In-situ TEM study of the ion irradiation behavior of U 3 Si 2 and U 3 Si 5

We report that U 3 Si 2 and U 3 Si 5 are two important uranium silicide phases currently under extensive investigation as potential fuel forms or components for light water reactors (LWRs) to enhance accident tolerance. In this paper, their irradiation behaviors are studied by ion beam irradiations with various ion mass and energies, and their microstructure evolution is investigated by in-situ transmission electron microscopy (TEM). U 3 Si 2 can easily be amorphized by ion beam irradiations (by 1MeV Ar 2+ or Kr 2+ ) at room temperature with the critical amorphization dose less than 1 dpa. The critical amorphization temperatures of U 3 Si 2 irradiated by 1MeV Kr 2+ and 1MeV Ar 2+ ion are determined as 580±10K and 540±5K, respectively. In contrast, U 3 Si 5 remains crystalline up to 8 dpa at room temperature and is stable against ion irradiation-induced amorphization up to ~50 dpa by either 1MeV Kr 2+ or 150KeV Kr + at 623K. In conclusion, these results provide valuable experimental data to guide future irradiation experiments, support the relevant post irradiation examination, and serve as the experimental basis for the validation of advanced fuel performance models

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal stability of helium bubble superlattice in Mo under TEM in-situ heating

Although the temperature window of He ion irradiation for gas bubble superlattice (GBS) formation was found to be in the range of approximately 0.15 – 0.35 melting point, the thermal stability of He GBS has not been fully investigated. This work reports the experiment using an in-situ heating holder in a transmission electron microscope (TEM). A 3.0 mm TEM disc sample of Mo (99.5% pure) was jet-polished and then irradiated with 40 keV He ions at 300°C to a fluence of 1.0E+17 ions/cm 2 , corresponding to a peak He concentration of approximately 10 at.%, in order to introduce He GBS. In-situ heating was conducted with a ramp rate of ~ 25°C/min, hold time of ~ 30 min, and temperature step of ~ 100°C up to 850°C (0.39T m ). The result shows exceptional thermal stability of He GBS in Mo with no noticeable change on GBS lattice constant and ordering. The implication of this unique and stable ordered microstructure on mechanistic understanding of GBS and its advanced application will be discussed.

36 MATERIALS SCIENCE↗

Microstructural characterization of as-cast U-20Pu-10Zr-3.86Pd and U-20Pu-10Zr-3.86Pd-4.3Ln

Palladium is being investigated as a potential additive to metallic fuel to bind fission product lanthanides, with the goal of reducing or preventing fuel-cladding chemical interactions (FCCI). A primary cause of FCCI is the lanthanide fission products moving to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. The current study is a scanning electron microscopy (SEM) and transmission electron microscopy (TEM) investigation of as-cast U-20Pu-10Zr-3.86Pd and U-20Pu-10Zr-3.86Pd-4.3Ln in wt%, where Ln = 53Nd-25Ce-16Pr-6La. In U-20Pu-10Zr-3.86Pd, PdZr2 is forming, along with a possible ternary phase between Pu, Zr, and Pd. Pu is also present in the Pd-Ln precipitates formed in U-20Pu-10Zr-3.86Pd-4.3Ln. In the LnPd phase, Pu appears to be substitutional, forming (Ln,Pu)Pd. The other prominent phase, which appears to be Ln7Pd3, has a fine, lamellar structure. As a result, the lanthanides remain essentially constant across this fine structure, but Pu and Pd alternate as to which has the higher concentration.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of annealed U-12Zr-4Pd and U-12Zr-4Pd-5Ln: Investigating Pd as a metallic fuel additive

Here, palladium is being investigated as a potential additive to metallic fuel to control fuel-cladding chemical interaction (FCCI). A primary cause of FCCI is the lanthanide fission products moving to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. The current study is a scanning electron microscopy (SEM) and transmission electron microscopy (TEM) characterization of annealed U-12Zr-4Pd and U-12Zr-4Pd-5Ln, where Ln=53Nd-25Ce-16Pr-6La. The present study shows that Pd preferentially binds the lanthanides, which will prevent lanthanide migration and interaction with the cladding. The SEM analysis indicates the 1:1 Pd-Ln compound is being formed, while the TEM analysis, due to higher resolution, found the 1:1 compound, as well as Pd-rich compounds Pd 2 Ln and Pd 3 Ln 2 .

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hydrothermal synthesis of silicon oxide clad uranium oxide nanowires

Here, a facile method to synthesize silicon oxide clad uranium oxide nanowires is presented. U 3 Si 2 , used as a precursor, was oxidized to produce uranium oxide nanocrystallites and amorphous silicon oxide under hydrothermal conditions at 300°C and a pressure of 7.8 × 10 6 Pa. The growth of uranium oxide nanowires was assisted by silicon oxide via assembling the uranium oxide nanocrystallites in an amorphous silicon oxide matrix. The microstructure and composition of silicon oxide clad uranium oxide nanowires were characterized by XRD, SEM, TEM, and EDS. The uranium oxide in the nanowires was determined as UO 2.34 with a fluoride cubic structure.

36 MATERIALS SCIENCE↗

Radiation-induced grain subdivision and bubble formation in U 3 Si 2 at LWR temperature

Here, U 3 Si 2 , an advanced fuel form proposed for light water reactors (LWR), has excellent thermal conductivity and a higher fissile element density. However, limited understanding of the radiation performance and fission gas behavior of U 3 Si 2 is available at LWR conditions. This study explores the irradiation behavior of U 3 Si 2 by 300 KeV Xe + ion beam bombardment combining with in-situ transmission electron microscopy (TEM) observation. The crystal structure of U 3 Si 2 is stable against radiation-induced amorphization at 350 °C even up to a very high dose of 64 displacements per atom (dpa). Grain subdivision of U 3 Si 2 occurs at a relatively low dose of 0.8 dpa and continues to above 48 dpa, leading to the formation of high-density nanoparticles. Nano-sized Xe gas bubbles prevail at a dose of 24 dpa, and Xe bubble coalescence was identified with an increase of irradiation dose. The volumetric swelling resulting from Xe gas bubble formation and coalescence was estimated with respect to radiation dose, and a 2.2% volumetric swelling was observed for U 3 Si 2 irradiated at 64 dpa considering fission gas only. Due to extremely high susceptibility to oxidation, the nano-sized U 3 Si 2 grains upon radiationinduced grain subdivision were oxidized to nanocrystalline UO 2 in a high vacuum chamber for TEM observation, eventually leading to the formation of UO 2 nanocrystallites up to 80 dpa.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure studies of U3Si2 fuel pellets sintered in argon vs. vacuum environment

A comparison study on the effects of sintering U3Si2 pellets under vacuum (~1x10-6 Torr) vs in argon has been carried out as part of a pellet fabrication process for potential light water reactor fuel application. A cross section of pellets sintered in each environment was examined using scanning electron microscopy (SEM) equipped with Energy dispersive spectroscopy (EDS). The average density of pellets sintered under vacuum and argon was 11.90 g/cm3 (97.5% theoretical density (TD)) and 11.37 g/cm3 (93.2% TD), respectively. SEM micrographs and EDS revealed the grain structure of pellets sintered under vacuum (vacuum samples) to be angular with a Si rich phase, U5Si4, along the grain boundaries, while grain structure of pellets sintered in argon (argon samples) reveals smaller average grain size and higher porosity with two separate Si rich phase inclusions: U5Si4 and USi. EDS confirmed the main phase in each pellet to be U3Si2 with an O rich phase inclusion. The estimated area percent of U3Si2 and the O rich phase in the samples from SEM image analysis was: argon samples 83.9% and 5.9% and vacuum samples 81.8% and 4.6%, respectively.

fuel fabrication↗

Interdiffusion Behavior of U{sub 3}Si{sub 2} and FeCrAl via Diffusion Couple Studies

Uranium Silicide (U{sub 3}Si{sub 2}) is in use as a dispersion plate fuel in test reactors, but has not been fully tested in light water reactor (LWR) conditions. U{sub 3}Si{sub 2} pellets have been fabricated for use in commercial LWRs as part of an accident tolerant fuel system U{sub 3}Si{sub 2} has a higher uranium loading density as well as a higher thermal conductivity relative to UO{sub 2}. FeCrAl alloy is a candidate cladding material to replace the industry standard, Zircaloy. FeCrAl has outstanding high-temperature mechanical strength and oxidation resistance under accident conditions. The U{sub 3}Si{sub 2}-FeCrAl system is expected to provide more than double the amount of time from a Scram until failure criteria for the reactor is met, as well as producing roughly half the amount of H{sub 2} in the event of a loss of coolant accident (LOCA). Uranium and iron have well know eutectics that may affect/enhance diffusion of the U{sub 3}Si{sub 2}/FeCrAl fuel system. The interaction of iron with molten uranium has been investigated In the U-Fe system, UFe{sub 2}, which melts congruently at 1235 deg. C, forms a eutectic with iron that melts at 1080 deg. C and has a composition of U-77at% Fe. UFe{sub 2} also forms a eutectic with uranium that melts at 725 deg. C and has a composition of U-34at% Fe. The U-34at% Fe eutectic extended the temperature range down to 740 deg. C. Regular operating temperatures for U{sub 3}Si{sub 2} fuel is expected to be around 300 - 400 deg. C. The eutectics of iron and uranium would nominally only be of concern in accident scenarios.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Strength improvement and purification of Yb 2 Si 2 O 7 -SiC nanocomposites by surface oxidation treatment

A two-step processing was developed to prepare Yb 2 Si 2 O 7 -SiC nanocomposites. Yb 2 Si 2 O 7 -Yb 2 SiO 5 -SiC composites were first fabricated by a solid state reaction/hot-pressing method. The composites were then annealed at 1250°C in air for 2 h to activate the oxidation of SiC, which effectively transformed the Yb 2 SiO 5 into Yb 2 Si 2 O 7 . The surface cracks purposely induced can be fully healed during the oxidation treatment. The treated composites have improved flexural strength compared to their pristine composites. As a result, the mechanism for crack-healing and silicate transformation have been proposed and discussed in detail.

36 MATERIALS SCIENCE↗

Microstructure studies of interdiffusion behavior of U 3 Si 2 /Zircaloy-4 at 800 and 1000 °C

Fuel swelling during normal reactor operations could lead to unfavorable chemical interactions when in contact with its cladding. As new fuel types are developed, it is crucial to understand the interaction behavior between fuel and its cladding. Diffusion experiments between U 3 Si 2 and Zricaloy-4 (Zry-4) were conducted at 800 and 1000°C up to 100 hours. The microstructure of pristine U 3 Si 2 and U 3 Si 2 /Zry-4 interdiffusion products were examined using scanning electron microscopy (SEM) and transmission electron microscopy (TEM) equipped with an energy dispersive X-ray spectroscopy (EDS) system. The primary interdiffusion product observed at 800°C is ZrSi 2 , with secondary phases of U-Zr in the Zry-4, and Fe-Cr-W-Zr-Si phases at Zry-4/ZrSi 2 interface and Fe-Cr-U-Si phases at ZrSi 2 /U-Si interface. As a result, the primary interdiffusion products at 1000°C were Zr 2 Si, U-Zr-Fe-Ni, U, U-Zr, and a low melting point phase U 6 Fe.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Irradiation effects in Generation IV nuclear reactor materials

Generation IV reactor structural materials will be exposed to high doses and temperatures during reactor operation that may lead to irradiation-induced degradation. This degradation will differ from that seen in light water reactors and therefore understanding mechanisms controlling material performance during irradiation is critical for evaluating viability of Generation IV nuclear reactor concepts. This chapter discusses irradiation effects and microstructural changes that affect mechanical properties and dimensional stability of Generation IV reactor materials.

36 MATERIALS SCIENCE↗

Effects of neutron irradiation of Ti 3 SiC 2 and Ti 3 AlC 2 in the 121–1085 °C temperature range

Herein we report on the formation of defects in response to neutron irradiation of polycrystalline Ti 3 SiC 2 and Ti 3 AlC 2 samples exposed to doses of 0.14±0.01, 1.6±0.1, and 3.4±0.1 displacements per atom (dpa) at irradiation temperatures of 121±12, 735±6 and 1085±68 °C. After irradiation to 0.14 dpa at 121 °C and 735 °C, black spots are observed in both Ti 3 SiC 2 and Ti 3 AlC 2 . After irradiation to 1.6 and 3.4 dpa at 735 °C, basal dislocation loops, with a Burgers vector of b = ½ [0001] are observed in Ti 3 SiC 2 , with loop diameters of 21±6 and 30±8 nm for 1.6 dpa and 3.4 dpa, respectively. In Ti3AlC2, larger dislocation loops, 75±34 nm in diameter are observed after 3.4 dpa at 735 °C, in addition to stacking faults. Impurity particles of TiC, as well as stacking fault TiC platelets in the MAX phases, are seen to form extensive dislocation loops under all conditions. Voids are observed at grain boundaries and within stacking faults after 3.4 dpa irradiation, with extensive void formation in the TiC regions at 1085 °C. Remarkably, denuded zones on the order of 1 µm are observed in Ti 3 SiC 2 after irradiation to 3.4 dpa at 735 °C. Small grains, 3-5 µm in diameter, are damage free after irradiation at 1085 °C at this dose. The presence of the A-layer in the MAX phases is seen to provide enhanced irradiation tolerance. Based on these results, and up to 3.41 dpa, Ti 3 SiC 2 remains a promising candidate for high temperature nuclear applications.

36 MATERIALS SCIENCE↗

Corrosion-induced microstructural developments in 316 stainless steel during exposure to molten Li 2 BeF 4 (FLiBe) salt

The microstructural evaluation and characterization of 316 stainless steel samples that were tested in molten Li 2 BeF 4 (FLiBe) salt were investigated in this study for evaluating its performance in high-temperature molten fluoride salts. Recently, 316 stainless steel and FLiBe salt are being actively considered as the main structural alloy and primary coolant of fluoride salt-cooled high-temperature reactor (FHR), a leading nuclear reactor concept for the next generation nuclear plants (NGNP). In support of the materials development for the FHR, high-temperature corrosion tests of 316 stainless steel in molten FLiBe salt at 700°C have been conducted in both bare graphite crucibles and 316 stainless steel-lined crucibles in an inert atmosphere for up to 3000 hours. The microstructure of the tested samples was comprehensively characterized using scanning electron microscopy (SEM) in conjunction with energy dispersive x-ray spectroscopy (EDS) and electron backscatter diffraction (EBSD), and scanning transmission electron microscopy (STEM) with EDS. In addition to the noticeable intergranular corrosion attack on surface, the corrosion in terms of the Cr depletion along high angle grain boundaries (15-180º) extended to 22µm in depth after 3000-hour exposure to molten FLiBe salt in graphite crucible. The coherent Σ3 grain boundary appeared high resistance to the Cr depletion. The substantial Cr depletion from the near-to-surface layer induced phase transformation from γ-martensite to α-ferrite phase (FeNi x ) during corrosion at 700ºC. Furthermore, the presence of graphite in the molten salt doubled the corrosion attack depth and led to the formation of round Mo2C, hexagonal Cr 7 C 3 and needle-like Al 4 C 3 phase within the alloy as deep as 50 µm after 3000-hour corrosion testing. Based on the microstructural analysis, the corrosion mechanisms of 316 stainless steel in molten FLiBe salt in different corrosion crucibles were illuminated through schematic diagrams. Additionally, a thermal diffusion controlled corrosion model was developed and validated by experimental data for predicting the long-term corrosion attack depth.

36 MATERIALS SCIENCE↗

Microstructure evolution in ion-irradiated of UO{sub 2}

Uranium dioxide (UO{sub 2}) is today's most widely used nuclear fuel in commercial light water reactors. The cumulative radiation damage during the fission process causes severe degradation in the thermophysical properties of UO{sub 2} fuels, which limits their lifetime and increases their operational cost. There are four main sources for decreasing the thermal conductivity during reactor-irradiation: i) irradiation induced defects, ii) solid fission products, iii) fission gas and volatile fission products, and iv) fission gas precipitation and porosity evolution. Therefore, investigating the defect production and evolution, and fission product transport under irradiation, and revealing their physical mechanisms is of great importance in understanding the degradation of thermophysical properties of UO{sub 2} fuels. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

MAX Phases for the Nuclear Industry: Possibilities and Pitfalls

By now it is well-established that the layered, machinable, hexagonal carbides and nitrides, with the general formula, M{sub n+1}AX{sub n}, (MAX) where n = 1 to 3, M is an early transition metal, A is an A-group (mostly groups 13 and 14) element and X is either C and/or N - sometimes referred to as polycrystalline nanolaminates because every basal plane is a potential deformation or delamination plane - combine some of the best attributes of metals and ceramics. Like metals, they are electrically and thermally conductive, most readily machinable (manual hack saw will suffice) not susceptible to thermal shock, plastic at high temperatures, and exceptionally damage tolerant. Like ceramics, some of them are elastically quite rigid, lightweight, and maintain their strengths to high temperatures. The ternaries Ti{sub 3}SiC{sub 2} and Ti{sub 2}AlC are also creep, fatigue and oxidation resistant. The impetus for this work was our conjecture - proven herein - that the presence of the pure A-layers in the MAX phases would result in extraordinary damage tolerance to neutron. After irradiation to 0.14 dpa at 121 deg. C and 735 deg. C, black spots are observed in both ternaries. After irradiation to higher doses, at 735 deg. C, basal dislocation loops, with a Burgers vector of b = 1/2 [0001] are observed in TAC with loop diameters of the order of the order of 25 nm. In TAC larger dislocation loops (75±34 nm) are observed after 3.4 dpa at 735 deg. C, in addition to stacking faults. In sharp contrast to the MAX phases, the TiC impurity particles in the former, form extensive dislocation loops at all conditions. Voids are observed at grain boundaries and within stacking faults after 3.4 dpa irradiation, with extensive void formation in the TiC regions at 1085 deg. C. Most remarkably, defect free, denuded zones, of the order of 1 μm, were observed after irradiation to 3.4 dpa at 735 deg. C. Small grains, 3-5 μm in diameter were totally damage free after irradiation at 1085 deg. C to this dose. When these results are compared to those of TiC, there is little doubt that the A-layers in the MAX phases, provide enhanced neutron irradiation tolerance. Based on these, and other results that will be touched upon, it is reasonable to conclude that Ti{sub 3}SiC{sub 2} is quite a promising candidate for high (> 500 deg. C) temperature nuclear applications. At lower temperatures anisotropic swelling results in microcracking. (authors)

36 MATERIALS SCIENCE↗

Effect of neutron irradiation on defect evolution in Ti 3 SiC 2 and Ti 2 AlC

Here, we report on the characterization of defects formed in polycrystalline Ti 3 SiC 2 and Ti 2 AlC samples exposed to neutron irradiation – up to 0.1 displacements per atom (dpa) at 350 ± 40 °C or 695 ± 25 °C, and up to 0.4 dpa at 350 ± 40 °C. Black spots are observed in both Ti 3 SiC 2 and Ti 2 AlC after irradiation to both 0.1 and 0.4 dpa at 350 °C. After irradiation to 0.1 dpa at 695 °C, small basal dislocation loops, with a Burgers vector of b = 1/2 [0001] are observed in both materials. At 9 ± 3 and 10 ± 5 nm, the loop diameters in the Ti 3 SiC 2 and Ti 2 AlC samples, respectively, were comparable. At 1 × 10 23 loops/m 3 , the dislocation loop density in Ti 2 AlC was ≈1.5 orders of magnitude greater than in Ti 3 SiC 2 , at 3 x 10 21 loops/m3. After irradiation at 350 °C, extensive microcracking was observed in Ti 2 AlC, but not in Ti 3 SiC 2 . The room temperature electrical resistivities increased as a function of neutron dose for all samples tested, and appear to saturate in the case of Ti 3 SiC 2 . The MAX phases are unequivocally more neutron radiation tolerant than the impurity phases TiC and Al 2 O 3 . Based on these results, Ti 3 SiC 2 appears to be a more promising MAX phase candidate for high temperature nuclear applications than Ti 2 AlC.

36 MATERIALS SCIENCE↗

High-temperature corrosion of UNS N10003 in molten Li 2 BeF 4 (FLiBe) salt

Here, corrosion testing of Hastelloy N in molten fluoride salt was performed in purified molten 2 7 LiF-BeF 2 (66-34mol%) (FLiBe) salt at 700°C for 1000 hours, in pure nickel and graphite capsules. In the nickel capsule tests, the near-surface region of the alloy exhibited an about 200 nm porous structure, an approximately 3.5 μm chromium depleted region, and MoSi 2 precipitates. In tests performed in graphite capsules, the alloy samples gained weight due to the formation of a variety of Cr 3 C 2 , Cr 7 C 3 , Mo 2 C and Cr 23 C 6 , carbide phases on the surface and in the subsurface regions of the alloy. A Cr depleted region was observed in the near-surface region where Mo thermally diffused toward either surface or grain boundary, which induced approximately 1.4 μm Ni 3 Fe alloy layer in this region. The carbide containing layer extended to about 7 μm underneath the Ni 3 Fe layer. The presence of graphite dramatically changes the mechanisms of corrosion attack in Hastelloy N in molten FLiBe salt. Evaluated by in terms of the depth of attack, graphite clearly accelerates corrosion, but the results appear to indicate that the formation of Cr 23 C 6 phase might stabilize the Cr and mitigate its dissolution in molten FLiBe salt.

36 MATERIALS SCIENCE↗