Engineering Papers⌕ Search

Engineering topics

Jenkins, Mark W.

Publications and source records attributed to Jenkins, Mark W..

Diagnosis of Factors Impacting Yield in Multilayer Devices for Superconducting Electronics

The ability to localize defects in order to understand failure mechanisms in complex superconducting electronics circuits, while operating at low temperature, does not yet exist. Here, this work applies thermally-induced voltage alteration (TIVA), to a biased superconducting electronics (SCE) circuit at ambient temperature. TIVA is a commonly used, laser-based failure analysis technique developed for silicon-based microelectronics. The non-operational circuit consisted of an arithmetic logic unit (ALU) in a high-frequency test bed designed at HYPRES and fabricated by MIT Lincoln Laboratory using their SFQ5ee process. Localized TIVA signals were correlated with reflected light images at the surface, and these sites were further investigated by scanning electron microscopy imaging of focused ion-beam cross-sections. The areas investigated, where prominent TIVA signals were observed, showed seams in the Nb wiring layers at contacts to Josephson junctions or inductors and/or disrupted junction morphologies. Finally, these results suggest that the TIVA technique can be used at ambient temperature to diagnose fabrication defects that may cause low temperature circuit failure.

36 MATERIALS SCIENCE↗

Precision Laser Annealing of Focal Plane Arrays

We present results from laser annealing experiments in Si using a passively Q-switched Nd:YAG microlaser. Exposure with laser at fluence values above the damage threshold of commercially available photodiodes results in electrical damage (as measured by an increase in photodiode dark current). We show that increasing the laser fluence to values in excess of the damage threshold can result in annealing of a damage site and a reduction in detector dark current by as much as 100x in some cases. A still further increase in fluence results in irreparable damage. Thus we demonstrate the presence of a laser annealing window over which performance of damaged detectors can be at least partially reconstituted. Moreover dark current reduction is observed over the entire operating range of the diode indicating that device performance has been improved for all values of reverse bias voltage. Additionally, we will present results of laser annealing in Si waveguides. By exposing a small (<10 um) length of a Si waveguide to an annealing laser pulse, the longitudinal phase of light acquired in propagating through the waveguide can be modified with high precision, <15 milliradian per laser pulse. Phase tuning by 180 degrees is exhibited with multiple exposures to one arm of a Mach-Zehnder interferometer at fluence values below the morphological damage threshold of an etched Si waveguide. No reduction in optical transmission at 1550 nm was found after 220 annealing laser shots. Modeling results for laser annealing in Si are also presented.

42 ENGINEERING↗

1 Mil Gold Bond Wire Study

In microcircuit fabrication, the diameter and length of a bond wire have been shown to both affect the current versus fusing time ratio of a bond wire as well as the gap length of the fused wire. This study investigated the impact of current level on the time-to-open and gap length of 1 mil by 60 mil gold bond wires. During the experiments, constant current was provided for a control set of bond wires for 250ms, 410ms and until the wire fused; non-destructively pull-tested wires for 250ms; and notched wires. The key findings were that as the current increases, the gap length increases and 73% of the bond wires will fuse at 1.8A, and 100% of the wires fuse at 1.9A within 60ms. Due to the limited scope of experiments and limited data analyzed, further investigation is encouraged to confirm these observations.

Huff, Johnathon D.↗

Conductor fusing and gapping for bond wires

In this paper, fusing of a metallic conductor is studied by judiciously using the solution of the one-dimensional heat equation, resulting in an approximate method for determining the threshold fusing current. The action is defined as an integration of the square of the wire current over time. The burst action (the action required to completely vaporize the material) for an exploding wire is then used to estimate the typical wire gapping action (involving wire fusing), from which gapping time can be estimated for a gapping current greater than a factor of two over the fusing current. The test data are used to determine the gapped length as a function of gapping current and to show, for a limited range, that the gapped length is inversely proportional to gapping time. The gapping length can be used as a signature of the fault current level in microelectronic circuits.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗