in lower aspect ratio (A = 2–2.5), shaping, and divertor configuration to narrow gaps to an FPP is described.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Impact of edge harmonic oscillations on the divertor heat flux in NSTX

Previously, ELM-free and inter-ELM divertor peak heat flux reduction induced by an edge harmonic oscillation (EHO) was observed in NSTX (K.F. Gan et al., 2017 Nucl. Fusion 57 126053). This paper introduces new analysis of the EHO impact on the divertor heat flux. It was found that enhanced edge turbulence significantly altered the divertor heat flux footprint in NSTX H-modes, relative to ELM-free discharges. When the background edge fluctuation level was low, the EHO significantly increased the heat flux width and decreased the divertor peak heat flux. When the background edge fluctuation level was high, the EHO actually increased the divertor peak heat flux. As a result, it was also found that the heat flux width increased with increasing frequency of the EHO.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Comparison of active impurity control between lithium and boron powder real-time injection in EAST

The lithium and boron powder have been successfully real-time injected into Experimental Advanced Superconducting Tokamak (EAST) high-confinement (H-) mode discharges, showing good wall conditioning effects, especially on the impurities control. Both of lithium and boron powder particles are gravitationally accelerated into the upper edge of a upper single null discharge. The lithium powder real-time injection effectively reduced the tungsten impurity content both in the plasma edge and core. Contrary to the lithium injection, the boron injection mainly reduced the impurities content in the plasma core, while the impurities increased in the edge. Furthermore, this mainly due to that there was an edge harmonic mode stimulated by boron injection, providing sufficient particles transport. Moreover, the impurities control through boron injection has much wider operation windows than lithium powder injection. Furthermore, there was accumulative wall conditioning effects after sequential boron powder injection discharges.

36 MATERIALS SCIENCE↗

Enhancement of edge turbulence concomitant with ELM suppression during boron powder injection in EAST

A reproducible, quasi-stationary edge localized mode (ELM)-suppressed scenario was obtained over a wide range of plasma parameters by continuous injection of boron (B) powder into an upper-single null discharge in the experimental advanced superconducting tokamak [Sun et al., Nucl. Fusion 61, 014002 (2021)]. This powder-induced ELM-absent regime is associated with an edge harmonic mode (EHM) that provides continuous particle exhaust to maintain constant density without confinement degradation and impurity accumulation, the latter of which is often observed in ELM-free regimes. A flow rate threshold of B powder injection, leading to a threshold intensity of the EHM, is necessary for full ELM suppression. The fundamental harmonic of the EHM exhibits a toroidal mode number n = 1. The mode is observable in the entire poloidal cross section with a peak near the upper X-point in an upper-single null configuration. Here, the EHM spans radially across the pedestal and scrape-off layer, peaking inside the separatrix. The EHM appears to be insensitive to q 95 , heating power, plasma toroidal rotation, and pedestal collisionality.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Wall conditioning and ELM mitigation with boron nitride powder injection in KSTAR

Results from KSTAR powder injection experiments, in which tens of milligrams of boron nitride (BN) were dropped into low-power H-mode plasmas, show an improvement in wall conditions in subsequent discharges and, in some cases, a reduction or elimination of edge-localized modes (ELMs). Injected powder is distributed by the plasma flow and is deposited on the wall and, over the course of several discharges, was observed to gradually reduce recycling by 33%, and decrease both the ELM amplitude and frequency. This is the first demonstration of the use of BN for ELM mitigation. In all of these experiments, an Impurity Powder Dropper (IPD) was used to introduce precise, controllable amounts of the materials into ELMy H-mode KSTAR discharges. The plasma duration was between 10 s and 15 s, I p = 500 kA, B T = 1 . 8 T, P NBI = 1 . 6 MW, and P ECH = 0 . 6 MW. Plasma densities were between 2 and 3 × 1 0 19 m -3 . In all cases, the pre-fill and startup gas-fueling was kept constant, suggesting that the decrease in baseline D &#x3B1; emission is in fact due to a reduction in recycling. The results presented herein highlight the viability of powder injection for intra-shot and between-shot wall conditioning