Engineering Papers⌕ Search

Engineering topics

Ji, Yichen

Publications and source records attributed to Ji, Yichen.

Site and Structural Requirements for the Dehydra-Decyclization of Cyclic Ethers on ZrO2

In this study, we examined the site and structural requirements for the dehydra-decyclization of cyclic ethers, tetrahydrofuran, and tetrahydropyran to produce conjugated dienes over ZrO2-based catalysts, a reaction that could be an important step in the use of biomass-derived sugars as a starting material to produce monomers for the plastics industry. To help identify the active sites for this reaction, studies were conducted in which ZrO2 surfaces were decorated with Na. These studies showed that Na was effective at poisoning the activity for the ring opening of cyclic ethers, but much less so for the dehydration of the resulting adsorbed alkoxides. The studies of the activity of different types of ZrO2 for the dehydra-decyclization reaction, including single crystals and ultra-thin films supported on MgAl2O4 and silica, also showed that the reaction was dependent on the local structure of the ZrO2 surface. The insights these results provide for identifying the active sites on the ZrO2 surface are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Selective dehydra-decyclization of cyclic ethers to conjugated dienes over zirconia

ZrO 2 provides high selectivity (>90%) to conjugated pentadienes through the dehydra-decyclization of C-5 cyclic ethers, even at high conversions. 1,3-Pentadiene was the major product in both reaction of 2-methyltetrahydrofuran and tetrahydropyran over ZrO 2 . The reaction of 3-methyltetrahydrofuran produced nearly stoichiometric amounts of isoprene. Other catalysts, including TiO 2 , γ-Al 2 O 3 , and H-ZSM-5, were generally much less selective and produced a mixture of diene isomers. A combination of TPD and steady-state measurements revealed that both piperylenes are exclusively produced through primary catalytic pathways from 2-methyltetrahydrofuran, avoiding any isomerization once formed. First-principle calculations on ZrO 2 imply the presence of an energetically favored, surface isomerization of ring-opened intermediates to conjugated alkenolates that selectively dehydrate to conjugated dienes, providing high selectivity to the desired products. Finally, the stabilization of the conjugated alkenolate is key for understanding the ability of ZrO 2 to selectively produce conjugated dienes from cyclic ethers, without the need for the thermo-limited diene isomerization.

1,3 -pentadiene↗

RFA Measurement of E-Cloud Generation Process at Fermilab Main Injector

Fermilab aims to provide greater beam power for the neutrino physics program. As the beam power increases, the unwanted production of secondary electrons in the beam pipe, known as ‘electron cloud’ or ‘E-cloud’ may become disruptive to high intensity operation. Instrumentation has been deployed in the Fermilab Main Injector (MI) to study E-cloud. One of these is a Retard Field Analyzer (RFA) that can be used to directly measure E-cloud generation at the location of the instrument. Studies of the dependence of E-cloud on beam intensity and bunch length have been carried out. The experimental results are compared to POSINST simulations. These simulations are guided by measurements from a Secondary Electron Yield (SEY) test stand installed in the MI to measure the SEY of materials such as the beam pipe stainless steel. The SEY has a strong influence on the E-cloud density. Results of these comprehensive studies comparing the RFA data with realistic MI simulations will be presented.

43 PARTICLE ACCELERATORS↗

Investigation of Rh–titanate (ATiO 3 ) interactions on high-surface-area perovskite thin films prepared by atomic layer deposition

Thin, ~1 nm films of CaTiO 3 , SrTiO 3 , and BaTiO 3 were deposited onto MgAl 2 O 4 by Atomic Layer Deposition (ALD) and studied as catalyst supports for Rh. Scanning Transmission Electron Microcopy (STEM) and X-Ray Diffraction (XRD) demonstrated that the films had the perovskite structure and formed uniform coatings stable up to 1073 K. Rh, added by ALD, interacted strongly with CaTiO 3 and somewhat less strongly with SrTiO 3 , while Rh on BaTiO 3 was similar to Rh on unmodified MgAl 2 O 4 . STEM measurements of Rh on CaTiO 3 films showed Rh remained well dispersed after repeated oxidations and reductions at 1073 K; however, the Rh was inactive for CO-oxidation. Rh formed small particles on SrTiO 3 films and was active for CO oxidation after reduction at 1073 K. The reducibility and catalytic activity of Rh/BaTiO 3 /MgAl 2 O 4 were similar to that of Rh/MgAl 2 O 4 . Evidence from CO-TPR, FTIR, and XPS all indicated that the degree of interaction between Rh and the three perovskite films can be ranked in the following order: Rh/CaTiO 3 /MgAl 2 O 4 > Rh/SrTiO 3 /MgAl 2 O 4 > Rh/BaTiO 3 /MgAl 2 O 4 . Here, bulk ex-solution catalysts, synthesized by reduction of ATi 0.98 Rh 0.02 O 3 (A = Ca, Sr, and Ba), were also examined for comparison.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dehydra-decyclization of tetrahydrofurans to diene monomers over metal oxides

The dehydra-decyclization of tetrahydrofuran (THF) to butadiene was investigated over a series of metal oxide catalysts, where a common set of chemical pathways was identified. Alongside butadiene, propene is formed via a retro-Prins condensation as the main side product typically observed. Reaction occurred at similar temperatures on each of the oxides, but tetragonal zirconia (t-ZrO 2 ) and monoclinic zirconia (m-ZrO 2 ) were unique in showing high selectivity to butadiene (>90%). Near quantitative yields to butadiene could be achieved over t-ZrO 2 at 673 K and a WHSV of 0.93 g THF gcat –1 h –1 . Through contact time studies, butadiene is determined to be a primary product. Methyl-substituted THF gave only moderate increases in rates and the products showed minimal isomerization of the carbon backbone. The t-ZrO 2 catalyst was found to be relatively stable with time on stream, experiencing coking as a likely source of deactivation. Complete regeneration of the catalyst was demonstrated through calcination alone, allowing for multiple regenerations with no irreversible loss in activity or selectivity. Lastly, the catalytic activity of zirconia was found to be structure insensitive, with t-ZrO 2 and m-ZrO 2 exhibiting similar initial activities; however, m-ZrO 2 was observed to deactivate much more rapidly.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atomic Layer Deposition for Preparing Isolated Co Sites on SiO 2 for Ethane Dehydrogenation Catalysis

Unlike Co clusters, isolated Co atoms have been shown to be selective for catalytic dehydrogenation of ethane to ethylene; however, preparation of isolated Co sites requires special preparation procedures. Here, we demonstrate that Atomic Layer Deposition (ALD) of tris(2,2,6,6-tetramethyl-3,5-heptanedionato)cobalt(III) (Co(TMHD) 3 ) on silica and other supports is effective in producing these isolated species. Silica-supported catalysts prepared with one ALD cycle showed ethylene selectivities greater than 96% at 923 K and were stable when CO 2 was co-fed with the ethane. Co catalysts prepared by impregnation formed clusters that were significantly less active, selective, and stable. Rates and selectivities also decreased for catalysts with multiple ALD cycles. Isolated Co catalysts prepared on Al 2 O 3 and MgAl 2 O 4 showed reasonable selectivity for ethane dehydrogenation but were not as effective as their silica counterpart.

36 MATERIALS SCIENCE↗

“Intelligent” Pt Catalysts Studied on High-Surface-Area CaTiO 3 Films

CaTiO 3 -supported Pt is sometimes referred to as an “Intelligent” catalyst because Pt can reversibly leave or enter the perovskite lattice following high-temperature reduction or oxidation; however, slow egress-ingress kinetics associated with large perovskite crystallites make these systems impractical. In this study, thin films (~1 nm) of CaTiO 3 were deposited onto MgAl 2 O 4 and then examined as catalyst supports for Pt and Pd. While Pd/CaTiO 3 /MgAl 2 O 4 showed adsorption and CO-oxidation properties that were essentially the same as Pd/MgAl 2 O 4 , the Pt/CaTiO 3 /MgAl 2 O 4 catalyst exhibited evidence for strong support interactions. Pt/CaTiO 3 /MgAl 2 O 4 showed high activity for CO oxidation following reduction at 1073 K, even though CO adsorption was suppressed; but the catalysts were dramatically less active after oxidation at 1073 K and reduction at 773 K. Both Pt/CaTiO 3 /MgAl 2 O 4 and a catalyst formed by ex-solution of CaTi 0.95 Pt 0.05 O 3 exhibited very low rates for toluene hydrogenation in comparison to Pt/MgAl 2 O 4 . Scanning Transmission Electron Microscopy (STEM) and Energy Dispersive Spectroscopy (EDS) showed that the CaTiO 3 films uniformly covered the MgAl 2 O 4 surface after both reduction and oxidation at 1073 K. Pt particles on reduced Pt/CaTiO 3 /MgAl 2 O 4 exhibited an unusual rhombohedral shape and may be flat, a further indication of strong interactions between the metal and the support. Low Energy Ion Scattering (LEIS) indicated that high-temperature reduction caused a restructuring of the CaTiO 3 . Lastly, the implications of these results for understanding catalysts formed by ex-solution of metals from a perovskite lattice are discussed.

36 MATERIALS SCIENCE↗

Probing direct carbon-carbon acylation of furans and long-chain acids over H-ZSM-5

The acylation of furan and 2-methylfuran (2-MF) with acetic acid (AA) and 1-hexanoic acid (HA) was studied over an H-ZSM-5 catalyst. Temperature-programmed desorption (TPD) measurements showed evidence that AA adsorbs strongly at Brønsted sites, with reaction to CO 2 and acetone beginning at 523 K, while both furan and 2-MF oligomerize upon adsorption at room temperature. Steady-state, flow-reactor measurements demonstrate that selectivities for the acylation reactions can approach 100% below 523 K when reactions are operated in excess organic acids, with maximum conversion limited by equilibrium. Coking becomes important when the reaction is operated in excess furan or 2-MF and at high reactant concentrations, while ketonization products are observed when the reaction is performed above 523 K. Lastly, potential uses for the reactions are discussed.

1-Hexanoic Acid↗

Electron Cloud Studies at Fermilab

The presence of unwanted electrons in an accelerator vacuum chamber, known as E-cloud (E-cloud) can potentially cause operational problems in the Fermilab Main Injector (MI) and Recycler Ring (RR). E-cloud has caused instability in the RR in the past, and although it is not currently a problem, there is measurable E-cloud in the MI accelerator. There are planned beam intensity increases due to upgrades of the Fermilab accelerator complex, so E-cloud could become a problem. Some work has been done by others previously to understand how low SEY (Secondary Electron Yield coefficient) coatings might mitigate production of E-cloud, and to model the mechanism whereby E-cloud causes beam instability. Using previous studies as a base, this research took several approaches toward understanding the risk of E-cloud at Fermilab. The evolution of the SEY of the SS316L (stainless steel), TiN coated SS316L, and amorphous carbon coated SS316L were measured in-situ using a SEY meas urement station in the MI tunnel. The SEY of these materials change over time either due to bombardment of the E-cloud, or disruption of vacuum conditions. The SEY evolution was tracked over a several year period to find out how long it takes for the SEY of each material to reach its lowest level, and how much the SEY rises during deconditioning periods of poor vacuum. The SEY measurement results can be used to determine whether the SS316L will be a problem at upgrade intensities, and if so, whether or not TiN and A-Carbon coatings can mitigate E-cloud related problems sufficiently. Direct measurements of the E-cloud were done as well, and compared to simulation. The E-cloud bombardment rate was measured at different beam intensities and bunch lengths. It was possible to get detailed information on how the E-cloud varies over the acceleration cycle, where sensitivity to bunch length is reflected in the evolution of the E-cloud. The Retarding Field Analyzer (RFA) measuring th e E-cloud bombardment rate was near the instrument that is u! sed to measure the SEY of the beam pipe material. This proximity provided an accurate SEY value for simulations, so that the simulated E-cloud bombardment rate could be better compared to measurement. Bunch length measurements and computations generated accurate bunch length information also needed as input for simulations. After this careful control of the input parameters, the POSINST simulations of E-cloud were a good match to direct measurements. This gave confidence that predictions could be made concerning the E-cloud densities at upgrade intensities. These densities were compared against corresponding proton densities to predict the SEY required to avoid instabilities. That prediction and the information provided by the SEY measurements provide helpful information regarding the risks of E-cloud effects at future beam intensities at Fermilab.

43 PARTICLE ACCELERATORS↗

Fast Transverse Instability and Electron Cloud Measurements in Fermilab Recycler

A new transverse instability is observed that may limit the proton intensity in the Fermilab Recycler. The instability is fast, leading to a beam-abort loss within two hundred turns. The instability primarily affects the first high-intensity batch from the Fermilab Booster in each Recycler cycle. This paper analyzes the dynamical features of the destabilized beam. The instability excites a horizontal betatron oscillation which couples into the vertical motion and also causes transverse emittance growth. This paper describes the feasibility of electron cloud as the mechanism for this instability and presents the first measurements of the electron cloud in the Fermilab Recycler. Direct measurements of the electron cloud are made using a retarding field analyzer (RFA) newly installed in the Fermilab Recycler. Indirect measurements of the electron cloud are made by propagating a microwave carrier signal through the beampipe and analyzing the phase modulation of the signal. The maximum betatron amplitude growth and the maximum electron cloud signal occur during minimums of the bunch length oscillation.

43 PARTICLE ACCELERATORS↗