Vacancy mechanism of oxygen diffusivity in bcc Fe: A first-principles study
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Jablonski, P D.
Explore the source record for details and available documents.
Molecular dynamics (MD) is a powerful tool to probe the thermodynamic and kinetic properties of solid, glass and liquid phases. In classical molecular dynamics (CMD), empirical models are used to describe the force by considering bond, bend and dihedral angle contributions with parameters fitted to experimental data or first-principles calculations of small clusters. In the ab initio molecular dynamics (AIMD), the forces are calculated on the fly using the first-principles density functional theory as discussed above. In the present work, we use AIMD simulations to follow the random walk of atoms in the liquid state. Based on the mean square displacements (MSD), the diffusion coefficients are calculated from the Einstein equation. Furthermore, we extend this approach to understand the diffusion in grain boundaries.
Cast forms of traditionally wrought Ni-base precipitation-strengthened superalloys are being considered for service in the ultra-supercritical conditions (760°C, 35MPa) of next-generation steam boilers and turbines. After casting and homogenization, these alloys were given heat-treatments typical for each in the wrought condition to develop the gamma-prime phase. Specimens machined from castings were creep-rupture tested in air at 800°C. In their wrought forms, alloy 282 is expected to precipitate M<SUB>23</SUB>C<SUB>6</SUB> within grain boundaries, alloy 740 is expected to precipitate several grain boundary phases including M<SUB>23</SUB>C<SUB>6</SUB>, G Phase, and η phase, and alloy 263 has M<SUB>23</SUB>C6 and MC within its grain boundaries. This presentation will correlate the observed creep-life of these cast alloys with the microstructures developed during creep-rupture tests, with an emphasis on the phase identification and chemistry of precipitated grain boundary phases. The suitability of these cast forms of traditionally wrought alloys for turbine and boiler components will also be discussed.
The high temperature components within conventional coal fired power plants are manufactured from ferritic/martensitic steels. In order to reduce greenhouse gas emissions the efficiency of pulverized coal steam power plants must be increased. The proposed steam temperature in the Advanced Ultra Supercritical (A-USC) power plant is high enough (760°C) that ferritic/martensitic steels will not work due to temperature limitations of this class of materials; thus Ni-based superalloys are being considered. The full size castings are quite substantial: ~4in thick, several feet in diameter and weigh 5-10,000lb each half. Experimental castings were quite a bit smaller, but section size was retained and cooling rate controlled in order to produce relevant microstructures. A multi-step homogenization heat treatment was developed in order to better deploy the alloy constituents. The castability of two traditionally wrought Ni-based superalloys to which minor alloy adjustments have been made in order to improve foundry performance is further explored.
We have developed a computationally based approach to optimizing the homogenization heat treatment of complex alloys. The Scheil module within the Thermo-Calc software is used to predict the as-cast segregation present within alloys, and DICTRA (Diffusion Controlled TRAnsformations) is used to model the homogenization kinetics as a function of time, temperature and microstructural scale. We will discuss this approach as it is applied to both Ni based superalloys as well as the more complex (computationally) case of alloys that solidify with more than one matrix phase as a result of segregation. Such is the case typically observed in martensitic steels. With these alloys it is doubly important to homogenize them correctly, especially at the laboratory scale, since they are austenitic at high temperature and thus constituent elements will diffuse slowly. The computationally designed heat treatment and the subsequent verification real castings are presented.
Oxide ridges formed during the transient stage oxidation of the scale evolution in iron alloys containing 22 wt % Cr that were held at 800 C in dry air. The surface oxidation process was imaged in situ through a confocal scanning laser microscope, and the results were correlated with postexperiment characterization through scanning electron microscopy and the DualBeam system (focus ion beam and electron beam) analysis combined with three-dimensional reconstruction. The oxide ridges that formed on top of the Cr oxide scale overlapped the intersections of the underlying alloy grain boundaries with the Cr oxide scale. Ridges were generally very small on grain boundaries with disorientation angles of less than 15{sup o}, and it was suggested that the boundaries of the surface grains in the alloy may serve as bottlenecks for the transport of scale-forming elements. The effects of La (120 and 290 ppm) and Ce (270 and 610 ppm) additions during melt-stage processing were also investigated.
This paper presents the high temperature mechanical properties of several experimental low coefficient of thermal expansion (CTE) alloys. The use of such alloys facilitate the extension of advanced ferritic stainless steels to higher use temperature in advanced power generation systems. We find that one of these alloys, J5 appears to be favorable for bridging ferritic alloys (operating up to ~600°C) to traditional nickel based superalloys (operating at 750°C).
Chromia (Cr2O3) forming ferritic stainless steels are being developed for interconnect application in Solid Oxide Fuel Cells (SOFC). A problem with these alloys is that in the SOFC environment chrome in the surface oxide can evaporate and deposit on the electrochemically active sites within the fuel cell. This poisons and degrades the performance of the fuel cell. The development of steels that can form conductive outer protective oxide layers other than Cr2O3 or (CrMn)3O4 such as TiO2 may be attractive for SOFC application. This study was undertaken to assess the oxidation behavior of ferritic stainless steel containing 1 weight percent (wt.%) Ti, in an effort to develop alloys that form protective outer TiO2 scales. The effect of Cr content (6–22 wt.%) and the application of a Ce-based surface treatment on the oxidation behavior (at 800° C in air+3% H2O) of the alloys was investigated. The alloys themselves failed to form an outer TiO2 scale even though the large negative {delta}G of this compound favors its formation over other species. It was found that in conjunction with the Ce-surface treatment, a continuous outer TiO2 oxide layer could be formed on the alloys, and in fact the alloy with 12 wt.% Cr behaved in an identical manner as the alloy with 22 wt.% Cr.
The corrosion behaviors of a low silicon and aluminum 430 stainless steel with and without ceria surface treatment were investigated in a simulated coal syngas at 800 {degree sign}C and in air. Thermodynamic calculations were made to predict carbon activities for the coal syngas as a function of temperature. At 800 {degree sign}C, carbon activity is ~1.1, which indicates that carbon that forms could diffuse into the steel and induce carbon corrosion, e.g. carburization and metal dusting. The surface morphology was investigated with X-ray diffraction and scanning electron microscopy. In coal gas, the scale formed on bare steel consisted of Mn1.5Cr1.5O4 and Cr2O3 and on ceria treated steel (Fe, Mn)O, FeCr2O4, Cr2O3, and CeCrO3. Both materials underwent carburization, but not metal dusting. The results of oxidation in air using a thermogravimetric apparatus confirmed that the 430 sample was less resistant to oxidation than the 430 treated with ceria.