Thermal annealing of laser damage precursors on fused silica surfaces

Previous studies have identified two significant precursors of laser damage on fused silica surfaces at fluences <35 J/cm2: photoactive impurities from polishing and surface fractures. We evaluate isothermal heating as a means of remediating the defect structure associated with surface fractures. Vickers indentations are applied to silica surfaces at loads between 0.5 and 10 N, creating fracture networks. The indentations are characterized before and following thermal annealing under various time and temperature conditions using confocal time-resolved photo-luminescence (CTP) imaging, and R/1 damage testing with 3-ns, 355-nm laser pulses. Improvements in the damage thresholds with reductions in CTP intensity are observed at temperatures well below the glass transition temperature (Tg). The damage threshold on 0.5-N indentations improves from <8 to >35 J/cm2 after annealing at approximately 750°C. Larger fracture networks require longer or higher temperature treatment to achieve similar results. At an annealing temperature >1100°C, optical microscopy indicates morphological changes in some of the fractures surrounding the indentations, although remnants of the original fractures are still observed. In conclusion, we demonstrate the potential of using isothermal annealing to improve the laser damage resistance of silica optics, and provide a means of further understanding the physics of optical damage and mitigation.

36 MATERIALS SCIENCE↗

Fracture Induced Sub-Band Absorption as a Precursor to Optical Damage on Fused Silica Surfaces

The optical damage threshold of indentation induced flaws on fused silica surfaces was explored. Mechanical flaws were characterized by laser damaged testing, SEM, optical, and photoluminescence microscopy. Localized polishing, chemical etching, and the control of indentation morphology were used to isolate the structural features which limit optical damage. A thin defect layer on fracture surfaces, including those smaller than the wavelength of visible light, was found to be the dominant source of laser damage initiation during illumination with 355nm, 3ns laser pulses. Little evidence was found that either displaced or densified material or fluence intensification plays a significant role in optical damage at fluences >35J/cm{sup 2}. Elimination of the defect layer was shown to increase the overall damage performance of fused silica optics.

36 MATERIALS SCIENCE↗

HF-based etching processes for improving laser damage resistance of fused silica optical surfaces

The effect of various HF-based etching processes on the laser damage resistance of scratched fused silica surfaces has been investigated. Conventionally polished and subsequently scratched fused silica plates were treated by submerging in various HF-based etchants (HF or NH{sub 4}F:HF at various ratios and concentrations) under different process conditions (e.g., agitation frequencies, etch times, rinse conditions, and environmental cleanliness). Subsequently, the laser damage resistance (at 351 or 355 nm) of the treated surface was measured. The laser damage resistance was found to be strongly process dependent and scaled inversely with scratch width. The etching process was optimized to remove or prevent the presence of identified precursors (chemical impurities, fracture surfaces, and silica-based redeposit) known to lead to laser damage initiation. The redeposit precursor was reduced (and hence the damage threshold was increased) by: (1) increasing the SiF{sub 6}{sup 2-} solubility through reduction in the NH4F concentration and impurity cation impurities, and (2) improving the mass transport of reaction product (SiF{sub 6}{sup 2-}) (using high frequency ultrasonic agitation and excessive spray rinsing) away from the etched surface. A 2D finite element crack-etching and rinsing mass transport model (incorporating diffusion and advection) was used to predict reaction product concentration. The predictions are consistent with the experimentally observed process trends. The laser damage thresholds also increased with etched amount (up to {approx}30 {micro}m), which has been attributed to: (1) etching through lateral cracks where there is poor acid penetration, and (2) increasing the crack opening resulting in increased mass transport rates. With the optimized etch process, laser damage resistance increased dramatically; the average threshold fluence for damage initiation for 30 {micro}m wide scratches increased from 7 to 41 J/cm{sup 2}, and the statistical probability of damage initiation at 12 J/cm{sup 2} of an ensemble of scratches decreased from {approx}100 mm{sup -1} of scratch length to {approx}0.001 mm{sup -1}.

42 ENGINEERING↗

Laser Damage Precursors in Fused Silica

There is a longstanding, and largely unexplained, correlation between the laser damage susceptibility of optical components and both the surface quality of the optics, and the presence of near surface fractures in an optic. In the present work, a combination of acid leaching, acid etching, and confocal time resolved photoluminescence (CTP) microscopy has been used to study laser damage initiation at indentation sites. The combination of localized polishing and variations in indentation loads allows one to isolate and characterize the laser damage susceptibility of densified, plastically flowed and fractured fused silica. The present results suggest that: (1) laser damage initiation and growth are strongly correlated with fracture surfaces, while densified and plastically flowed material is relatively benign, and (2) fracture events result in the formation of an electronically defective rich surface layer which promotes energy transfer from the optical beam to the glass matrix.

42 ENGINEERING↗

Ultra-fast photoluminescence as a diagnostic for laser damage initiation

Using high-sensitivity confocal time-resolved photoluminescence (CTP) techniques, we report an ultra-fast photoluminescence (40ps-5ns) from impurity-free surface flaws on fused silica, including polished, indented or fractured surfaces of fused silica, and from laser-heated evaporation pits. This fast photoluminescence (PL) is not associated with slower point defect PL in silica which has characteristic decay times longer than 5ns. Fast PL is excited by the single photon absorption of sub-band gap light, and is especially bright in fractures. Regions which exhibit fast PL are strongly absorptive well below the band gap, as evidenced by a propensity to damage with 3.5eV ns-scale laser pulses, making CTP a powerful non-destructive diagnostic for laser damage in silica. The use of CTP to provide insights into the nature of damage precursors and to help develop and evaluate new damage mitigation strategies will be presented.

42 ENGINEERING↗

Metallic-like photoluminescence and absorption in fused silica surface flaws

Using high-sensitivity confocal time-resolved photoluminescence (PL) techniques, we report an ultra-fast PL (40ps-5ns) from impurity-free surface flaws on fused silica, including polished, indented or fractured surfaces of fused silica, and from laser-heated evaporation pits. This PL is excited by the single photon absorption of sub-band gap light, and is especially bright in fractures. Regions which exhibit this PL are strongly absorptive well below the band gap, as evidenced by a propensity to damage with 3.5eV ns-scale laser pulses.