Revealing the Roles of CuF 2 /NiF 2 Incorporation in the Electrochemical Performance of FeF 3 Cathodes in Solid‐State Batteries

Mixed metal fluorides have been considered as a promising candidate to lower the voltage hysteresis of conversion-type iron fluoride cathodes, but their cycling stability is limited due to transition metal dissolution and interphase growth in liquid electrolyte batteries. Here, we study the role of incorporating CuF 2 and NiF 2 in the electrochemical performance of FeF 3 cathode in halide-based solid-state batteries to test whether we can transfer the kinetic benefit of low voltage hysteresis to solid-state batteries while using solid electrolyte to eliminate transition metal dissolution and stabilize the interphase. Synchrotron X-ray absorption spectroscopy results indicated the redox reactions are attributed to Cu 0 /Cu + and Fe 0 /Fe 2+ in 25CuF 2 -75FeF 3 and Ni 0 /Ni 2+ and Fe 0 /Fe 3+ in 10NiF 2 -90FeF 3 . While no apparent improvement in electrode kinetics can be observed, the incorporation of CuF 2 and NiF 2 can largely improve the cycling stability of FeF 3 cathodes. In conclusion, the results demonstrate the advantages of using solid-state concept to improve the cycling stability of conversion-type cathodes.

25 ENERGY STORAGE

Anode-less Solid-State Li–S Batteries Enabled by Fe-Stabilized Polysulfides

Anode-less solid-state lithium-sulfur batteries (SSLSBs) with lithium sulfide (Li 2 S) as the cathode promise a high energy density and ease of manufacturing. However, Li 2 S is plagued by poor conductivity, sluggish activation kinetics, and a poor cycle life. Here, in this study, we report an FeCl 3 -activated Li 2 S (FLS) cathode with solid-state polysulfide intermediates generated through a redox reaction between FeCl 3 and Li 2 S. This strategy is shown to boost the electrical conductivity of Li 2 S by 7 orders of magnitude and lower the activation barrier. During cycling, Fe plays a significant role in stabilizing the highly active polysulfide species, contributing to the exceptional electrochemical performance. The FLS cathode achieves 80% capacity retention over 500 cycles with >99% Li 2 S utilization. Furthermore, a Li-metal-free (anode-less) full cell retained over 80% of its initial capacity after 240 cycles. This work underscores the promise of leveraging Fe-stabilized polysulfides in enabling high-energy, long-lasting, solid-state Li-S batteries.

25 ENERGY STORAGE

Revealing key structures for reversible sulfur redox in amorphous polymeric sulfur

Amorphous polymeric sulfur cathodes, such as sulfurized polyacrylonitrile (SPAN), enable high-energy lithium-sulfur batteries without cobalt or nickel, leveraging abundant sulfur. However, the limited in situ understanding of their synthesis and electrochemistry has impeded targeted optimization. Here, in this study, we integrate operando high-energy total scattering with sulfur K-edge X-ray absorption spectroscopy to monitor SPAN's formation and cycling in real time. Our results show that S-C bond formation halts further fusion of cyclized polyacrylonitrile, fostering π-π stacking and a transition from long-chain to short-chain sulfur-critical for reversible sulfur redox. These features synergistically minimize polysulfide dissolution and charge-transfer resistance, enabling optimized SPAN to achieve high capacity retention over 1,000 cycles. Operando X-ray absorption spectroscopy reveals that residual protons drive thiol-thione tautomerism, with lithium replacement during the first discharge causing ~20% irreversible capacity loss. To enhance performance, minimizing -NH groups and expanding pyridine networks are key. These findings transform SPAN optimization from empirical tuning to mechanism‑guided engineering and point the way towards sulfur loadings and energy densities competitive with state‑of‑the‑art Li‑ion cathodes.

25 ENERGY STORAGE