Point Defects in CdZnTe Crystals Grown by Different Techniques

We studied, by current deep-level transient spectroscopy (I-DLTS), point defects in CdZnTe detectors grown by different techniques. We identified 12 different traps with energy levels from 7 meV to 1.1 eV. Although the levels of most of the identified defects were independent of the crystal growth techniques, nevertheless there were some associated differences in the traps energies and densities.

36 MATERIALS SCIENCE↗

Effect of Te Inclusions in CdZnTe Crystals at Different Temperatures

CdZnTe crystals often exhibit nonuniformities due to the presence of Te inclusions and dislocations. High concentrations of such defects in these crystals generally entail severe charge-trapping, a major problem in ensuring the device's satisfactory performance. In this study, we employed a high-intensity, high-spatial-resolution synchrotron x-ray beam as the ideal tool to generate charges by focusing it over the large Te inclusions, and then observing the carrier's response at room- and at low-temperatures. A high spatial 5-{micro}m resolution raster scan revealed the fine details of the presence of extended defects, like Te inclusions and dislocations in the CdZnTe crystals. A noticeable change was observed in the efficiency of electron charge collection at low temperature (1 C), but it was hardly altered at room-temperature.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Defect Levels of Indium-doped CdMnTe Crystals

Using photoluminescence (PL) and current deep-level transient spectroscopy (I-DLTS), we investigated the electronic defects of indium-doped detector-grade CdMnTe:In (CMT:In) crystals grown by the vertical Bridgman method. We similarly analyzed CdZnTe:In (CZT:In) and undoped CdMnTe (CMT) crystals grown under the amount of same level of excess Te and/or indium doping level to detail the fundamental properties of the electronic defect structure more readily. Extended defects, existing in all the samples, were revealed by synchrotron white beam x-ray diffraction topography and scanning electron microscopy. The electronic structure of CMT is very similar to that of CZT, with shallow traps, A-centers, Cd vacancies, deep levels, and Te antisites. The 1.1-eV deep level, revealed by PL in earlier studies of CZT and CdTe, were attributed to dislocation-induced defects. In our I-DLTS measurements, the 1.1-eV traps showed different activation energies with applied bias voltage and an exponential dependence on the trap-filling time, which are typical characteristics of dislocation-induced defects. We propose a new defect-trap model for indium-doped CMT crystals.

36 MATERIALS SCIENCE↗

Influence of contacts on charge collection in an Au/CdTe/Au detector: A Simulation

We report our simulations on the influence of contacts on charge collection in semi-insulating (CdZn)Te with Au contacts under radiation flux, employing simultaneous solutions of the drift-diffusion and Poisson equations. The type of the space charge and the distribution of the electric field in the Au/(CdZn)Te/Au structure at high fluxes reflect the combined influence of charge generated by band bending at the electrodes, and from photogenerated carriers trapped at deep levels. We show that the space charge originating from the latter approaches dominance at high fluxes while the influence of the contacts becomes negligible. The ratio of trapping and collection times at low fluxes strongly depends on band bending, due mainly to a change in the occupation of deep levels by injection or depletion from the contacts. Such dependence is weak at high fluxes; in this case, the space charge due to trapped carriers prevails over that formed due to band bending. These phenomena can cause the formation an electric-field minimum within the device (the pinch point), the position of which is influenced by the nature of the contacts. The field minimum can completely disappear or develop into a dead layer as band bending changes.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Contacts for high-resistivity (Cd,Mn)Te crystals

Semi-insulating (Cd,Mn)Te crystals offer a material that may compete well with the commonly used (Cd,Zn)Te crystals for manufacturing large-area X- and gamma-ray detectors. The Bridgman growth method yields good quality, high-resistivity (10{sup 9} - 10{sup 10} {Omega} {center_dot} cm) crystals of (Cd,Mn)Te:V. Doping the as-grown crystals with the compensating agent vanadium ({approx} 10{sup 16} cm{sup -3}) ensures their high resistivity; thereafter, annealing them in cadmium vapors reduces the number of cadmium vacancies. Applying the crystals as detectors necessitates having satisfactory electrical contacts. Accordingly, we explored various techniques of ensuring good electrical contacts to these semi-insulating (Cd,Mn)Te crystals, assessing metallic layers, monocrystalline semiconductor layers, and amorphous (or nanocrystalline) semiconductor layers. We found that ZnTe heavily doped ({approx} 10{sup 18} cm{sup -3}) with Sb, and CdTe heavily doped ({approx} 10{sup 17} cm{sup -3}) with In, proved satisfactory semiconductor contact layers. They subsequently enabled us to establish good contacts (with only narrow tunneling barriers) to the Au layer that usually constitutes the most external contact layer. We outline our technology of applying electrical contacts to semi-insulating (Cd,Mn)Te, and describe some important properties.

(Cd↗

Extended defects in CdZnTe crystals: Effects on device performance

We explored some unique defects in a batch of cadmium zinc telluride (CdZnTe) crystals, along with dislocations and Te-rich decorated features, revealed by chemical etching. We extensively investigated these distinctive imperfections in the crystals to identify their origin, dimensions, and distribution in the bulk material. We estimated that these features ranged from 50 to 500 {micro}m in diameter, and their depth was about 300 {micro}m. The density of these features ranged between 2 x 10{sup 2} and 1 x 10{sup 3} per cm{sup 3}. We elaborated a model of them and projected their effect on charge collection and spectral response. In addition, we fabricated detectors with these defective crystals and acquired fine details of charge-transport phenomena over the detectors volume using a high-spatial resolution (25 {micro}m) X-ray response mapping technique. We related the results to better understand the defects and their influence on the charge-transport properties of the devices. The role of the defects was identified by correlating their signatures with the findings from our theoretical model and our experimental data.

98 NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL P↗

Effective surface passivation of CdMnTe materials

Passivation is an important process that reduces surface leakage current and its attendant noise. We treated detector-grade large-volume CdMnTe:In samples with an (NH{sub 4})-based passivant, and compared the results with untreated samples by measuring current-voltage characteristics, surface recombination velocity, Raman spectroscopy, and charge-collection mapping. The leakage current of the passivated CdMnTe (CMT) detectors decreased five to ten times, and surface recombination declined five to six times, depending on the passivation conditions applied. We satisfactorily explained these improvements in detector performance as resulting from different passivation layers that were generated by distinct chemical reactions, as determined by the pH of the passivant.

36 MATERIALS SCIENCE↗

Defect levels and thermomigration of Te precipitates in CdZnTe:Pb

Semi-insulating Cd0.9Zn0.1Te:Pb crystals were grown by the vertical Bridgman method. Measurements of the current deep level transient spectroscopy (I-DLTS) revealed three trap levels in this material. Unlike other compensating dopants, CdZnTe:Pb samples do not show any Cd-vacancies defects and A-center levels. We subjected them to temperature-gradient annealing in Cd overpressure at 490–717 1C, and recorded an exponential relationship between the annihilation time of Te precipitates and the annealing temperature. The energy resolution of an annealed CdZnTe:Pb detector, tested using a 137Cs radioactive source, gave an energy resolution of 2.5%.

98 NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL P↗

Investigations of Cadmium Manganese Telluride Crystals for Room-temperature Radiation Detection

Cadmium manganese telluride (CMT) has high potential as a material for room-temperature nuclear-radiation detectors. We investigated indium-doped CMT crystals taken from the stable growth region of the ingot and compared its characteristics with that from the last-to-freeze region. We employed different techniques, including synchrotron white-beam x-ray topography (SWBXT), current-voltage (I-V) measurement, and low-temperature photoluminescence spectra, and we also assessed their responses as detectors of radiation exposure. The crystal from the stable growth region proved to be superior to that from the last-to-freeze region; it is a single-grain crystal, free of twins, and displayed a resistivity higher by one order of magnitude. The segregation of indium dopant in the ingot might be responsible for its better resistivity. Furthermore, we recorded a good response in the detector fabricated from the crystal taken from the stable growth region; its ({mu}{tau})e value was 2.6 x 10{sup -3} cm{sup 2}/V, which is acceptable for thin detectors, including their application in medicine.

36 MATERIALS SCIENCE↗

Te Inclusions in CZT Detectors: New Method for Correcting Their Adverse Effects

Both Te inclusions and point defects can trap the charge carriers generated by ionizing particles in CdZnTe (CZT) detectors. The amount of charge trapped by point defects is proportional to the carriers' drift time and can be corrected electronically. In the case of Te inclusions, the charge loss depends upon their random locations with respect to the electron cloud. Consequently, inclusions introduce fluctuations in the charge signals, which cannot be easily corrected. In this paper, we describe direct measurements of the cumulative effect of Te inclusions and its influence on the response of CZT detectors of different thicknesses and different sizes and concentrations of Te inclusions. We also discuss a means of partially correcting their adverse effects.

74 ATOMIC AND MOLECULAR PHYSICS↗

Investigations of Cadmium Manganese Telluride Crystals for Room-Temperature Radiation Detection

Cadmium manganese telluride (CMT) has high potential as a material for room-temperature nuclear-radiation detectors. We investigated indium-doped CMT crystals taken from the stable growth region of the ingot, and compared its characteristics with that from the last-to-freeze region. We employed different techniques, including synchrotron white-beam X-ray topography (SWBXT), current-voltage (I-V) measurements, and low-temperature photoluminescence spectra, and we also assessed their responses as detectors to irradiation exposure. The crystal from the stable growth region proved superior to that from the last-to-freeze region; it is a single-grain crystal, free of twins, and displayed a resistivity higher by two orders-of-magnitude. The segregation of indium dopant in the ingot might be responsible for its better resistivity. Furthermore, we recorded a good response in the detector fabricated from the crystal taken from the stable growth region; its ({mu}{tau}){sub e} value was 2.6 x 10{sup -3} cm{sup 2}/V, which is acceptable for thin detectors, including for applications in medicine.

98 NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL P↗