Multiorbital charge-density wave excitations and concomitant phonon anomalies in Bi 2 Sr 2 LaCuO 6+δ

Charge-density waves (CDWs) are ubiquitous in underdoped cuprate superconductors. As a modulation of the valence electron density, CDWs in hole-doped cuprates possess both Cu-3d and O-2p orbital character owing to the strong hybridization of these orbitals near the Fermi level. Here, we investigate underdoped Bi 2 Sr 1.4 La 0.6 CuO 6+δ using resonant inelastic X-ray scattering (RIXS) and find that a short-range CDW exists at both Cu and O sublattices in the copper-oxide (CuO 2 ) planes with a comparable periodicity and correlation length. Furthermore, we uncover bond-stretching and bond-buckling phonon anomalies concomitant to the CDWs. Comparing to slightly overdoped Bi 2 Sr 1.8 La 0.2 CuO 6+δ , where neither CDWs nor phonon anomalies appear, we highlight that a sharp intensity anomaly is induced in the proximity of the CDW wavevector (Q CDW ) for the bond-buckling phonon, in concert with the diffused intensity enhancement of the bond-stretching phonon at wavevectors much greater than Q CDW . Our results provide a comprehensive picture of the quasistatic CDWs, their dispersive excitations, and associated electron-phonon anomalies, which are key for understanding the competing electronic instabilities in cuprates.

36 MATERIALS SCIENCE↗

Failure analysis of field-failed bypass diodes

Defective bypass diodes are often found as the largest factor leading to power loss in solar modules. Here, we report on failure mechanisms by investigating shunted bypass diodes from a rooftop installation, using a combination of multiple characterizations including current–voltage analysis, thermal-runaway testing, X-ray computed tomography, lock-in thermography, focused ion-beam cross-section imaging, chemical decapsulation, optical microscopy, and scanning electron microscopy with energy-dispersive X-ray spectroscopy. Differing from static discharge typically associated with lightning strikes on modules, we found diode failure by the mechanism of thermal damage under continuous, long-term overstress in forward bias. Our conclusion is based on evidence of energy dissipated—the small to medium extent of melt-through on the Schottky diode face. The diode failure shows distortions or roughening of the Schottky diode metal-semiconductor interface with the die attach, and some failures are accompanied by die-attach solder melting. We propose that nonuniform irradiance on the modules caused diode shunting due to extended periods of heat dissipation in the modules, because modules in this string were placed in two different orientations. In contrast, a second parallel module string of the same module type on the same rooftop with a unique plane of array did not show any diode failures. The thermal damage failure of melt-through was caused by the long-term current generated by overstressing of diodes that may have had crystalline and impurity defects.

14 SOLAR ENERGY↗

Thin-Film Solar Cells with 19% Efficiency by Thermal Evaporation of CdSe and CdTe

CdTe-based solar cells exhibiting 19% power conversion efficiency were produced using widely available thermal evaporation deposition of the absorber layers on SnO2-coated glass with or without a transparent MgZnO buffer layer. Evaporating CdSe and CdTe sequentially by thermal evaporation and subsequent CdCl2 annealing establishes efffective CdSeTe band grading as well as dense, large-grain films. These results show that high-performance II-VI photovoltaics can be made by inexpensive, commercially available evaporation systems without the need to build customized equipment, enabling CdTe photovoltaics research and manufacturing to be more accessible to the broader photovoltaics community.

14 SOLAR ENERGY↗

Comparison of PID Shunting in Polycrystalline and Single-Crystal Silicon Modules via Multi-Scale, Multi-Technique Characterization

We used the methods we reported last year to investigate potential-induced degradation (PID). We have now applied these methods to single-crystalline silicon modules that have degraded during field deployment, as well as in minimodules stressed in the laboratory. We will compare these results to the polycrystalline results presented last year. Small cores have been removed from the modules and subjected to analysis. We use a combination of photoluminescence and dark lock-in thermography imaging, laser marking, electron-beam induced current measurements, and subsequent focused ion-beam marking to allow analysis of individual defects via time-of-flight secondary-ion mass spectrometry (TOF-SIMS) to investigate the root-cause mechanism for PID shunting. We see a direct correlation between recombination active shunts and sodium content. The sodium content in shunted areas peaks at the SiN/Si interface and is consistently observed at a concentration of 0.1%-1% in shunted areas. TOF-SIMS data taken on degraded and non-degraded single-crystalline sample areas show a similar trend as in the polycrystalline samples: more sodium is seen in the degraded areas.

14 SOLAR ENERGY↗

Fill Factor Loss in Fielded Photovoltaic Modules Due to Metallization Failures, Characterized by Luminescence and Thermal Imaging

Understanding the causes of photovoltaic module failure in the field can be achieved using spatially-resolved imaging tools in combination with current-voltage (IV) characterization. We evaluate 23 field-degraded modules by comparing their IV characteristics with module images obtained by electroluminescence, photoluminescence, UV-fluorescence, and dark lock-in thermography. We identify primarily metallization failures (metallization series resistance, solder point heating, broken fingers, disrupted interconnects) in these modules that has led to a severe drop in the fill factor and up to 35% power loss over only 2 years of deployment.

14 SOLAR ENERGY↗

In-situ Microscopy Characterization of Cu(In,Ga)Se2 Potential-Induced Degradation

We report on the role of sodium in potentialinduced degradation (PID) of Cu(In, Ga)Se 2 (CIGS) solar cells. In-situ microscopy characterizations on AFM platform were performed on two stressed CIGS device under room temperature (RT) and high temperature (HT) at 85 degrees C. During PID stressing we observed depletion region gets wider as Na migrates, p-n junction becomes leaky at RT for over a month; and similar junction evolution was observed for HT-stressed sample, eventually the junction collapsed after 18 hours. The diode behaviors were confirmed by dark I-V measurement. Time-of Flight secondary-ion mass spectrometry reveals that the Na accumulates on ZnO and CdS side, as well as the upper layer of CIGS layer. The results indicate that Na drifted by the voltage applied on the soda-lime glass, then diffuse through the whole device. And the sodium profiles have different points of evolution due to the temperature differences between the two stressed samples. The consistent results unambiguously show how Na from substrate glass causes PID in CIGS solar cells.

14 SOLAR ENERGY↗

High Performance GaAs Solar Cells Grown at High Growth Rates by Atmospheric-Pressure Dynamic Hydride Vapor Phase Epitaxy

We report GaAs solar cells grown at rates exceeding 300 um/h by atmospheric-pressure dynamic hydride vapor phase epitaxy (D-HVPE). The surface morphology of the GaAs layers grown at those rates is smooth, with root mean square surface roughness of < 1.4 nm. We grew GaAs solar cells at rates from 35 - 309 um/h with negligible degradation in open circuit voltages (VOC), which ranged from 1.04 - 1.07 V. We showed the slight decrease in VOC is due to lack of doping optimization at higher growth rates. Deep level transient spectroscopy measurements showed low point defect densities that increases slightly with growth rate from 35 - 309 um/h. The low point defect concentrations and the high VOCs indicate that high material quality can be maintained at these extremely high growth rates, enabling the deposition of high efficiency cells in mere seconds instead of hours.

14 SOLAR ENERGY↗

Laser Cutting and Micromachining for Localized and Targeted Solar Cell Characterization

Laser cutting and micromachining can be applied to solar cell materials for processing and characterization applications. An ultrashort pulse (USP) laser with sub-picosecond pulse width can remove material with minimal thermal effects or damage, which is termed `cold ablation'. Such USP laser cutting and scribing can be implemented for isolating areas within a larger cell while maintaining electrical performance and preventing laser-induced damage and shunting. Laser micromachining has been used to isolate a shunt to improve cell performance and to isolate a small, selected area to define a sample suitable for deep level transient spectroscopy.

14 SOLAR ENERGY↗

Extracting Optical Bandgaps from Luminescence Images of Perovskite Solar Cells

We report a camera-based method to capture optical bandgap images of perovskite solar cells (PSCs). It is fast and non-destructive. It can also provide micron-scale spatial resolution. This imaging technique utilizes well-defined and relatively symmetrical band-to-band luminescence spectra emitted from perovskite materials. Their spectra can be fitted with Gaussian functions whose peak locations are similar to absorption thresholds and thus represent the material optical bandgaps. We apply the technique to resolve relative variations in optical bandgaps across various PSCs, and to show optical bandgap inhomogeneity within the same device due to material degradation and impurities. Degradation and impurities were found to both cause optical bandgap shifts inside the materials. Our results are independently confirmed with photoluminescence and absorption spectroscopy.

14 SOLAR ENERGY↗

From Modules to Atoms: Techniques and Characterization for Identifying and Understanding Device-Level Photovoltaic Degradation Mechanisms

This report documents how degraded modules are analyzed for the characterization of cell-level performance reduction. The primary degradation topics presented here are 1) potential-induced degradation, 2) defect metastability and impurity diffusion, and 3) partial-shading-induced reverse-bias breakdown. Imaging techniques, such as electroluminescence imaging, photoluminescence imaging, and lock-in thermography provide spatial information of full modules on the meter scale. Area of interest can then be imaged with higher spatial resolution by zooming in with fields of view near the mm scale. We document procedures for coring cell samples from selected regions of interest using mechanical drilling. The small samples are then of suitable size for various microscopic analyses using techniques such as scanning electron microscopy, time-of-flight secondary ion spectrometry, atomic force microscopy, electron beam induced current, transmission electron microscopy, and atom probe tomography, which can provide chemical, structural, and electrical characterization down to the atomic scale.

14 SOLAR ENERGY↗

Characterization and modeling of reverse-bias breakdown in Cu(In,Ga)Se 2 photovoltaic devices

Partial shading of series-connected thin-film photovoltaic modules can force shaded cells into reverse bias, which can cause rapid and irreversible power loss and reduce the practical module lifespan. Unfortunately, this is a common occurrence in field-deployed modules due to the myriad of environmental factors that can result in partial shading. In this work, we identify as-grown nonuniformities in the Cu(In,Ga)Se 2 (CIGS) absorber layers as the points of origin for the damage induced under reverse-bias conditions. The structure and chemistry associated with inclusions and voids in the CIGS films cause these features to act as resistive heating elements in reverse-bias conditions. This localized resistive heating provides the energy required to induce thermal runaway breakdown in the CIGS devices, resulting in damage to charge collection and reduced active area of a device. This mechanism is also described with a robust device model to connect the experimental observations with their physical origins.

14 SOLAR ENERGY↗

Laser Cutting and Micromachining for Localized and Targeted Solar Cell Characterization

Laser cutting and micromachining can be applied to solar cell materials for processing and characterization applications. An ultrashort pulse (USP) laser with sub-picosecond pulse width can remove material with minimal thermal effects or damage, which is termed 'cold ablation'. Such USP laser cutting and scribing can be implemented for isolating areas within a larger cell while maintaining electrical performance and preventing laser-induced damage and shunting. Laser micromachining has been used to isolate a shunt to improve cell performance and to isolate a small, selected area to define a sample suitable for deep level transient spectroscopy.

14 SOLAR ENERGY↗

In-situ Microscopy Characterization of Cu(In,Ga)Se2 Potential-Induced Degradation: Preprint

We report on the role of sodium in potential-induced degradation (PWe report on the role of sodium in potential-induced degradation (PID) of Cu(In, Ga)Se2 (CIGS) solar cells. In-situ microscopy characterizations on AFM platform were performed on two stressed CIGS device under room temperature (RT) and high temperature (HT) at 85 degrees C. During PID stressing we observed depletion region gets wider as Na migrates, p-n junction becomes leaky at RT for over a month; and similar junction evolution was observed for HT-stressed sample, eventually the junction collapsed after 18 hours. The diode behaviors were confirmed by dark I-V measurement. Time-of-Flight secondary-ion mass spectrometry reveals that the Na accumulates on ZnO and CdS side, as well as the upper layer of CIGS layer. The results indicate that Na drifted by the voltage applied on the soda-lime glass, then diffuse through the whole device. And the sodium profiles have different points of evolution due to the temperature differences between the two stressed samples. The consistent results unambiguously show how Na from substrate glass causes PID in CIGS solar cells.ID) of Cu(In, Ga)Se2 (CIGS) solar cells. In-situ microscopy characterizations on AFM platform were performed on two stressed CIGS device under room temperature (RT) and high temperature (HT) at 85 degrees C. During PID stressing we observed depletion region gets wider as Na migrates, p-n junction becomes leaky at RT for over a month; and similar junction evolution was observed for HT-stressed sample, eventually the junction collapsed after 18 hours. The diode behaviors were confirmed by dark I-V measurement. Time-of-Flight secondary-ion mass spectrometry reveals that the Na accumulates on ZnO and CdS side, as well as the upper layer of CIGS layer. The results indicate that Na drifted by the voltage applied on the soda-lime glass, then diffuse through the whole device. And the sodium profiles have different points of evolution due to the temperature differences between the two stressed samples. The consistent results unambiguously show how Na from substrate glass causes PID in CIGS solar cells.

14 SOLAR ENERGY↗

Large-Area Material and Junction Damage in c-Si Solar Cells by Potential-Induced Degradation

A new potential-induced degradation (PID) mechanism for c-Si is reported. Multiple characterization techniques in various aspects of a material's chemical, structural, electrical, and optoelectrical nature, as well as in atomic, nanometer, micrometer, millimeter, and cell and module scales, are combined. All results point consistently to a new discovery: substantial large-area deterioration of materials and junctions plays a major role.

14 SOLAR ENERGY↗

Prediction of Potential-Induced Degradation Rate of Thin-Film Modules in the Field Based on Coulombs Transferred

We validated the use of coulombs transferred between the active cell circuit and ground as an index for quantitatively predicting degradation rate in the field for two thin-film module types undergoing potential-induced degradation (PID). The dependence was determined by comparing the degradation rate and leakage current in the field (Cocoa, Florida) to accelerated tests (85 degrees C, 85% relative humidity), both with the application of -1,000 V bias to the cell circuit. The two module types, which degraded about 4% and 11% in power after application of 96 h of bias in chamber, degraded 5% in the field by PID within 200 days and 6 days, respectively. The signatures of PID in the thin-film modules by electroluminescence, photoluminescence, and thermography are shown so that PID in fielded thin-film modules can be identified.

14 SOLAR ENERGY↗

Artifact-Free Coring Procedures for Removing Samples from Photovoltaic Modules for Microscopic Analysis

An important step in producing more reliable and efficient photovoltaic modules is to establish a relationship between the microscopic properties of modules deployed in the field for many years and efficiency-related parameters. The first step in accomplishing this task is to be able to identify and remove small areas from these modules without causing any damage to these samples. In this work, we will describe two different procedures to core small areas of deployed and stressed solar panels produced with different materials (Si, CIGS, and CdTe), and we will prove that these processes did not damage the cored material. We will also show that the coring procedure changes for different types of photovoltaic modules.

14 SOLAR ENERGY↗

Thin-Film Module Reverse-Bias Breakdown Sites Identified by Thermal Imaging

Thin-film module sections are stressed under reverse bias to simulate partial shading conditions. Such stresses can cause permanent damage in the form of "wormlike" defects due to thermal runaway. When large reverse biases with limited current are applied to the cells, dark lock-in thermography (DLIT) can detect where spatially-localized breakdown initiates before thermal runaway leads to permanent damage. Predicted breakdown defect sites have been identified in both CIGS and CdTe modules using DLIT. These defects include small pinholes, craters, or voids in the absorber layer of the film that lead to builtin areas of weakness where high current densities may cause thermal damage in a partial-shading event.

14 SOLAR ENERGY↗